# US 2013/0027462 A1 · Direct inkjet imaging lithographic plates, methods for imaging and pre-press treatment

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0027462 A1
- Document ID: US20130027462A1
- Status: Published application
- Kind: A1
- Application number: 13/511,096
- Filed: 2010-11-17
- Published: 2013-01-31
- Earliest claimed: 2009-11-23
- Assignees: VIM Technologies, Inc.
- Inventors: Michael Karp; Aida Porat; Sergei Bonder; Zeev Savion; Boris Brant
- Web page: https://patentgrep.com/patent/US20130027462A1

## CPC

- B41C 1/1066: {by spraying with powders, by using a nozzle, e.g. an ink jet system, by fusing a previously coated powder, e.g. with a laser}
- B41J 2/0057: {where an intermediate transfer member receives the ink before transferring it on the printing material}
- B41J 2/2107: {characterised by the ink properties (supplying ink in a solid state B41J2/17593)}
- B41C: PROCESSES FOR THE MANUFACTURE OR REPRODUCTION OF PRINTING SURFACES (photomechanical processes for producing printing surfaces G03F; photoelectrical processes for producing printing surfaces G03G)
- B41J: TYPEWRITERS; SELECTIVE PRINTING MECHANISMS, i.e. MECHANISMS PRINTING OTHERWISE THAN FROM A FORME; CORRECTION OF TYPOGRAPHICAL ERRORS

## Abstract

Wet lithographic printing members for imaging by an inkjet printer using pigment-based aqueous ink and method for calibrating the amount of the inkjet ink to be injected in solid areas of an image are disclosed. An exemplary printing member can comprises a base substrate and a top hydrophilic coating layer having a thickness in the range of 2 to 10 microns above the base substrate. A volume of less than 10 nl/mm2 of inkjet ink is used in order to image areas in which the image is solid. Areas of the top hydrophilic coating layer, which are imagewise covered by aqueous pigmented inkjet ink, become hydrophobic. In some embodiments after imaging, the surface of the imaged printing member can be treated with acidic colloidal silica solution. Exemplary treatment can comprise wiping the surface of the imaged printing member with the acidic colloidal silica solution.

## Claims

### Claim 1

A wet lithographic printing member for imaging by an inkjet printer using pigment-based aqueous ink, comprising:
a base substrate of the wet lithographic printing member;
a top hydrophilic coating layer having a thickness in the range of 2 to 10 microns above the base substrate, wherein the coating layer comprises hydrophilic polymer, inorganic particles and crosslinking agent;
wherein areas of the top hydrophilic coating layer, which are imagewise covered by aqueous pigmented inkjet ink, are hydrophobic and was imaged with limited amount of ink per printed surface less than 10 nl/mm2.

### Claim 2 (depends on 1)

The wet lithographic printing member of claim 1, wherein volume of the inkjet ink in solid areas of the image is in the range of 2 to 10 nl/mm2.

### Claim 3 (depends on 2)

The wet lithographic printing member of claim 2, wherein volume of the inkjet ink in solid areas of the image is in the range of 4 to 7 nl/mm2.

### Claim 4 (depends on 1)

The wet lithographic printing member of claim 1, wherein the coating layer weight is between 3 to 15 g/sq.m.

### Claim 5 (depends on 4)

The wet lithographic printing member of claim 4, wherein the coating layer weight is between 3 to 6 g/sq.m.

### Claim 6 (depends on 1)

The wet lithographic printing member of claim 1, wherein the hydrophilic polymer comprises polyvinyl alcohol or polyvinyl-alcohol derivatives.

### Claim 7 (depends on 1)

The wet lithographic printing member of claim 1, wherein the inorganic particles comprises colloid silica.

### Claim 8 (depends on 1)

The wet lithographic printing member of claim 1, wherein the substrate is coated with primer underlaying the hydrophylic layer.

### Claim 9 (depends on 1)

The wet lithographic printing member of claim 1, wherein the substrate is aluminum.

