# US 2012/0301677 A1 · Method of forming oriented block copolymer line patterns, block copolymer line patterns formed thereby, and their use to form patterned articles

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2012/0301677 A1
- Document ID: US20120301677A1
- Status: Published application
- Kind: A1
- Application number: 13/480,506
- Filed: 2012-05-25
- Published: 2012-11-29
- Earliest claimed: 2011-05-25
- Assignees: University of Massachusetts; The Regents of the University of California; Unist Academy-Industry Research Corporation
- Inventors: Thomas P. Russell; Sung Woo Hong; Doug Hyun Lee; Soojin Park; Ting Xu
- Web page: https://patentgrep.com/patent/US20120301677A1

## CPC

- B05D 3/0466: {the gas being a non-reacting gas (B05D3/0406 takes precedence)}
- B05D 3/10: by other chemical means
- B05D 3/107: {Post-treatment of applied coatings}
- B81C 1/00031: {Regular or irregular arrays of nanoscale structures, e.g. etch mask layer (photomechanical, e.g. photolithographic, production of textured or patterned surfaces G03F7/00; lithographic processes for making patterned surfaces using printing and stamping G03F7/0002)}
- B81C 1/00055: {Grooves}
- B81C 1/00063: {Trenches}
- B81C 1/00071: {Channels}
- B81C 1/00079: {Grooves not provided for in groups B81C1/00063 - B81C1/00071}
- G03F 7/0002: {Lithographic processes using patterning methods other than those involving the exposure to radiation, e.g. by stamping}
- B05D 3/0254: {After-treatment}
- B05D 5/02: to obtain a matt or rough surface
- B81C 2201/0149: Forming nanoscale microstructures using auto-arranging or self-assembling material
- Y10T 428/24521: with component conforming to contour of nonplanar surface
- B05D: PROCESSES FOR APPLYING FLUENT MATERIALS TO SURFACES, IN GENERAL (conveying articles or workpieces through baths of liquid B65G, e.g. B65G49/02)
- B81C: PROCESSES OR APPARATUS SPECIALLY ADAPTED FOR THE MANUFACTURE OR TREATMENT OF MICROSTRUCTURAL DEVICES OR SYSTEMS (making microcapsules or microballoons B01J13/02; processes or apparatus specially adapted for the manufacture or treatment of piezoelectric, electrostrictive or magnetostrictive elements per se H10N30/01)
- G03F: PHOTOMECHANICAL PRODUCTION OF TEXTURED OR PATTERNED SURFACES, e.g. FOR PRINTING, FOR PROCESSING OF SEMICONDUCTOR DEVICES; MATERIALS THEREFOR; ORIGINALS THEREFOR; APPARATUS SPECIALLY ADAPTED THEREFOR; (phototypographic composing devices B41B; photosensitive materials or processes for photographic purposes G03C; electrophotography, sensitive layers or processes therefor G03G)
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A block copolymer film having a line pattern with a high degree of long-range order is formed by a method that includes forming a block copolymer film on a substrate surface with parallel facets, and annealing the block copolymer film to form an annealed block copolymer film having linear microdomains parallel to the substrate surface and orthogonal to the parallel facets of the substrate. The line-patterned block copolymer films are useful for the fabrication of magnetic storage media, polarizing devices, and arrays of nanowires.

## Claims

### Claim 1

A method of preparing a block copolymer film comprising a line pattern, comprising:
forming a block copolymer film on a substrate surface comprising parallel facets; and
annealing the block copolymer film to form an annealed block copolymer film comprising linear microdomains parallel to the substrate surface and orthogonal to the parallel facets;
wherein the parallel facets of the substrate are characterized by a pitch λ;
wherein the block copolymer in bulk comprises a hexagonal array of cylindrical microdomains characterized by a center-to-center spacing, L2, of adjacent cylindrical microdomains; and
wherein λ/L2 is either less than or equal to 0.73 or greater than or equal to 1.4.

### Claim 2 (depends on 1)

The method of claim 1, wherein the linear microdomains have a periodicity of about 15 to about 60 nanometers.

### Claim 3 (depends on 1)

The method of claim 1, wherein the annealed block copolymer film has an order parameter, f, of at least 0.95 over an area of at least 0.5 millimeter2.

### Claim 4 (depends on 1)

The method of claim 1, wherein the annealed block copolymer film has an order parameter, f, over an area of at least 0.5 millimeter2 that is greater than the corresponding order parameter for the substrate surface.

### Claim 5 (depends on 1)

The method of claim 1, wherein the block copolymer film has a thickness of about L1 to about 2L1, wherein L1 is a center-to-center domain spacing of cylindrical microdomains in bulk block copolymer.

### Claim 6 (depends on 1)

The method of claim 1, wherein the block copolymer comprises about 65 to about 80 volume percent of a major block and about 20 to about 35 volume percent of a minor block.

### Claim 7 (depends on 1)

The method of claim 1, wherein the block copolymer film comprises a block copolymer selected from the group consisting of polystyrene-b-poly(ethylene oxide), polystyrene-b-poly(2-vinylpyridine), polystyrene-b-poly(4-vinylpyridine), polystyrene-b-polybutadiene, polystyrene-b-polydimethylsiloxane, polystyrene-b-polylactide, and polystyrene-b-poly(methyl methacrylate).

