# US 2013/0074931 A1 · Polymer interlayers comprising epoxidized vegetable oil

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0074931 A1
- Document ID: US20130074931A1
- Status: Published application
- Kind: A1
- Application number: 13/240,834
- Filed: 2011-09-22
- Published: 2013-03-28
- Earliest claimed: 2011-09-22
- Inventors: Wenjie Chen; Yinong Ma
- Web page: https://patentgrep.com/patent/US20130074931A1

## CPC

- C08K 5/1515: Three-membered rings
- B32B 17/10605: {Type of plasticiser}
- B32B 17/10761: {containing vinyl acetal}
- C08K 5/103: with polyalcohols
- C08K 5/11: of acyclic polycarboxylic acids
- C08L 29/14: Homopolymers or copolymers of acetals or ketals obtained by polymerisation of unsaturated acetals or ketals or by after-treatment of polymers of unsaturated alcohols
- H10F 19/804: {Materials of encapsulations}
- Y02E 10/50: Photovoltaic [PV] energy
- Y10T 428/31844: Of natural gum, rosin, natural oil or lac
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- H10F: INORGANIC SEMICONDUCTOR DEVICES SENSITIVE TO INFRARED RADIATION, LIGHT, ELECTROMAGNETIC RADIATION OF SHORTER WAVELENGTH OR CORPUSCULAR RADIATION
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

An interlayer comprised of a thermoplastic resin, varying amounts of an epoxidized vegetable oil, and, optionally, a conventional plasticizer. The use of a thermoplastic resin, an epoxidized vegetable (plant) oil, and, optionally, a conventional plasticizer creates synergy allowing the flow of the interlayer to be increased without sacrificing other characteristics typically associated with an increased flow (e.g., increased blocking and creep, exudation, surface roughness formation, decreased mechanical strength, and decreased manufacturing capability). In this regard, the epoxidized vegetable oil acts as a flow improvement agent, resulting in a high-flow interlayer. As a result, a thinner interlayer can be utilized in forming multiple layer panels because the resulting thinner interlayer has improved flow properties.

## Claims

### Claim 1

A high-flow interlayer comprising:
poly(vinyl butyral) resin; and
a mixture comprising:
at least one plasticizer selected from the group consisting of: triethylene glycol di-(2-ethylhexanoate), triethylene glycol di-(2-ethylbutyrate), triethylene glycol diheptanoate, tetraethylene glycol diheptanoate, dihexyl adipate, dioctyl adipate, hexyl cyclohexyladipate, diisononyl adipate, heptylnonyl adipate, and dibutyl sebacate; and
epoxidized vegetable oil;
wherein the interlayer comprises about 15 to about 100 parts mixture per one hundred parts poly(vinyl butyral) resin.

### Claim 2 (depends on 1)

The high-flow interlayer of claim 1, wherein the mixture comprises about 10 to about 75 parts plasticizer selected from said group per one hundred parts poly(vinyl butyral) resin.

### Claim 3 (depends on 1)

The interlayer of claim 1, wherein the mixture comprises about 25 to about 50 parts plasticizer selected from said group per one hundred parts poly(vinyl butyral) resin.

### Claim 4 (depends on 1)

The high-flow interlayer of claim 1, wherein the mixture comprises about 5 to about 90 parts epoxidized vegetable oil per one hundred parts poly(vinyl butyral) resin.

### Claim 5 (depends on 1)

The high-flow interlayer of claim 1, wherein the mixture comprises about 5 to about 25 parts epoxidized vegetable oil per one hundred parts poly(vinyl butyral) resin.

### Claim 6 (depends on 1)

The high-flow interlayer of claim 1, wherein the epoxidized vegetable oil is selected from the group consisting of: epoxidized soybean oil and epoxidized linseed oil.

### Claim 7 (depends on 1)

The high-flow interlayer of claim 1, wherein the epoxidized vegetable oil is epoxidized soybean oil.

### Claim 8 (depends on 1)

The high-flow interlayer of claim 1, wherein the interlayer is a multilayered interlayer.

