# US 2013/0092280 A1 · Electric resistance welded oil country tubular goods and manufacturing method of electric resistance welded oil country tubular goods

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0092280 A1
- Document ID: US20130092280A1
- Status: Published application
- Kind: A1
- Application number: 13/806,688
- Filed: 2012-02-03
- Published: 2013-04-18
- Earliest claimed: 2011-04-19
- Assignees: Nippon Steel & Sumitomo Metal Corporation
- Inventors: Mitsuru Sawamura; Hitoshi Asahi
- Web page: https://patentgrep.com/patent/US20130092280A1

## CPC

- B23K 11/00: Resistance welding; Severing by resistance heating
- B21C 37/08: Making tubes with welded or soldered seams {(with helically arranged seams B21C37/122)}
- B23K 11/002: {specially adapted for particular articles or work}
- B23K 11/0073: {Butt welding of long articles advanced axially}
- C21D 1/18: Hardening (C21D1/02 takes precedence); Quenching with or without subsequent tempering (quenching devices C21D1/62)
- C21D 1/25: Hardening, combined with annealing between 300 degrees Celsius and 600 degrees Celsius, i.e. heat refining ("Vergüten")
- C21D 8/0226: {Hot rolling}
- C21D 8/0263: {following hot rolling}
- C21D 8/10: during manufacturing of tubular bodies
- C21D 9/08: for tubular bodies or pipes
- C22C 38/001: {containing N}
- C22C 38/02: containing silicon
- C22C 38/04: containing manganese
- C22C 38/06: containing aluminium
- C22C 38/12: containing tungsten, tantalum, molybdenum, vanadium, or niobium
- C22C 38/14: containing titanium or zirconium
- F16L 9/00: Rigid pipes
- F16L 13/02: Welded joints
- B23K 2101/06: Tubes
- B23K 2101/10: Pipe-lines
- B23K 2103/04: Steel {or steel} alloys
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- B21C: MANUFACTURE OF METAL SHEETS, WIRE, RODS, TUBES, PROFILES OR LIKE SEMI-MANUFACTURED PRODUCTS OTHERWISE THAN BY ROLLING; AUXILIARY OPERATIONS USED IN CONNECTION WITH METAL-WORKING WITHOUT ESSENTIALLY REMOVING MATERIAL
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- F16L: PIPES; JOINTS OR FITTINGS FOR PIPES; SUPPORTS FOR PIPES, CABLES OR PROTECTIVE TUBING; MEANS FOR THERMAL INSULATION IN GENERAL

## Abstract

[Summary] [Object] There are provided electric resistance welded oil country tubular goods having strength corresponding to API specification 5CT P110 without a heat treatment being performed on the whole steel pipe and further having excellent toughness, and a manufacturing method of an electric resistance welded oil country tubular goods. [Solution] Electric resistance welded oil country tubular goods according to the present invention have a chemical composition that contains, in mass %, C: 0.05 to 0.12%, Si: 0.03 to 0.5%, Mn: 0.80 to 2.2%, P: 0.03% or less, S: 0.003% or less, Al: 0.08% or less, Nb: 0.01% to 0.10%, Ti: 0.005 to 0.03%, B: 0.0005 to 0.0030%, and N: 0.008% or less, and in which Ti>3.4 N is satisfied, its balance is composed of Fe and inevitable impurities, and, VC90 is 15 to 40.

## Claims

### Claim 1

An electric resistance welded oil country tubular goods comprising:
a chemical composition that contains, in mass %,
C: 0.05 to 0.12%,
Si: 0.03 to 0.5%,
Mn: 0.80 to 2.2%,
P: 0.03% or less,
S: 0.003% or less,
Al: 0.08% or less,
Nb: 0.01% to 0.10%,
Ti: 0.005 to 0.03%,
B: 0.0005 to 0.0030%, and
N: 0.008% or less and in which Ti>3.4 N is satisfied, its balance is composed of Fe and inevitable impurities, and VC90 defined by Expression (1) below is 15 to 40, where a C content (%) is represented by [C], an Si content (%) is represented by [Si], an Mn content (%) is represented by [Mn], an Ni content (%) is represented by [Ni], a Cu content (%) is represented by [Cu], a Cr content (%) is represented by [Cr], and a Mo content (%) is represented by [Mo].
log VC90=2.94−0.75(2.7[C]+0.4[Si]+[Mn]+0.45[Ni]+0.45[Cu]+0.8[Cr]+2[Mo]) (1)

### Claim 2 (depends on 1)

The electric resistance welded oil country tubular goods according to claim 1, further containing one type or two types or more selected from, in mass %,
Ni: 1% or less,
Cu: 1% or less,
Mo: 0.3% or less,
Cr: 0.8% or less,
V: 0.1% or less, and
Ca: 0.0060% or less.