### Claim 10 (depends on 9)

The wet lithographic printing member of claim 9, wherein the aluminum surface is silicated prior to coating.

### Claim 11 (depends on 9)

The wet lithographic printing member of claim 9, wherein the aluminum is grained, anodized and silicated prior to coating.

### Claim 12 (depends on 9)

The wet lithographic printing member of claim 9, wherein the aluminum is grained and silicated prior to coating.

### Claim 13 (depends on 1)

The wet lithographic printing member of claim 1, wherein the substrate is polyester.

### Claim 14 (depends on 1)

The wet lithographic printing member of claim 1, wherein the polyester has is antistatic treated surface.

### Claim 15 (depends on 1)

The wet lithographic printing member of claim 1, wherein the coating layer is imaged by Epson Stylus Pro 4880 with Cyan ink.

### Claim 16 (depends on 1)

The wet lithographic printing member of claim 1, wherein the coating layer is imaged by Epson Stylus Pro 7900.

### Claim 17 (depends on 1)

The wet lithographic printing member of claim 1, wherein after being imagewise covered by aqueous pigmented inkjet ink the imagewise covered wet lithographic printing member is treated with acidic colloidal silica solution.

### Claim 18 (depends on 17)

The wet lithographic printing member of claim 17, wherein the concentration in water of the acidic colloidal silica is in the range of 1 to 20%.

### Claim 19 (depends on 17)

The wet lithographic printing member of claim 17, wherein the concentration in water of the acidic colloidal silica is in the range of 3 to 10%.

### Claim 20

A method, comprising:
a. loading to an inkjet printer a wet-lithographic-printing plate having base substrate and a hydrophilic coating layer having a thickness in the range of 2 to 10 microns over the base substrate, wherein the hydrophilic coating layer comprises hydrophilic polymer, inorganic particles and cross-linking agent;
b. configuring the inkjet printer such that the volume of the inkjet ink to be injected over a mm2 of solid image area is between 2 and 10 nl;
c. printing the wet-lithographic-printing plate by using water-based pigment inkjet ink to create an imaged-wet-lithographic-printing plate;
d. observing the results, if the inkjet image on the imaged-wet-lithographic-printing plate is smeared, then repeats steps b-d with reduced volume of inkjet ink; if the inkjet image is not smeared, then proceed to step e;
e. installing the imaged-wet-lithographic-printing plate on a wet lithographic press machine and run few thousands of copies;
f. observing the results of sampled copies during running over the wet lithographic press machine, if image elements on one or more of the sampled copies disappeared during the printing press, then repeats the steps b-f with reduced volume of inkjet ink; if solid image areas have lower optical density than in expected range, then repeats the steps b-f with increased volume of inkjet ink; if the image is OK, then store the setting to be used for imaging similar wet lithographic printing members.

### Claim 21 (depends on 20)

The method of claim 20, wherein adjusting the printing process further comprising adjusting a RIP engine that is associated with an inkjet printer.

### Claim 22 (depends on 20)

The method of claim 20, wherein reducing the volume of the inkjet ink is implemented by reducing at least one parameter selected from a group of parameters consisting of ink-reduction factor and drop volume.

### Claim 23 (depends on 20)

The method of claim 20, wherein the substrate is aluminum.

### Claim 24 (depends on 20)

The method of claim 20, wherein the printing process is implemented by Epson Stylus Pro 4880 with Cyan ink.

### Claim 25 (depends on 20)

The member of claim 20, wherein the coating layer is imaged by Epson Stylus Pro 7900 with Cyan ink.

### Claim 26 (depends on 20)

The method of claim 20, wherein the act of installing the imaged-wet-lithographic-printing plate on a wet lithographic press further comprising treating the imaged-wet-lithographic-printing plate with acidic colloidal silica solution.

### Claim 27 (depends on 26)

The method of claim 26, wherein the concentration in water of the acidic colloidal silica is in the range of 1 to 20%.

### Claim 28 (depends on 26)

The method of claim 26, wherein the concentration in water of the acidic colloidal silica is in the range of 3 to 10%.