### Claim 8 (depends on 1)

The method of claim 1, wherein the block copolymer film comprises a polystyrene-b-poly(ethylene oxide).

### Claim 9 (depends on 1)

The method of claim 1, wherein the substrate consists essentially of a single crystal.

### Claim 10 (depends on 1)

The method of claim 1, wherein the substrate is selected from the group consisting of crystalline silicon, doped crystalline silicon, and crystalline aluminum oxide.

### Claim 11 (depends on 1)

The method of claim 1, wherein the substrate comprises a polymeric replica of a crystalline surface comprising parallel facets.

### Claim 12 (depends on 11)

The method of claim 11, wherein the polymeric replica comprises a polymer selected from the group consisting of poly(ethylene terephthalate)s, poly(butylene terephthalate)s, polydimethylsiloxanes, polytetrafluoroethylenes, random copolymers of tetrafluoroethylene and hexafluoropropylene, and polyimides derived from pyromellitic dianhydride and 4,4′-oxydianiline.

### Claim 13 (depends on 1)

The method of claim 1, wherein said annealing the block copolymer film comprises thermal annealing.

### Claim 14 (depends on 1)

The method of claim 1, wherein said annealing the block copolymer film comprises solvent vapor annealing.

### Claim 15 (depends on 14)

The method of claim 14, wherein the block copolymer comprises about 65 to about 80 volume percent of a major block and about 20 to about 35 volume percent of a minor block, and wherein said solvent vapor annealing comprises exposing the block copolymer film to a vapor of a solvent in which the minor block is more soluble than the major block.

### Claim 16 (depends on 14)

The method of claim 14, wherein the block copolymer comprises a polystyrene-b-poly(ethylene oxide), and wherein said solvent vapor annealing comprises exposing the block copolymer film to a solvent vapor comprising water and tetrahydrofuran.

### Claim 17 (depends on 14)

The method of claim 14, wherein the block copolymer comprises a polystyrene-b-poly(ethylene oxide), and wherein said solvent vapor annealing comprises exposing the block copolymer film to a first solvent vapor comprising water, then exposing the block copolymer film to a second solvent vapor comprising water and tetrahydrofuran.

### Claim 18 (depends on 14)

The method of claim 14, wherein said solvent vapor annealing comprises exposing the block copolymer film to a solvent vapor for about 1 to about 4 hours at a temperature of about 15 to about 30° C.

### Claim 19 (depends on 1)

The method of claim 1, wherein said annealing the block copolymer film comprises thermal annealing and solvent vapor annealing.

### Claim 20 (depends on 1)

The method of claim 1, wherein λ/L2 is less than or equal to 0.73.

### Claim 21 (depends on 1)

The method of claim 1, wherein λ/L2 is greater than or equal to 1.4.

### Claim 22 (depends on 1)

The method of claim 1, wherein said annealing the block copolymer film comprises annealing the block copolymer film to form a first annealed block copolymer film comprising a hexagonal array of cylindrical microdomains having a major axis normal to the film, and further annealing the first annealed block copolymer film to form the annealed block copolymer film comprising linear microdomains parallel to the substrate surface and orthogonal to the parallel facets.

### Claim 23 (depends on 1)

The method of claim 1,
wherein the block copolymer film has a thickness of about L1 to about 2L1, wherein L1 is a center-to-center domain spacing of cylindrical microdomains in bulk block copolymer;
wherein the block copolymer film comprises a polystyrene-b-poly(ethylene oxide);
wherein the polystyrene-b-poly(ethylene oxide) comprises about 65 to about 80 volume percent of a polystyrene block and about 20 to about 35 volume percent of a poly(ethylene oxide) block;
wherein the substrate comprises crystalline aluminum oxide or a poly(butylene terephthalate) replica of a crystalline aluminum oxide surface;
wherein said solvent vapor annealing comprises exposing the block copolymer film to a solvent vapor comprising water and tetrahydrofuran for about 1 to about 4 hours at a temperature of about 15 to about 30° C.; and
wherein the annealed block copolymer film has an order parameter, f, of at least 0.95 over an area of at least 0.5 millimeter2.

### Claim 24 (depends on 1)

A structured article prepared by the method of claim 1 and comprising:
a substrate comprising a surface comprising parallel facets characterized by a pitch, λ, corresponding to the separation between adjacent facets; and
a block copolymer film comprising a surface contacting the substrate surface comprising parallel facets; wherein the block copolymer in bulk comprises a hexagonal array of cylindrical microdomains characterized by a center-to-center spacing, L2, of adjacent cylindrical microdomains;
wherein λ/L2 is either less than or equal to 0.73 or greater than or equal to 1.4.

### Claim 25

A structured article, comprising:
a substrate comprising a surface comprising parallel facets characterized by a pitch, λ, corresponding to the separation between adjacent facets; and
a block copolymer film comprising a surface contacting the substrate surface comprising parallel facets; wherein the block copolymer in bulk comprises a hexagonal array of cylindrical microdomains characterized by a center-to-center spacing, L2, of adjacent cylindrical microdomains;
wherein λ/L2 is either less than or equal to 0.73 or greater than or equal to 1.4.