# US 2012/0267538 A1 · Multi-element x-ray detector, its rear-earth luminescent materials, production of multi-element scintillator and detector in general

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2012/0267538 A1
- Document ID: US20120267538A1
- Status: Published application
- Kind: A1
- Application number: 13/390,323
- Filed: 2009-08-13
- Published: 2012-10-25
- Earliest claimed: 2009-08-13
- Inventors: Vladimir Nikolaevich Ulasyuk; Naum Petrovich Soschin
- Web page: https://patentgrep.com/patent/US20120267538A1

## CPC

- G01T 1/20187: {Position of the scintillator with respect to the photodiode, e.g. photodiode surrounding the crystal, the crystal surrounding the photodiode, shape or size of the scintillator}
- C09K 11/7789: {Oxysulfides}
- G01T: MEASUREMENT OF NUCLEAR OR X-RADIATION (radiation analysis of materials, mass spectrometry G01N23/00; tubes for determining the presence, intensity, density or energy of radiation or particles H01J47/00)
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE

## Abstract

The invention relates to X-ray technology and medical diagnostics, and can be used for carrying out gamma flaw detection on various articles and piping systems. The technical result is an increase in contrast of the integrated image that is produced. A multi-element X-ray radiation detector consists of a flat multi-element scintillator in the form of a discrete set of hetero-phase luminescent elements which are arranged in the cells of a mesh made from a metal which absorbs X-ray radiation and reflects light, the increment size of which mesh corresponds to the increment size of the photo receiver matrix. The metallic mesh that forms the multi-element luminescent scintillator is made from elements having an atomic number from N=26 (iron) to N=74 (tungsten), has silver-plated coils, and separates the scintillator elements optically from one another. The coils of the mesh have a diameter from 0.06 mm to 0.16 mm, and the area of the effective cross section of the mesh is between 45% to 82%. The scintillator consists of an X-ray luminophore based on a multi-ligand oxysulphide of gadolinium-lutetium-europium with the addition of bismuth and rhenium, and also fluorine, chlorine, bromine and iodine. The process of synthesis is carried out in two stages. In the first stage, oxyhalides of the elements making up a cationic subgroup are formed by reacting the initial coprecipitated oxides of rare earth elements, Bi and Re, with ammonium halides. The resulting product is then subjected to repeated thermal treatment in an alkali chalcogenide melt.

## Claims

### Claim 1

A multi-element X-ray detector, including a plate-type multi-element scintillator which transforms X-rays falling onto an external surface of the scintillator into visible light and a photodetector matrix which optically contacts with an emitting surface of the scintillator and transforms optical radiation emitted on the inner surface of the scintillator into an electrical signal; its main feature is that the above-mentioned multi-element scintillator combines a discrete set of hetero-phase luminescent elements positioned in cells of a grid made of X-ray absorbing and light reflecting metal with geometrical dimensions for spacing, cross-section and interconnection thickness for each particular luminescent element, and coincide with the actions of a photodetector matrix; a rear side of the aforesaid metal grid has an x-ray-sensitive layer, while its front surface has a multi-element semiconductor matrix with element-to-element contact with a luminescent detector; these contacting elements are simultaneously excited by X-ray radiation with energy 30 to 140 keV.

### Claim 2 (depends on 1)

The multi-element X-ray detector as per claim 1, wherein the metal grid is made of elements with atomic numbers between N=24 to N=74, where the grid size is 2-4, 20-40 or 40-60 turns per 1 mm.

### Claim 3 (depends on 1)

The Multi-element X-ray detector as per claim 1, wherein the X-ray-sensitive layer is a multi-elemental mosaic comprised of a layer of X-ray luminescent arranged by cells of a metallic grid made of elements with atomic numbers 24 to 74.

### Claim 4 (depends on 1)

The multi-element X-ray detector as per claim 1, wherein its rear side is coated with a double-layer reflecting film 2000 Å to 6000 Å thick while on the detector there is a layer of metallic silver below 1000 Å thick which is overcoated with a reflecting aluminum layer below 5000 Å thick.

### Claim 5 (depends on 1)

The multi-element X-ray detector as per claim 1, further comprising grid turns that are galvanically coated with a reflecting silver layer below 2000 Å thick.

