# US 2013/0011598 A1 · Electronic device and method for manufacturing same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2013/0011598 A1
- Document ID: US20130011598A1
- Status: Published application
- Kind: A1
- Application number: 13/614,475
- Filed: 2012-09-13
- Published: 2013-01-10
- Earliest claimed: 2010-03-19
- Assignees: Asahi Glass Company, Limited
- Inventors: Sohei Kawanami; Yoshinori Ami; Yoko Mitsui
- Web page: https://patentgrep.com/patent/US20130011598A1

## CPC

- H01J 9/26: Sealing together parts of vessels
- C03C 3/14: containing boron
- C03C 8/04: containing zinc
- C03C 8/18: containing free metals
- C03C 8/24: Fusion seal compositions being frit compositions having non-frit additions, i.e. for use as seals between dissimilar materials, e.g. glass and metal; Glass solders
- C03C 23/0025: {by a laser beam}
- H01G 9/2077: {Sealing arrangements, e.g. to prevent the leakage of the electrolyte}
- H10K 30/88: Passivation; Containers; Encapsulations
- G02F 1/1339: Gaskets; Spacers; Sealing of cells
- G02F 2202/28: Adhesive materials or arrangements
- H01J 2211/446: Electromagnetic shielding means; Antistatic means
- H01J 2211/48: Sealing, e.g. seals specially adapted for leading-in conductors
- H10K 59/871: {Self-supporting sealing arrangements}
- H10K 59/8722: {Peripheral sealing arrangements, e.g. adhesives, sealants}
- Y02E 10/542: Dye sensitized solar cells
- Y02E 10/549: Organic PV cells
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- Y10T 428/239: Complete cover or casing
- H01J: ELECTRIC DISCHARGE TUBES OR DISCHARGE LAMPS (spark-gaps H01T; electric arc lamps H05B31/00; particle accelerators H05H)
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- H01G: CAPACITORS; CAPACITORS, RECTIFIERS, DETECTORS, SWITCHING DEVICES, LIGHT-SENSITIVE OR TEMPERATURE-SENSITIVE DEVICES OF THE ELECTROLYTIC TYPE (selection of specified materials as dielectric H01B3/00; capacitors having potential barriers H10D1/62, H10K10/10)
- H10K: ORGANIC ELECTRIC SOLID-STATE DEVICES
- G02F: OPTICAL DEVICES OR ARRANGEMENTS FOR THE CONTROL OF LIGHT BY MODIFICATION OF THE OPTICAL PROPERTIES OF THE MEDIA OF THE ELEMENTS INVOLVED THEREIN; NON-LINEAR OPTICS; FREQUENCY-CHANGING OF LIGHT; OPTICAL LOGIC ELEMENTS; OPTICAL ANALOGUE/DIGITAL CONVERTERS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

When local heating by use of laser sealing or the like is applied, the bonding strength between glass substrates and a sealing layer is improved to provide an electronic device having increased reliability. An electronic device includes a first glass substrate, a second glass substrate, and a sealing layer to seal an electronic element portion disposed between these glass substrates. The sealing layer is a layer obtained by locally heating a sealing material by an electromagnetic wave, such as laser light or infrared light, to melt-bond the sealing material, the sealing material containing sealing glass, a low-expansion filler and an electromagnetic wave absorber. In the first and second glass substrates, each reacted layer is produced to have a maximum depth of at least 30 nm from an interface with the sealing layer.

## Claims

### Claim 1

An electronic device comprising:
a first glass substrate having a surface including a first sealing region;
a second glass substrate having a surface, the surface including a second sealing region corresponding to the first sealing region and disposed so as to face the surface of the first glass substrate;
an electronic element portion disposed between the first glass substrate and the second glass substrate; and
a sealing layer formed between the first sealing region of the first glass substrate and the second sealing region of the second glass substrate so as to seal the electronic element portion;
wherein the sealing layer comprises a melted and solidified layer which is obtained by locally heating a sealing material, the sealing material containing sealing glass, a low-expansion filler and an electromagnetic wave absorbent, and wherein reacted layers are produced in the first and second glass substrates by reaction with the sealing layer, each of the reacted layers having a maximum depth of at least 30 nm from an interface with the sealing layer.

### Claim 2 (depends on 1)

The electronic device according to claim 1, wherein the reacted layers have central portions formed in a shape protruding toward the first and second glass substrates in comparison with portions thereof in the vicinity of end portions.

### Claim 3 (depends on 1)

The electronic device according to claim 1, wherein each of the reacted layers has a cross-sectional area of at least 50 μm2.

### Claim 4 (depends on 1)

The electronic device according to claim 1, wherein the sealing glass comprises bismuth glass containing 70 to 90% of Bi2O3, 1 to 20% of ZnO, 2 to 12% of B2O3, and 10 to 380 ppm of Na2O by mass proportion.

### Claim 5 (depends on 1)

The electronic device according to claim 1, wherein the electromagnetic wave absorbent comprises a compound containing at least one metal selected from a group consisting of Fe, Cr, Mn, Co, Ni and Cu, or a compound containing such metal, and the sealing material contains the electromagnetic wave absorbent in a range of 0.1 to 40% by volume proportion.

### Claim 6 (depends on 5)

The electronic device according to claim 5, containing the electromagnetic wave absorbent in a range of 0.1 to 10% by volume property.

