# US 2012/0266723 A1 · Processing copper sulfide ores

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2012/0266723 A1
- Document ID: US20120266723A1
- Status: Published application
- Kind: A1
- Application number: 13/089,780
- Filed: 2011-04-19
- Published: 2012-10-25
- Earliest claimed: 2011-04-19
- Assignees: University of Education
- Inventors: Iffat Tahira Siddique; Izhar Ul Haq Khan
- Web page: https://patentgrep.com/patent/US20120266723A1

## CPC

- C22B 15/0019: {Chloridizing roasting (segregation C22B15/0023)}
- C22B 15/0073: {containing nitrogen}
- C22B 15/0086: {by physical methods}
- Y02P 10/20: Recycling
- C22B: PRODUCTION AND REFINING OF METALS (electrolytic C25); PRETREATMENT OF RAW MATERIALS
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

Copper is chemically extracted from crude ores by first roasting it at temperature up to 500° C. for 90 minutes, then treating it with ammonium salt followed by leaching with sulfuric acid to obtain a soluble copper mass for further purification.

## Claims

### Claim 1

A method for extracting copper from crude copper ore comprising:
Reducing said crude copper to a size ranging from 50-200 microns Adding to above said crude copper aluminum chloride equal in quantity to about 1/20 to ⅕ of the quantity of said crude ore;
Roasting above mixture at 450-600° C. for 80-100 minutes;
Cooling down above mixture to room temperature;
Adding above mixture to a 0.25 to 3% sulfuric acid solution in a ratio of one part above mixture to five parts of said sulfuric acid solution;
Allowing above slurry to stand to leach for a period of 0.1-3 hours;
Decanting the solution above slurry;
Filtering said decanted solution;
Drying said filtered decanted solution to crystallize copper.

### Claim 2 (depends on 1)

The method of extracting copper of claim 1 wherein said sulfuric acid solution is replaced with a solution of nitric acid or hydrochloric acid.

### Claim 3 (depends on 1)

The method of extracting copper of claim 1 wherein said period for stand to leach is 1-5 minutes.

### Claim 4 (depends on 1)

The method of extracting copper of claim 1 wherein the percent of said copper extracted is above 80%.

### Claim 5 (depends on 1)

The method of extracting copper of claim 1 wherein said crystallized copper is further extracted using a solvent.