### Claim 3 (depends on 1)

The electric resistance welded oil country tubular goods according to claim 1, wherein
the electric resistance welded oil country tubular goods has a yield stress of 758 to 965 MPa and a tensile strength of 862 MPa or more.

### Claim 4 (depends on 1)

The electric resistance welded oil country tubular goods according to claim 1, wherein
the electric resistance welded oil country tubular goods does not have yield point elongation in a test result of a tensile test.

### Claim 5 (depends on 1)

The electric resistance welded oil country tubular goods according to claim 1, wherein
the electric resistance welded oil country tubular goods has a yield to tensile ratio of 85% to 95%.

### Claim 6 (depends on 1)

The electric resistance welded oil country tubular goods according to claim 1, wherein
a structure of the electric resistance welded oil country tubular goods other than a structure of an electric resistance welded portion is made of a bainite uniform structure.

### Claim 7 (depends on 2)

The electric resistance welded oil country tubular goods according to claim 2, wherein
the electric resistance welded oil country tubular goods has a yield stress of 758 to 965 MPa and a tensile strength of 862 MPa or more.

### Claim 8 (depends on 2)

The electric resistance welded oil country tubular goods according to claim 2, wherein
the electric resistance welded oil country tubular goods does not have yield point elongation in a test result of a tensile test.

### Claim 9 (depends on 2)

The electric resistance welded oil country tubular goods according to claim 2, wherein
the electric resistance welded oil country tubular goods has a yield to tensile ratio of 85% to 95%.

### Claim 10 (depends on 2)

The electric resistance welded oil country tubular goods according to claim 2, wherein
a structure of the electric resistance welded oil country tubular goods other than a structure of an electric resistance welded portion is made of a bainite uniform structure.

### Claim 11

An electric resistance welded oil country tubular goods manufactured by hot-rolling a steel slab and performing coiling at 300° C. or lower to make a hot-rolled steel plate, and then forming the hot-rolled steel plate into a pipe shape and subjecting edge surfaces to electric resistance welding, the a steel slab having a chemical composition that contains, in mass %,
C: 0.05 to 0.12%,
Si: 0.03 to 0.5%,
Mn: 0.80 to 2.2%,
P: 0.03% or less,
S: 0.003% or less,
Al: 0.08% or less,
Nb: 0.01% to 0.10%,
Ti: 0.005 to 0.03%,
B: 0.0005 to 0.0030%, and
N: 0.008% or less and in which Ti>3.4 N is satisfied, its balance is composed of Fe and inevitable impurities, and VC90 defined by Expression (1) below is 15 to 40, where a C content (%) is represented by [C], an Si content (%) is represented by [Si], an Mn content (%) is represented by [Mn], an Ni content (%) is represented by [Ni], a Cu content (%) is represented by [Cu], a Cr content (%) is represented by [Cr], and a Mo content (%) is represented by [Mo].
log VC90=2.94−0.75(2.7[C]+0.4[Si]+[Mn]+0.45[Ni]+0.45[Cu]+0.8[Cr]+2[Mo]) (1)

### Claim 12 (depends on 11)

The electric resistance welded oil country tubular goods according to claim 11, further containing one type or two types or more selected from, in mass %,
Ni: 1% or less,
Cu: 1% or less,
Mo: 0.3% or less,
Cr: 0.8% or less,
V: 0.1% or less, and
Ca: 0.0060% or less.

### Claim 13 (depends on 11)

The electric resistance welded oil country tubular goods according to claim 11, wherein
the electric resistance welded oil country tubular goods is manufactured without performing a heat treatment with respect to a pipe body after the electric resistance welding.

### Claim 14 (depends on 11)

The electric resistance welded oil country tubular goods according to claim 11, wherein
the electric resistance welded oil country tubular goods has a yield stress of 758 to 965 MPa and a tensile strength of 862 MPa or more.