### Claim 6 (depends on 1)

The multi-element X-ray detector as per claim 1, further comprising metal woven, coiled or galvanically deposited grid sheets used for producing a cellular multi-element structure of the detector's X-ray-sensitive layer featuring above 48% (basically, above 61%) “live cross-section” with more than 3 wires per 1 mm of the grid sheet length.

### Claim 7 (depends on 1)

The multi-element X-ray detector as per claim 1, wherein the metal grid are comprised of woven grid sheets made of stainless steel, nickel or bronze with a “live cross-section” below 64.5%, or coiled grid sheets made of tungsten wire with a “live cross-section” below 85%.

### Claim 8 (depends on 1)

The multi-element X-ray detector as per claim 1, wherein its X-ray-sensitive layer is made of a dispersed medium presented by polycarbonate featuring a refractive index n=1.59 to 1.60, which encapsulates the dispersed medium comprised of rear-earth X-ray luminescent grains with a refractive index n=2.2.

### Claim 9 (depends on 1)

The multi-element X-ray detector as per claim 1, wherein the multi-element X-ray detector utilizes a cast method of production which involves a distribution of liquid suspension of X-ray luminescent in a solution of polymer binder over a surface of a photodetector matrix; this polymer binder is polycarbonate with a molecular mass M=10000-15000 carbon units, dissolved in a low-boiling solvent such as methylene chloride; a powder X-ray luminescent amounts 20 to 56% of the polymer by mass.

### Claim 10 (depends on 1)

The multi-element X-ray detector as per claim 1, wherein the photodetector matrix is made of multiple layers of amorphous or polycrystalline silicone by means of an optical photolithography process and chemical etching.

### Claim 11 (depends on 1)

The multi-element X-ray detector as per claim 1, wherein the X-ray-sensitive layer is applied directly onto the photodetector matrix with a metallic grid sheet fixed above so that optical centers of the photodetectors are positioned exactly against the centers of the “live cross-section” of each grid cell.

### Claim 12 (depends on 1)

The multi-element X-ray detector as per claim 1, wherein the X-ray-sensitive layer is applied onto a separate plate made of X-ray-penetrable material with a metallic grid sheet fixed above; this grid is attached against the photodetector matrix with its cellular side holding an X-ray luminescent so that optical centers of the photodetectors are positioned exactly against the centers of the “live cross-section” of each grid cell.

### Claim 13 (depends on 1)

The multi-element X-ray detector as per claim 1, wherein the multi-element X-ray detector's contrast ratio is above 50% with a resolution above 4 line pairs per 1 millimeter.

### Claim 14 (depends on 1)

A Rear-earth X-ray luminophore for the multi-element X-ray detector as per claim 1 with active compounds of rear-earth elements characterized in that its hetero-phase discrete luminescent elements contain monocrystalline microscopic grains of rear-earth luminescent obtained from multiligand oxysulphides of elements such as gadolinium, lutetium, europium, dysprosium, bismuth and rhenium, and where, in their base, oxygen is partly substituted with halogen, and sulphur is partly substituted with nitrogen, thus having a stoichiometric formula as follows
(ΣMe)2O2−x(ΣHal)x/2N−3x/2S1+y
where ΣMe=Gd and/or Lu and/or Dy and/or Eu and/or Bi and/or Re,
Hal=F−1 and/or Cl−1 and/or Br−1 and/or J−1,
0.01<x≦50.08, 0.001≦y≦0.01,
while the grains of said luminescent are shaped in three-dimensional polygons coated with a disperse phase of polymer binder in a ratio 20 to 65%.

### Claim 15 (depends on 1, 14)

A production method for X-ray luminophore as per claim 14 for multi-element X-ray detector as per claim 1 through the method of codeposition of rear-earth compositions with subsequent heat treatment in a molten compounded of rear-earth ions and d-shell ions (Bi, Re, Br−1, Cl−1 and J−1) characterized in that the synthesis is in two stages; the first stage produces oxyhalides of cationic subgroup elements through a reaction between the originally codeposited oxides of rear-earth elements, Bi and Re, and ammonium halides under a temperature of T=400° C. to T=700° C. for 1 to 4 hours with secondary heat treatment in molten chalcogenides where the molecular ratio is 1:1 to 1:3 under a temperature of T=800° C. to T=1200° C. for 2 to 8 hours with subsequent leaching of the finished product with water or mineral acid solutions.