### Claim 7 (depends on 1)

The electronic device according to claim 1, wherein the low-expansion filler comprises at least one member selected from the group consisting of silica, alumina, zirconia, zirconium silicate, aluminum titanate, mullite, cordierite, eucryptite, spodumene, a zirconium phosphate compound, a tin oxide compound and a silica solid solution, and the sealing material contains the low-expansion filler in a range of 1 to 50% by volume proportion.

### Claim 8 (depends on 1)

The electronic device according to claim 1, containing the low-expansion filler in a range of 10 to 50% by volume property.

### Claim 9 (depends on 1)

The electronic device according to claim 1, wherein the sealing layer has a thickness of 2 to 15 μm and a width of 0.2 to 1.5 mm.

### Claim 10

A process for producing an electronic device, comprising:
preparing a first glass substrate having a surface including a first sealing region;
preparing a second glass substrate having a surface including a second sealing region corresponding to the first sealing region, and a sealing material layer formed in the second sealing region, the sealing material layer comprising a fired layer of a sealing material containing sealing glass, a low-expansion filler and an electromagnetic wave absorbent, the sealing glass comprising bismuth glass containing 70 to 90% of Bi2O3, 1 to 20% of ZnO, 2 to 12% of B2O3, and 10 to 380 ppm of an alkaline metal oxide by mass proportion;
laminating the first glass substrate and the second glass substrate through the sealing material layer with the surface of the first glass substrate and the surface of the second glass substrate facing each other; and
irradiating the sealing material layer with an electromagnetic wave through the first glass substrate and/or the second glass substrate to locally heat the e sealing material layer such that when the sealing glass has a softening point temperature of T (° C.), the sealing material layer is heated at a temperature in a range of at least (T+200° C.) to at most (T+800° C.), whereby the sealing material layer is melted to form a sealing layer to seal an electronic element portion disposed between the first glass substrate and the second glass substrate.

### Claim 11 (depends on 10)

The process according to claim 10, wherein the step for forming the sealing layer comprises producing layers reacted with the sealing layer in the first and second glass substrates such that each of the reacted layers has a maximum depth of at least 30 nm from an interface with the sealing layer.

### Claim 12 (depends on 11)

The process according to claim 11, further comprising producing the reacted layers so as to have central portions formed in a shape protruding toward the first and second glass substrates in comparison with portions thereof in the vicinity of end portions.

### Claim 13 (depends on 10)

The process according to claim 10, comprising irradiating the sealing material layer with laser light as the electromagnetic wave, the laser light having an output density in a range of 250 to 10,000 W/cm2.

### Claim 14 (depends on 10)

The process according to claim 10, comprising irradiating the sealing material layer with infrared light as the electromagnetic wave, the laser light having an output density in a range of 1 to 30 kW/cm2.

### Claim 15 (depends on 10)

The process according to claim 10, comprising wherein the bismuth glass in the sealing glass contains Na2O in a range of 100 to 350 ppm, and the sealing material layer is irradiated with the electromagnetic wave such that the sealing material layer is heated at a temperature in a range of at least (T+300° C.) to at most (T+500° C.).

### Claim 16

A process for producing an electronic device, comprising:
preparing a first glass substrate having a surface including a first sealing region;
preparing a second glass substrate having a surface including a second sealing region corresponding to the first sealing region, and a sealing material layer formed in the second sealing region, the sealing material layer comprising a fired layer of a sealing material containing sealing glass, a low-expansion filler and an electromagnetic wave absorbent, the sealing glass comprising bismuth glass containing 70 to 90% of Bi2O3, 1 to 20% of ZnO, 2 to 12% of B2O3, and 10 to 380 ppm of Na2O by mass proportion;
laminating the first glass substrate and the second glass substrate through the sealing material layer with the surface of the first glass substrate and the surface of the second glass substrate facing each other; and
irradiating the sealing material layer with an electromagnetic wave through the first glass substrate and/or the second glass substrate to locally heat the sealing material layer such that when the sealing glass has a softening point temperature of T (° C.), the sealing material layer is heated at a temperature in a range of at least (T+200° C.) to at most (T+800° C.), whereby the sealing material layer is melted to form a sealing layer to seal an electronic element portion disposed between the first glass substrate and the second glass substrate.

### Claim 17 (depends on 16)

The process according to claim 16, wherein the step for forming the sealing layer comprises producing layers reacted with the sealing layer in the first and second glass substrates such that each of the reacted layers has a maximum depth of at least 30 nm from an interface with the sealing layer.

### Claim 18 (depends on 16)

The process according to claim 16, further comprising producing the reacted layers so as to have central portions formed in a shape protruding toward the first and second glass substrates in comparison with portions thereof in the vicinity of end portions.

### Claim 19 (depends on 16)

The process according to claim 16, comprising irradiating the sealing material layer with laser light as the electromagnetic wave, the laser light having an output density in a range of 250 to 10,000 W/cm2.

### Claim 20 (depends on 16)

The process according to claim 16, comprising irradiating the sealing material layer with infrared light as the electromagnetic wave, the laser light having an output density in a range of 1 to 30 kW/cm2.

### Claim 21 (depends on 16)

The process according to claim 16, comprising wherein the bismuth glass in the sealing glass contains Na2O in a range of 100 to 350 ppm, and the sealing material layer is irradiated with the electromagnetic wave such that the sealing material layer is heated at a temperature in a range of at least (T+300° C.) to at most (T+500° C.).