### Claim 15 (depends on 11)

The electric resistance welded oil country tubular goods according to claim 11, wherein
the electric resistance welded oil country tubular goods does not have yield point elongation in a test result of a tensile test.

### Claim 16 (depends on 11)

The electric resistance welded oil country tubular goods according to claim 11, wherein
the electric resistance welded oil country tubular goods has a yield to tensile ratio of 85% to 95%.

### Claim 17 (depends on 11)

The electric resistance welded oil country tubular goods according to claim 11, wherein
a structure of the electric resistance welded oil country tubular goods other than a structure of an electric resistance welded portion is made of a bainite uniform structure.

### Claim 18 (depends on 12)

The electric resistance welded oil country tubular goods according to claim 12, wherein
the electric resistance welded oil country tubular goods is manufactured without performing a heat treatment with respect to a pipe body after the electric resistance welding.

### Claim 19 (depends on 12)

The electric resistance welded oil country tubular goods according to claim 12, wherein
the electric resistance welded oil country tubular goods has a yield stress of 758 to 965 MPa and a tensile strength of 862 MPa or more.

### Claim 20 (depends on 12)

The electric resistance welded oil country tubular goods according to claim 12, wherein
the electric resistance welded oil country tubular goods does not have yield point elongation in a test result of a tensile test.

### Claim 21 (depends on 12)

The electric resistance welded oil country tubular goods according to claim 12, wherein
the electric resistance welded oil country tubular goods has a yield to tensile ratio of 85% to 95%.

### Claim 22 (depends on 12)

The electric resistance welded oil country tubular goods according to claim 12, wherein
a structure of the electric resistance welded oil country tubular goods other than a structure of an electric resistance welded portion is made of a bainite uniform structure.

### Claim 23

A manufacturing method of an electric resistance welded oil country tubular goods comprising:
hot-rolling a steel slab;
performing coiling at 300° C. or lower to make a hot-rolled steel plate;
then forming the hot-rolled steel plate into a pipe shape; and
subjecting edge surfaces to electric resistance welding,
the steel slab having a chemical composition that contains, in mass %,
C: 0.05 to 0.12%,
Si: 0.03 to 0.5%,
Mn: 0.80 to 2.2%,
P: 0.03% or less,
S: 0.003% or less,
Al: 0.08% or less,
Nb: 0.01% to 0.10%,
Ti: 0.005 to 0.03%,
B: 0.0005 to 0.0030%, and
N: 0.008% or less and in which Ti>3.4 N is satisfied, its balance is composed of Fe and inevitable impurities, and VC90 defined by Expression (1) below is 15 to 40, where a C content (%) is represented by [C], an Si content (%) is represented by [Si], an Mn content (%) is represented by [Mn], an Ni content (%) is represented by [Ni], a Cu content (%) is represented by [Cu], a Cr content (%) is represented by [Cr], and a Mo content (%) is represented by [Mo].
log VC90=2.94−0.75(2.7[C]+0.4[Si]+[Mn]+0.45[Ni]+0.45[Cu]+0.8[Cr]+2[Mo]) (1)

### Claim 24 (depends on 23)

The manufacturing method of the electric resistance welded oil country tubular goods according to claim 23, further containing one type or two types or more selected from, in mass %,
Ni: 1% or less,
Cu: 1% or less,
Mo: 0.3% or less,
Cr: 0.8% or less,
V: 0.1% or less, and
Ca: 0.0060% or less.

### Claim 25 (depends on 23)

The manufacturing method of the electric resistance welded oil country tubular goods according to claim 23, wherein
a cooling rate in a range of 650 to 300° C. is set to 15 to 50° C./s.

### Claim 26 (depends on 23)

The manufacturing method of the electric resistance welded oil country tubular goods according to claim 23, wherein
a heat treatment with respect to a pipe body is not performed after the electric resistance welding.

### Claim 27 (depends on 24)

The manufacturing method of the electric resistance welded oil country tubular goods according to claim 24, wherein
a cooling rate in a range of 650 to 300° C. is set to 15 to 50° C./s.

### Claim 28 (depends on 24)

The manufacturing method of the electric resistance welded oil country tubular goods according to claim 24, wherein
a heat treatment with respect to a pipe body is not performed after the electric resistance welding.