### Claim 9

A multiple layer panel, the panel comprising:
at least one rigid substrate; and
a high-flow interlayer comprising:
poly(vinyl butyral) resin; and
a mixture comprising:
at least one plasticizer selected from the group consisting of: triethylene glycol di-(2-ethylhexanoate), triethylene glycol di-(2-ethylbutyrate), triethylene glycol diheptanoate, tetraethylene glycol diheptanoate, dihexyl adipate, dioctyl adipate, hexyl cyclohexyladipate, diisononyl adipate, heptylnonyl adipate, and dibutyl sebacate; and
epoxidized vegetable oil;
wherein the interlayer comprises about 15 to about 100 parts mixture per one hundred parts poly(vinyl butyral) resin.

### Claim 10 (depends on 9)

The multiple layer panel of claim 9, wherein the mixture comprises about 5 to about 90 parts epoxidized vegetable oil per one hundred parts poly(vinyl butyral) resin.

### Claim 11 (depends on 9)

The multiple layer panel of claim 9, wherein the epoxidized vegetable oil is selected from the group consisting of: epoxidized soybean oil and epoxidized linseed oil.

### Claim 12 (depends on 9)

The multiple layer panel of claim 9, wherein the panel further comprises a photovoltaic cell, wherein the high-flow interlayer encapsulates the photovoltaic cell.

### Claim 13

An interlayer comprising:
a poly(vinyl butyral) layer comprising about 60 to about 100 parts epoxidized vegetable per 100 parts poly(vinyl butyral) and having a glass transition temperature of about 10° C. or less.

### Claim 14 (depends on 13)

The interlayer of claim 13, wherein the poly(vinyl butyral) layer has a glass transition temperature of about 4° C. or less.

### Claim 15 (depends on 13)

The interlayer of claim 13, the poly(vinyl butyral) layer further comprising:
at least one plasticizer selected from the group consisting of: triethylene glycol di-(2-ethylhexanoate), triethylene glycol di-(2-ethylbutyrate), triethylene glycol diheptanoate, tetraethylene glycol diheptanoate, dihexyl adipate, dioctyl adipate, hexyl cyclohexyladipate, diisononyl adipate, heptylnonyl adipate, and dibutyl sebacate,
wherein the poly(vinyl butyral) layer comprises a combined total of less than about 100 parts epoxidized vegetable oil and plasticizer per one hundred parts poly(vinyl butyral).

### Claim 16 (depends on 13)

The interlayer of claim 13, wherein the interlayer is a multilayered interlayer.

### Claim 17 (depends on 13)

The interlayer of claim 13, further comprising a second poly(vinyl butyral) layer and a third poly(vinyl butyral) layer, the second and third poly(vinyl butyral) layers having glass transition temperatures of about 25° C. to about 40° C., wherein the first poly(vinyl butyral) layer is disposed between the second and third poly(vinyl butyral) layers.

### Claim 18

An interlayer comprising:
a poly(vinyl butyral) layer comprising between 2 and 20 parts epoxidized vegetable per 100 parts poly(vinyl butyral) and having a glass transition temperature of about 35° C. or greater.

### Claim 19 (depends on 18)

The interlayer of claim 18, wherein the poly(vinyl butyral) layer has a glass transition temperature of about 39° C. or greater.

### Claim 20 (depends on 18)

The interlayer of claim 18, the poly(vinyl butyral) layer further comprising:
at least one plasticizer selected from the group consisting of: triethylene glycol di-(2-ethylhexanoate), triethylene glycol di-(2-ethylbutyrate), triethylene glycol diheptanoate, tetraethylene glycol diheptanoate, dihexyl adipate, dioctyl adipate, hexyl cyclohexyladipate, diisononyl adipate, heptylnonyl adipate, and dibutyl sebacate,
wherein the poly(vinyl butyral) layer comprises a combined total of about 50 or less parts epoxidized vegetable oil and plasticizer per one hundred parts poly(vinyl butyral).

### Claim 21 (depends on 18)

The interlayer of claim 18, wherein the interlayer is a multilayered interlayer.

### Claim 22 (depends on 18)

The interlayer of claim 18, further comprising a second poly(vinyl butyral) layer and a third poly(vinyl butyral) layer, the second and third poly(vinyl butyral) layers having glass transition temperatures of about 20° C. to about 35° C., wherein the first poly(vinyl butyral) layer is disposed between the second and third poly(vinyl butyral) layers.