# US 2013/0076477 A1 · Fe-GROUP-BASED SOFT MAGNETIC POWDER

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0076477 A1
- Document ID: US20130076477A1
- Status: Published application
- Kind: A1
- Application number: 13/702,379
- Filed: 2011-06-07
- Published: 2013-03-28
- Earliest claimed: 2010-06-09
- Assignees: Sintokogio, Ltd.
- Inventors: Yasushi Kino
- Web page: https://patentgrep.com/patent/US20130076477A1

## CPC

- H01F 1/01: of inorganic materials (H01F1/44 takes precedence)
- B22F 9/082: {atomising using a fluid (using centrifugal force B22F9/10)}
- C22C 1/02: by melting {(C22C1/1036 takes precedence)}
- C22C 38/02: containing silicon
- C22C 38/08: containing nickel {(C22C38/105 takes precedence)}
- C22C 38/10: containing cobalt
- C22C 38/12: containing tungsten, tantalum, molybdenum, vanadium, or niobium
- C22C 38/26: with niobium or tantalum
- C22C 38/34: with more than 1.5% by weight of silicon
- H01F 1/20: in the form of particles, e.g. powder (H01F1/147 takes precedence)
- H01F 41/0246: {Manufacturing of magnetic circuits by moulding or by pressing powder (magnetic cores made by moulding or by pressing powder H01F27/255; soft magnetic particles H01F1/20, H01F1/36)}
- B22F 2009/0828: {with water}
- H01F: MAGNETS; INDUCTANCES; TRANSFORMERS; SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER
- C22C: ALLOYS (treatment of alloys C21D, C22F)

## Abstract

The present invention provides a Fe-group-based soft magnetic powder that is used for the pressed powder magnetic cores for a choke coil, reactor coil, etc., and that has a higher magnetic permeability. At least one selected from Fe, Co, or Ni that is generally used is used as the main component of the Fe-group-based alloy (iron-based alloy) soft magnetic powder. The soft magnetic powder is produced by adding a small amount of Nb (0.05-4 wt %) or V, Ta, Ti, Mo, or W, to the molten metal and by means of an inexpensive method such as the water-atomizing method.

## Claims

### Claim 1

Crystalline Fe-group-based soft magnetic powder having a basic composition expressed by the compositional formula T100-x-yMxM′y (where T is a main component that is at least one element selected from Fe group; M is a component that improves magnetic permeability; M′ is a component that gives corrosion resistance; x is 0-15 at %; y is 0-15 at %; and x+y is 0-25 at %), wherein a trace component that modifies magnetic property, which component is at least one transition metal selected from groups IV-VI, is comprised in 0.05-4.0 weight parts based on 100 weight parts of the entire composition expressed by the compositional formula.

### Claim 2

Crystalline Fe-group-based soft magnetic powder having a composition expressed by the compositional formula T100-x-yMxM′yNz (where T is a main component that is at least one element selected from Fe group; M is a component that improves magnetic permeability; M′ is a component that gives corrosion resistance; N is a trace component that modifies magnetic property), wherein a trace component that modifies magnetic property is at least one transition metal selected from groups IV-VI, and x is 0-15 at %; y is 0-15 at %; x+y is 0-25 at %; and z is 0.015-2.4 at %.

### Claim 3 (depends on 1, 2)

The Fe-group-based soft magnetic powder of claim 1 or 2, wherein the trace component that modifies magnetic property is at least one element selected from Nb, V, Ta, Ti, Mo, and W of transition metals of groups IV-VI.

### Claim 4 (depends on 3)

The Fe-group-based soft magnetic powder of claim 3 wherein the trace component that modifies magnetic property is Nb.

### Claim 5 (depends on 1, 2)

The Fe-group-based soft magnetic powder of claim 1 or 2, wherein the component that improves magnetic permeability M is at least one selected from Si, Ni, and Co, and the component that gives corrosion resistance M′ is either Cr or Al.

### Claim 6 (depends on 5)

The Fe-group-based soft magnetic powder of claim 5 wherein T is Fe, M is Si, and M′ is Cr, and x is 2-10 at %; y is 2-10 at %; and x+y is 4-15 at %.

### Claim 7 (depends on 1, 2)

The Fe-group-based soft magnetic powder of claim 1 or 2 wherein the particles of the powder have an average diameter of 0.5-100 μm.

### Claim 8 (depends on 1, 2)

The Fe-group-based soft magnetic powder of claim 1 or 2 wherein the soft magnetic powder is manufactured by a water-atomizing process.

### Claim 9 (depends on 1, 2)

A pressed powder magnetic core that is formed from the composition comprising soft magnetic powder of claim 1 or 2 and binder(s) wherein the soft magnetic powder 100 weight parts is mixed with the binder of 1-10 weight parts.