# US 2013/0081759 A1 · Low-temperature-sinterable bonding material, and bonding method using the bonding material

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0081759 A1
- Document ID: US20130081759A1
- Status: Published application
- Kind: A1
- Application number: 13/702,718
- Filed: 2011-06-10
- Published: 2013-04-04
- Earliest claimed: 2010-06-11
- Assignees: Dowa Electronics Materials Co., Ltd.
- Inventors: Keiichi Endoh; Yutaka Hisaeda; Akihiro Miyazawa; Aiko Nagahara; Toshihiko Ueyama
- Web page: https://patentgrep.com/patent/US20130081759A1

## CPC

- B22F 1/00: Metallic powder; Treatment of metallic powder, e.g. to facilitate working or to improve properties
- B22F 1/054: Nanosized particles
- B22F 1/056: {Submicron particles having a size above 100 nm up to 300 nm}
- B22F 1/102: Metallic powder coated with organic material
- B32B 37/12: characterised by using adhesives
- B82Y 30/00: Nanotechnology for materials or surface science, e.g. nanocomposites
- C09J 1/00: Adhesives based on inorganic constituents
- C22C 5/06: Alloys based on silver
- H05K 3/32: electrically connecting electric components or wires to printed circuits
- H05K 3/346: Solder materials or compositions specially adapted therefor
- H10W 72/013: {of die-attach connectors}
- B22F 2303/10: Optional alloy component
- B22F 2998/00: Supplementary information concerning processes or compositions relating to powder metallurgy
- H05K 2201/0224: Conductive particles having an insulating coating
- H05K 2201/0257: Nanoparticles
- H05K 2203/1131: Sintering, i.e. fusing of metal particles to achieve or improve electrical conductivity
- H10W 72/07331: {Connecting techniques}
- H10W 72/30: Die-attach connectors
- H10W 72/325: {Die-attach connectors having a filler embedded in a matrix}
- H10W 72/351: {Materials of die-attach connectors}
- H10W 72/352: {comprising metals or metalloids, e.g. solders}
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- B82Y: SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES; MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES; MANUFACTURE OR TREATMENT OF NANOSTRUCTURES
- C09J: ADHESIVES; NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL; ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE; USE OF MATERIALS AS ADHESIVES (preparation of glue or gelatine C09H)
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- H05K: PRINTED CIRCUITS; CASINGS OR CONSTRUCTIONAL DETAILS OF ELECTRIC APPARATUS; MANUFACTURE OF ASSEMBLAGES OF ELECTRICAL COMPONENTS
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

Provided is a bonding material which enables formation of a bonded article in nitrogen, and can exhibit bonding strength to withstand practical use while having reduced bonding fluctuations between samples without a heat treatment procedure under pressurized or high temperature conditions. The bonding material comprises: silver nanoparticles having an average primary particle diameter of 1 to 200 nm and coated with an organic substance having 8 carbon atoms or less; a dispersion medium having a boiling point of 230° C. or higher; and a flux component including an organic matter having at least two carboxyl groups. Particularly, it is preferable to use the silver nanoparticles and submicron silver particles in combination.

## Claims

### Claim 1

A bonding material, comprising silver nanoparticles having an average primary particle diameter of 1 to 200 nm and coated with an organic substance having 8 carbon atoms or less, and a dispersion medium having a boiling point of 230° C. or higher.

### Claim 2 (depends on 1)

The bonding material according to claim 1, further comprising submicron silver particles having an average particle diameter of 0.5 to 3.0 μm.

### Claim 3 (depends on 1)

The bonding material according to claim 1, wherein the dispersion medium having a boiling point of 230° C. or higher is octanediol.

### Claim 4 (depends on 1)

The bonding material according to claim 1, further comprising an organic matter having at least two carboxyl groups as a flux component.

### Claim 5 (depends on 4)

The bonding material according to claim 4, wherein the organic matter having at least two carboxyl groups further has an ether bond.

### Claim 6 (depends on 4)

The bonding material according to claim 4, wherein the organic matter having at least two carboxyl groups is oxydi(acetic acid).

### Claim 7 (depends on 1)

The bonding material according to claim 1, wherein at least one of the organic matters which coat the surface of silver nanoparticles has 6 carbon atoms.

### Claim 8

A method for bonding two different substances, comprising the steps of: applying to a bonding surface a bonding material including silver nanoparticles having at least an average primary particle diameter of 1 to 200 nm and coated with an organic substance having 8 carbon atoms or less, an organic matter having at least two carboxyl groups and at least one ether bond as a flux component, and a dispersion medium having a boiling point of 230° C. or higher (applying step); placing an object to be bonded on the bonding material; pre-firing for heating to a predetermined temperature with the object to be bonded being placed; and main-firing for heating to a temperature higher than the temperature of the pre-firing.

### Claim 9 (depends on 8)

The bonding method according to claim 8, wherein the steps of the pre-firing and the main-firing are carried out under an inert gas atmosphere.

### Claim 10 (depends on 8)

The bonding method according to claim 8, wherein the step of the main-firing is carried out at temperatures of 200° C. or higher and 500° C. or lower.