# US 2012/0325046 A1 · Method for Producing a Fracture-Divided Component, and Component Produced According to the Method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2012/0325046 A1
- Document ID: US20120325046A1
- Status: Published application
- Kind: A1
- Application number: 13/602,924
- Filed: 2012-09-04
- Published: 2012-12-27
- Earliest claimed: 2010-03-09
- Assignees: Bayerische Motoren Werke Aktiengesellschaft
- Inventors: Clemens Luchner; Marc Kronenberg; Rolf Koring; Ralf Kowollik
- Web page: https://patentgrep.com/patent/US20120325046A1

## CPC

- F16C 9/045: {the bearing cap of the connecting rod being split by fracturing}
- B21B 15/00: Arrangements for performing additional metal-working operations specially combined with or arranged in, or specially adapted for use in connection with, metal-rolling mills
- F16C 33/14: Special methods of manufacture; Running-in
- B21B 2261/00: Product parameters
- B21B 2265/12: Rolling load or rolling pressure; roll force
- B21B 2267/00: Roll parameters
- B23P 17/00: Metal-working operations, not covered by a single other subclass or another group in this subclass
- F16C 2220/20: by sintering pulverised material, e.g. powder metallurgy
- F16C 2220/44: by rolling
- F16C 2220/46: by forging
- F16C 2220/62: by turning, boring, drilling
- F16C 2220/70: by grinding
- F16C 2223/00: Surface treatments; Hardening; Coating
- F16C 2223/02: Mechanical treatment, e.g. finishing
- F16C 2223/18: with induction hardening
- F16C 2223/46: by welding, e.g. by using a laser to build a layer
- F16C 2322/12: Rolling apparatus, e.g. rolling stands, rolls
- Y10T 29/49231: I.C. [internal combustion] engine making
- Y10T 29/49272: with liner, coating, or sleeve
- Y10T 29/49636: Process for making bearing or component thereof
- Y10T 74/2142: Pitmans and connecting rods
- Y10T 74/2159: Section coupled
- Y10T 74/216: Bearings, adjustable
- F16C: SHAFTS; FLEXIBLE SHAFTS; ELEMENTS OR CRANKSHAFT MECHANISMS; ROTARY BODIES OTHER THAN GEARING ELEMENTS; BEARINGS
- B21B: ROLLING OF METAL (auxiliary operations used in connection with metal-working operations covered in B21, see B21C; bending by rolling B21D; manufacture of particular objects, e.g. screws, wheels, rings, barrels, balls, by rolling B21H; pressure welding by means of a rolling mill B23K20/04)
- B23P: METAL-WORKING NOT OTHERWISE PROVIDED FOR; COMBINED OPERATIONS; UNIVERSAL MACHINE TOOLS (arrangements for copying or controlling B23Q)
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A method for producing a fracture-divided component, in particular a connecting rod, with an at least partially coated bore includes the steps of: providing an unfinished component; applying a coating of a bearing material to a bore surface; and working the coating, in order to compensate internal tensile stresses in the coating, before fracture division of the component. Alternatively, the method for producing a fracture-divided component, in particular a connecting rod, having an at least partially coated bore includes the steps of: providing an unfinished component; applying a coating of a bearing material to a bore surface before fracture division of the component; and forming a counter-hardness zone before the application of the coating in order to generate compressive stresses which oppose the internal tensile stresses of the coating.

## Claims

### Claim 1

A method of producing a fracture-divided component having an at least partially coated bore, the method comprising the acts of:
providing an unfinished component,
applying a coating of a bearing material to a bore surface of the component; and
working the coating in order to compensate internal tensile stresses in the coating, before a fracture division of the component.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the working comprises the act of:
rolling the coating.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the coating is reduced to a defined measurement before the working.

### Claim 4 (depends on 1)

The method according to claim 1, wherein, in addition to the working of the coating, a counter-hardness zone is formed for generating counter-compressive stresses, which oppose internal tensile stresses of the coating.

### Claim 5 (depends on 4)

The method according to claim 4, wherein the counter-hardness zone is formed before the applying of the coating.

### Claim 6 (depends on 1)

The method according to claim 1, wherein the component is a connecting rod for an engine.

### Claim 7 (depends on 4)

The method according to claim 4, wherein the counter-hardness zone is formed at an outer contour of the component.

### Claim 8 (depends on 4)

The method according to claim 4, wherein the counter-hardness zone is formed on the component bore to be coated.

### Claim 9 (depends on 4)

The method according to claim 4, wherein at least one of a size, shape, position and hardening depth of the counter-hardness zone is determined experimentally.

### Claim 10 (depends on 1)

The method according to claim 1, wherein the applying of the coating is carried out by thermally applying the coating using a laser.

### Claim 11 (depends on 1)

The method according to claim 1, wherein the bearing material for the coating is a low-melting material.

### Claim 12 (depends on 11)

The method according to claim 11, wherein the low-melting material is a Sn-based material.

### Claim 13

A method of producing a fracture-divided component having an at least partially coated bore, the method comprising the acts of:
providing an unfinished component;
applying a coating of a bearing material to a bore surface of the component before a fracture division of the component; and
forming a counter-hardness zone before applying of the coating for generating counter-compressive stresses which oppose internal tensile stresses of the coating.

### Claim 14 (depends on 13)

The method according to claim 13, wherein the counter-hardness zone is formed at an outer contour of the component.

### Claim 15 (depends on 13)

The method according to claim 13, wherein the counter-hardness zone is formed on the component bore to be coated.

### Claim 16 (depends on 13)

The method according to claim 13, wherein at least one of a size, shape, position and hardening depth of the counter-hardness zone is determined experimentally.

### Claim 17 (depends on 13)

The method according to claim 13, wherein the applying of the coating is carried out by thermally applying the coating using a laser.

### Claim 18 (depends on 13)

The method according to claim 13, wherein the bearing material for the coating is a low-melting material.

### Claim 19 (depends on 18)

The method according to claim 18, wherein the low-melting material is a Sn-based material.

### Claim 20 (depends on 1)

A component produced according to the method of claim 1.

### Claim 21 (depends on 20)

The component according to claim 20, wherein the component is a connecting rod for an engine.

### Claim 22 (depends on 13)

A component produced according to the method of claim 13.

### Claim 23 (depends on 22)

The component according to claim 22, wherein the component is a connecting rod for an engine.