# US 2012/0269714 A1 · Method of Producing Calcite Capable of Controlling a Grain Size Thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2012/0269714 A1
- Document ID: US20120269714A1
- Status: Published application
- Kind: A1
- Application number: 13/450,058
- Filed: 2012-04-18
- Published: 2012-10-25
- Earliest claimed: 2011-04-20
- Assignees: Korea Institute of Geoscience and Mineral Resources
- Inventors: Young Nam Jang; Kyoung Won Ryu; Myung Gyu Lee; Seung Woo Lee; Kyung Sun Song; Jun Hwan Bang; Soo Chun Chae
- Web page: https://patentgrep.com/patent/US20120269714A1

## CPC

- C01F 11/181: {Preparation of calcium carbonate by carbonation of aqueous solutions and characterised by control of the carbonation conditions}
- C01P 2002/72: by d-values or two theta-values, e.g. as X-ray diagram
- C01P 2002/77: by unit-cell parameters, atom positions or structure diagrams
- C01P 2002/88: by thermal analysis data, e.g. TGA, DTA, DSC
- C01P 2004/03: obtained by SEM
- C01P 2004/30: extending in three dimensions
- C01P 2004/38: cube-like
- C01P 2004/39: parallelepiped-like
- C01P 2004/40: prism-like
- C01P 2004/41: octahedron-like
- C01P 2004/61: Micrometer sized, i.e. from 1-100 micrometer
- C01P 2004/62: Submicrometer sized, i.e. from 0.1-1 micrometer
- C01F: COMPOUNDS OF THE METALS BERYLLIUM, MAGNESIUM, ALUMINIUM, CALCIUM, STRONTIUM, BARIUM, RADIUM, THORIUM, OR OF THE RARE-EARTH METALS (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts of peroxyacids C01B15/00; sulfides or polysulfides of magnesium, calcium, strontium, or barium C01B17/42; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds other than ammonia or cyanogen containing nitrogen and non-metals and optionally metals C01B21/082; amides or imides of silicon C01B21/087}; metal {imides or} amides C01B21/092, {C01B21/0923}; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanic acid C01C3/14; salts of cyanamide C01C3/16; thiocyanates C01C3/20; {double sulfates of magnesium with sodium or potassium C01D5/12; with other alkali metals C01D15/00, C01D17/00})
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS

## Abstract

Provided is a method of synthesizing high-purity calcite capable of controlling a grain size thereof, by reacting an aqueous calcium chloride solution with CO2 gas under strong alkaline condition, to crystallize into white and ultra-fine grain calcite. The method of synthesizing fine-grain calcite according to the present disclosure can decrease super-saturation by producing calcite under the strong alkaline conditions, thereby suppressing generation and growth of grain, resulting in controlling the grain size. Therefore, the above method is useful in producing high-purity ultra-fine grain calcite and can control the grain size of calcite from several hundreds of nanometers to several tens of nanometers by regulating the concentration of an aqueous caustic soda solution.

## Claims

### Claim 1

A method of producing calcite capable of controlling a grain size thereof, in which an aqueous calcium chloride solution and an aqueous caustic soda solution are reacted with each other while CO2 gas is flown thereinto, under room temperature and room pressure, to crystallize into high-purity single-phase calcite, wherein concentrations of the aqueous calcium chloride solution and the aqueous caustic soda solution are adjusted to produce calcite having a grain size of several micrometers to several tens of nanometers.

### Claim 2 (depends on 1)

The method of claim 1, comprising:
a) preparing source materials by preparing an aqueous caustic soda solution and an aqueous calcium chloride solution;
b) performing crystallization by slowly adding the aqueous calcium chloride solution to the aqueous caustic soda solution under room temperature and room pressure and at the same time blowing CO2 gas thereinto, to crystallize into calcite; and
c) obtaining high-purity single-phase calcite by separating solid and liquid from each other in a slurry crystallized in Step b), and drying the solid.

### Claim 3 (depends on 1)

The method of claim 1, wherein the aqueous caustic soda solution has a concentration of 1 to 10N, and the aqueous calcium chloride solution has a concentration of 1 to 10M.

### Claim 4 (depends on 1)

The method of claim 1, wherein an input amount of CO2 gas is 0.3 to 5 L/min.

### Claim 5 (depends on 2)

The method of claim 2, wherein the aqueous caustic soda solution has a concentration of 1 to 10N, and the aqueous calcium chloride solution has a concentration of 1 to 10M.

### Claim 6 (depends on 2)

The method of claim 2, wherein an input amount of CO2 gas is 0.3 to 5 L/min.

### Claim 7 (depends on 1)

The method of claim 1, wherein a calcite grain having a small gain size is produced by increasing the concentrations of the aqueous caustic soda solution.