Process for Recovering a Transition Metal Compound
AssigneeBorealis AG
InventorsPertti Elo, Sameer Vijay, Kimmo Hakala, Soile Rautio, Ismo Lehtiniemi
Life of this patent
Estimating the term…
Loading patent…
AssigneeBorealis AG
InventorsPertti Elo, Sameer Vijay, Kimmo Hakala, Soile Rautio, Ismo Lehtiniemi
Estimating the term…
The present application aims to provide a process for producing a solid polymerization catalyst component, including the steps of (A) producing a solution with a transition metal compound and a solvent; (B) solidifying a component with the transition metal compound to produce the solid polymerization catalyst component in a solidification stage; (C) recovering from the solidification stage a liquid stream containing a minor amount of the transition metal compound dissolved therein and a solid catalyst stream; and (D) recovering the transition metal component from the liquid stream, characterized in that step (D) may include concentrating the solution to produce a first product stream including the solvent and being essentially free of the transition metal compound and a second product stream including the solvent and the transition metal compound, characterized in that the concentration is conducted within a temperature range of from 0 to 100 degrees Celsius.
A Process for producing a solid polymerization catalyst component comprising the steps of (A) producing a solution comprising a transition metal compound and a solvent;
Dependencies are inferred from the claim text.