# US 2012/0325379 A1 · Method for producing a corrosion-resistant, workable sheet metal with full-surface coating of the joined, thermally treated steel sheets

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2012/0325379 A1
- Document ID: US20120325379A1
- Status: Published application
- Kind: A1
- Application number: 12/376,211
- Filed: 2007-07-26
- Published: 2012-12-27
- Earliest claimed: 2006-08-04
- Assignees: Rasselstein AG
- Inventors: Harald Baulig; Bernd Baumann; Josef Kesselem; Helmut Oberhoffer; Andrea Link; Reiner Sauer
- Web page: https://patentgrep.com/patent/US20120325379A1

## CPC

- C25D 17/005: {Contacting devices}
- B23K 15/0053: {Seam welding}
- B23K 26/1423: {the flow carrying an electric current}
- B23K 26/144: the fluid stream containing particles, e.g. powder
- B23K 26/242: Fillet welding, i.e. involving a weld of substantially triangular cross section joining two parts
- B23K 26/702: {Auxiliary equipment}
- C21D 9/50: for welded joints
- C25D 5/02: Electroplating of selected surface areas
- C25D 5/06: Brush or pad plating
- C25D 17/10: Electrodes {, e.g. composition, counter electrode}
- C25D 17/14: for pad-plating
- B23K 2101/185: {Tailored blanks}
- C25D: PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTION OF COATINGS; ELECTROFORMING; APPARATUS THEREFOR
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)

## Abstract

The invention relates to a method of producing corrosion-resistant and workable sheet metal consisting of uncoated steel sheets (1, 1′), comprising the following steps: —placing the steel sheets (1, 1′) in abutting relationship, —welding the or each joint groove (14) by butt joint welding by means of a welding beam (13) for forming a weld (2) along the respective joint groove (4), —thermal treatment of the or each weld (2) directly after or even during the forming of the weld (2) by means of an annealing beam (15), —full-surface coating of the joined steel sheets (1, 1′), including the or each weld (2), after cooling the welds (2), with a metallic coating.

## Claims

### Claim 1

Method for producing corrosion-resistant and workable sheet metal consisting of uncoated steel sheets comprising the following steps:
placing the steel sheets in abutting relationship
welding the or each joint groove by butt-joint welding by means of a welding beam for forming a weld along the respective joint groove,
thermal treatment of the or each weld directly after or even during the forming of weld by means of an annealing beam, wherein, during cooling after welding, the temperature of weld is held in a temperature range between 800° C. and 500° C. by the annealing beam for a time period of 1 to 3 seconds in order to prevent martensite formation in the region of weld.
full-surface coating of the joined steel sheets, including the or each weld, after cooling the welds, with a metallic coating.

### Claim 2

Method for producing corrosion-resistant and workable sheet metal consisting of the steel sheets coated with a metallic coating comprising the following steps:
placing the coated steel sheets in abutting relationship
welding the or each joint groove by butt-joint welding by means of a welding beam for forming a weld along the respective joint groove,
thermal treatment of the or each weld directly after or even during the forming of weld by means of an annealing beam, wherein, during cooling after welding, the temperature of weld is held in a temperature range between 800° C. and 500° C. by the annealing beam for a time period of 1 to 3 seconds in order to prevent martensite formation in the region of weld.
applying a strip-shaped metallic coating onto each weld after cooling the weld.

### Claim 3 (depends on 1)

Method according to claim 1, wherein the coating of the steel sheets takes place by electrodeposition, especially by galvanic tinning, zinc coating or galvanic chrome-plating.

### Claim 4 (depends on 1)

Method according to claim 1 wherein the annealing beam follows the welding beam in the welding direction.

### Claim 5 (depends on 1)

Method according to claim 1, wherein the annealing beam is incident on the weld as a line focus.

### Claim 6 (depends on 1)

Method according to claim 1, wherein the temperature of weld is held in a temperature range between 800° C. and 500° C. during cooling after welding for a time period of 1.5 to 2 seconds by means of an annealing beam.

### Claim 7 (depends on 2)

Method according to claim 2, wherein the coating of weld is effected by electrodeposition on weld.

### Claim 8 (depends on 7)

Method according to claim 7, wherein an electrical voltage is applied on the steel sheets referenced to an anode which runs along the weld at a distance from it for electrodeposition on weld, and an electrolyte is simultaneously applied onto the weld.

### Claim 9 (depends on 7)

Method according to claim 7, wherein the coated steel sheets can be tin-plated or special chrome-plated steel sheets, and in that the electrolyte contains dissolved tin cations or chromium cations.

### Claim 10 (depends on 8)

Method according to claim 8 wherein the electrolyte has an electrical conductivity of 50-500 mS/cm.

### Claim 11 (depends on 8)

Method according to claim 8, wherein the electrolyte is applied onto the weld via a pad; this pad contacts the weld and is made from electrically nonconductive open-cell material.

### Claim 12 (depends on 11)

Method according to claim 11, wherein the pad contacts the surface of weld at a prescribed pressure and covers it completely.

### Claim 13 (depends on 8)

Method according to claim 8, wherein the electrolyte is sprayed onto the weld via a tube provided with at least one spray opening or spray nozzle.

### Claim 14 (depends on 7)

Method according to claim 7, wherein the steel sheets are held mostly flat in one plane during the electrodeposition on weld by means of clamping elements in the region around the weld.

### Claim 15 (depends on 8)

Method according to claim 8, wherein the steel sheets are cleaned of electrolyte residues that remain on the surface after electrodeposition on weld at least in the region around the weld.

### Claim 16 (depends on 1)

Method according to claim 1, wherein the cooling time of weld is prolonged by the annealing beam such that the cooling rate with which the weld cools is held below the cooling rate at which martensite formation could have taken place in the region of the weld without the effect of annealing beam.

### Claim 17 (depends on 2)

Method according to claim 2 wherein the annealing beam follows the welding beam in the welding direction.

### Claim 18 (depends on 2)

Method according to claim 2, wherein the annealing beam is incident on the weld as a line focus.

### Claim 19 (depends on 1)

Method according to claim 1, wherein the temperature of weld is held in a temperature range between 800° C. and 500° C. during cooling after welding for a time period of 1.5 to 2 seconds by means of an annealing beam.