# US 2012/0267598 A1 · Semiconductor device and method for manufacturing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2012/0267598 A1
- Document ID: US20120267598A1
- Status: Published application
- Kind: A1
- Application number: 13/499,956
- Filed: 2010-10-04
- Published: 2012-10-25
- Earliest claimed: 2009-10-09
- Assignees: NEC Corporation
- Inventors: Yukihiro Sakotsubo; Masayuki Terai; Munehiro Tada; Yuko Yabe; Yukishige Saito
- Web page: https://patentgrep.com/patent/US20120267598A1

## CPC

- H10P 14/69394: {the material containing titanium, e.g. TiO2}
- H10N 70/021: {Formation of switching materials, e.g. deposition of layers}
- H10N 70/24: {based on migration or redistribution of ionic species, e.g. anions, vacancies}
- H10N 70/826: {adapted for essentially vertical current flow, e.g. sandwich or pillar type devices}
- H10N 70/8833: {Binary metal oxides, e.g. TaOx}
- H10P 14/6314: {of a metallic layer}
- H10P 14/6329: {using physical ablation of a target, e.g. physical vapour deposition or pulsed laser deposition}
- H10P 14/662: {Laminate layers, e.g. stacks of alternating high-k metal oxides (adhesion layers or buffer layers H10P14/6508, H10P14/6548)}
- H10P 14/69393: {the material containing tantalum, e.g. Ta2O5}
- H10B 63/30: {comprising selection components having three or more electrodes, e.g. transistors}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10N: ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR
- H10B: ELECTRONIC MEMORY DEVICES

## Abstract

A semiconductor device includes at least first and second electrodes, and a layer including a transition metal oxide layer sandwiched between the first and second electrodes. The transition metal oxide layer includes first and second transition metal oxide layers formed of different first and second transition metals, respectively. The first transition metal oxide layer is provided on the first electrode side, the second transition metal oxide layer is provided on the second electrode side, the first transition metal oxide layer and the second transition metal oxide layer are in contact with each other, the first transition metal oxide layer has an oxygen concentration gradient from the interface between the first transition metal oxide layer and the second transition metal oxide layer toward the first electrode side, and the oxygen concentration at the interface is greater than the oxygen concentration on the first electrode side.

## Claims

### Claim at position 1

1-12. (canceled)

### Claim 13

A semiconductor device including at least a first electrode, a second electrode, and a transition metal oxide layer sandwiched between the first electrode and the second electrode, wherein
the transition metal oxide layer includes a first transition metal oxide layer formed of a first transition metal and a second transition metal oxide layer formed of a second transition metal different from the first transition metal,
the first transition metal oxide layer is provided on the first electrode side,
the second transition metal oxide layer is provided on the second electrode side,
the first transition metal oxide layer and the second transition metal oxide layer are in contact with each other,
the first transition metal oxide layer has an oxygen concentration gradient from an interface between the first transition metal oxide layer and the second transition metal oxide layer toward the first electrode side, and
the oxygen concentration at the interface is greater than the oxygen concentration on the first electrode side.

### Claim 14 (depends on 13)

The semiconductor device described in claim 13 in which the first transition metal oxide layer is amorphous.

### Claim 15 (depends on 13)

The semiconductor device described in claim 13 in which the second transition metal oxide layer is amorphous.

### Claim 16 (depends on 13)

The semiconductor device described in claim 13 in which a composition of the first transition metal oxide at the interface between the first transition metal oxide layer and the second transition metal oxide layer is a stoichiometric composition.

### Claim 17 (depends on 13)

The semiconductor device described in claim 13 in which the first transition metal oxide layer includes any one of titanium oxide, zirconium oxide, and nickel oxide.

### Claim 18 (depends on 13)

The semiconductor device described in claim 13 in which the second transition metal oxide layer includes any one of tantalum oxide, zirconium oxide, and tantalum silicon oxide.

### Claim 19 (depends on 13)

The semiconductor device described in claim 13 in which an absolute value of a free energy of oxidation of the second transition metal is greater than that of the first transition metal.

### Claim 20 (depends on 13)

The semiconductor device described in claim 13 in which the first electrode includes any one of gold, nickel, cobalt, platinum, ruthenium, iridium, titanium, an alloy of these or an oxide of these, nitride, fluoride, carbide, and silicide and
the second electrode includes any one of gold, nickel, cobalt, platinum, ruthenium, iridium, titanium, an alloy of these or an oxide of these, nitride, fluoride, carbide, and silicide.

### Claim 21 (depends on 13)

The semiconductor device described in claim 13 in which the first electrode includes a metal whose absolute value of a free energy of oxidation is smaller than that of the first transition metal and which is electrically-conductive after it is oxidized.

### Claim 22

A method for manufacturing a semiconductor device in which at least
(a) a step for oxidizing a first transition metal layer provided on a first electrode by plasma oxidation to form a first transition metal oxide layer,
(b) a step for forming a second transition metal oxide layer formed of a transition metal different from the first transition metal on the first transition metal oxide layer after the step (a), and
(c) a step for forming a second electrode on the second transition metal oxide layer after the step (b) are performed.

### Claim 23 (depends on 22)

The method for manufacturing a semiconductor device described in claim 22 wherein the first transition metal layer is formed of titanium and the second transition metal oxide layer is formed of tantalum oxide.

### Claim 24 (depends on 22)

The method for manufacturing a semiconductor device described in claim 22 wherein in the step (a), the plasma oxidation is performed at a film forming temperature of 250 degrees C. or higher but equal to or lower than 400 degrees C.