# US 2012/0267011 A1 · Sulfur treatment for copper zinc alloys

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2012/0267011 A1
- Document ID: US20120267011A1
- Status: Published application
- Kind: A1
- Application number: 13/302,374
- Filed: 2011-11-22
- Published: 2012-10-25
- Earliest claimed: 2011-04-25
- Inventors: Benjamin L. Lawrence
- Web page: https://patentgrep.com/patent/US20120267011A1

## CPC

- C23C 8/08: only one element being applied
- C23C 8/42: only one element being applied
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)

## Abstract

Brass components exhibiting excellent resistance to dezincification corrosion and stress corrosion cracking are prepared without, or with a reduced need for, corrosion inhibiting additives by developing a metal-sulfide rich barrier layer at the surfaces of the component. Brass components treated as disclosed exhibit corrosion resistance as determined by standardized testing that yields dezincification penetration less than 200 microns in depth and exhibits no stress corrosion cracking.

## Claims

### Claim 1

A finished brass component having a metal-sulfide rich barrier at surfaces of the component.

### Claim 2 (depends on 1)

A brass component in accordance with claim 1, in which the zinc content is at least 15% by weight.

### Claim 3 (depends on 1)

A brass component in accordance with claim 1, in which the zinc content is at least 33% by weight.

### Claim 4 (depends on 1)

A brass component in accordance with claim 1, having a lead content of 0.25% by weight or less.

### Claim 5 (depends on 1)

A brass component in accordance with claim 1, having a tin content sufficient to reduce dezincification.

### Claim 6 (depends on 1)

A brass component in accordance with claim 1, having a tin content of from 0.5% to 1.5% by weight.

### Claim 7 (depends on 1)

A brass component in accordance with claim 1, having a single alpha-phase structure and an arsenic, antimony and/or phosphorous content sufficient to reduce dezincification.

### Claim 8 (depends on 1)

A brass component in accordance with claim 1, having a single alpha-phase structure and at least one of arsenic, antimony and phosphorous in amount of from 0.05% to 0.15% by weight.

### Claim 9 (depends on 1)

A brass component in accordance with claim 1, which is corrosion resistant as determined by standardized testing that yields dezincification penetration less than 200 microns in depth and exhibits no stress corrosion cracking.

### Claim 10 (depends on 9)

A brass component in accordance with claim 9, which does not contain an amount of silicon or phosphorous that is sufficient to impart corrosion resistance.

### Claim 11 (depends on 1)

A brass component in accordance with claim 1, that is corrosion resistant as determined by standardized testing that yields dezincification penetration less than 200 microns in depth and exhibits no stress corrosion cracking and which exhibits improved free-machining properties as compared with brass components comprising lead, bismuth, silicon and/or phosphorous in an amount sufficient to impart corrosion resistance.

### Claim 12 (depends on 1)

A brass component in accordance with claim 1, having a zinc content of from 15% to 45% by weight that is configured for use as a press connection plumbing component.

### Claim 13 (depends on 1)

A brass component in accordance with claim 1, which is configured for use as a plumbing product.

### Claim 14 (depends on 1)

A brass component in accordance with claim 1, which is a valve component, a plumbing fitting, or a faucet component.

### Claim 15 (depends on 1)

A brass component in accordance with claim 1, in which the medical-sulfide rich barrier is a layer having a thickness of from about 9 microns to 12 microns.

### Claim 16

A process of making a corrosion resistant brass component comprising:
contacting surfaces of a finished brass component with a fluid containing labile sulfur.

### Claim 17 (depends on 16)

A process in accordance with claim 16, in which the fluid containing labile sulfur is a liquid solution.

### Claim 18 (depends on 16)

A process in accordance with claim 16, in which the fluid containing labile sulfur is a gaseous atmosphere.

### Claim 19 (depends on 17)

A process in accordance with claim 17, in which the liquid solution is a sulfuric acid solution.

### Claim 20 (depends on 19)

A process in accordance with claim 19, further comprising including a tin-containing compound in the sulfuric acid solution.

### Claim 21 (depends on 19)

A process in accordance with claim 19, in which one or both of the brass component and the sulfuric acid are at an elevated temperature.

### Claim 22 (depends on 21)

A process in accordance with claim 21, in which the elevated temperature is from 150° F. (65.6° C.) to 210° F. (98.9° C.).

### Claim 23 (depends on 21)

A process in accordance with claim 21, in which the elevated temperature is from 170° F. (76.7° C.) to 190° F. (87.8° C.).

### Claim 24 (depends on 21)

A process in accordance with claim 21, in which the elevated temperature is from 175° F. (79.4° C.) to 185° F. (85° C.).

### Claim 25 (depends on 21)

A process in accordance with claim 21, in which the elevated temperature is from 179° F. (81.7° C.) to 181° F. (82.8° C.).

### Claim 26 (depends on 18)

A process in accordance with claim 18, in which the surfaces of the brass component are contacted with a sulfur-rich atmosphere at an elevated temperature for a time sufficient to cause a reaction between the sulfur and the metal at the surface of the brass component.

### Claim 27 (depends on 26)

A process in accordance with claim 26, in which the elevated temperature is from 500° F. (260° C.) to 1500° F. (815.6° C.).

### Claim 28 (depends on 26)

A process in accordance with claim 26, in which the elevated temperature is from 900° F. (482.2° C.) to 1200° F. (648.9° C.).

### Claim 29 (depends on 26)

A process in accordance with claim 26, in which the elevated temperature is from 1050° F. (565.6° C.) to 1150° F. (621.1° C.).

### Claim 30 (depends on 26)

A process in accordance with claim 26, in which the elevated temperature is from 1075° F. (579.4° C.) to 1125° F. (607.2° C.).

### Claim 31 (depends on 26)

A process in accordance with claim 26, in which the time is at least 15 minutes.

### Claim 32 (depends on 26)

A process in accordance with claim 26, in which the sulfur-rich atmosphere is generated by combustion of potassium bisulfate.