Water/oil repellent composition, method for its production and method for treating article
AssigneeAsahi Glass Company, Limited
InventorsTakao HIRONO, Yuuichi Oomori, Minako Shimada, Shuichiro Sugimoto
Life of this patent
Estimating the term…
Loading patent…
AssigneeAsahi Glass Company, Limited
InventorsTakao HIRONO, Yuuichi Oomori, Minako Shimada, Shuichiro Sugimoto
Estimating the term…
To provide a water/oil repellent composition which is capable of imparting sufficient dynamic water repellency to the surface of an article, has high stability of the particles of the copolymer, and presents a low environmental impact, a method for its production, and a method for treating an article. A water/oil repellent composition comprising a copolymer (A) having structural units based on a monomer (a) having a C1-6 polyfluoroalkyl group, structural units based on a (meth)acrylate (b) having a C20-30 alkyl group and structural units based on a halogenated olefin (c), a surfactant (B), and a medium (C), wherein the medium (C) comprises water and a propylene glycol type solvent, and the amount of the propylene glycol type solvent is from 35 to 80 parts by mass per 100 parts by mass of the copolymer (A).
A water/oil repellent composition comprising a copolymer (A) having structural units based on the following monomer (a), structural units based on the following monomer (b) and structural units based on the following monomer (c), a surfactant (B), and a medium (C), wherein the medium (C) comprises water and a propylene glycol type solvent, and the amount of the propylene glycol type solvent is from 35 to 80 parts by mass per 100 parts by mass of the copolymer (A):
A method for producing a water/oil repellent composition, which comprises polymerizing a monomer mixture comprising the following monomer (a), the following monomer (b) and the following monomer (c) in a medium (C) in the presence of a surfactant (B) and a polymerization initiator to obtain a copolymer (A), wherein the medium (C) comprises water and a propylene glycol type solvent, and the amount of the propylene glycol type solvent is from 35 to 80 parts by mass per 100 parts by mass of the monomer mixture: