# US 2012/0258567 A1 · Reaction methods to form group ibiiiavia thin film solar cell absorbers

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2012/0258567 A1
- Document ID: US20120258567A1
- Status: Published application
- Kind: A1
- Application number: 13/443,815
- Filed: 2012-04-10
- Published: 2012-10-11
- Earliest claimed: 2009-12-07
- Assignees: SoloPower, Inc.
- Inventors: Serdar AKSU; Mustafa PINARBASI
- Web page: https://patentgrep.com/patent/US20120258567A1

## CPC

- H10F 77/126: {comprising only Group I-III-VI chalcopyrite materials, e.g. CuInSe2, CuGaSe2 or CuInGaSe2 [CIGS]}
- H10F 10/167: comprising Group I-III-VI materials, e.g. CdS/CuInSe2 [CIS] heterojunction photovoltaic cells
- H10P 14/203: {using transformation of metal, e.g. oxidation or nitridation}
- H10P 14/2923: {being conductive materials, e.g. metallic silicides}
- H10P 14/3241: {being conductive materials}
- H10P 14/3436: {being chalcogenide semiconductor materials not being oxides, e.g. ternary compounds}
- H10P 14/3441: {Conductivity type}
- Y02E 10/541: CuInSe2 material PV cells
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H10F: INORGANIC SEMICONDUCTOR DEVICES SENSITIVE TO INFRARED RADIATION, LIGHT, ELECTROMAGNETIC RADIATION OF SHORTER WAVELENGTH OR CORPUSCULAR RADIATION
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

The present invention provides a method to form Group IBIIIAVIA solar cell absorber layers on continuous flexible substrates. In a preferred aspect, the method forms a Group IBIIIAVIA absorber layer for manufacturing photovoltaic cells by providing a workpiece having a precursor layer formed over a substrate, the precursor layer including copper, indium, gallium, selenium and a dopant of a Group IA material; heating the precursor layer to a first temperature; reacting the precursor layer at the first temperature for a first predetermined time to transform the precursor layer to a partially formed absorber structure; cooling down the partially formed absorber structure to a second temperature, wherein both the first temperature and the second temperature are above 400° C.; and reacting the partially formed absorber structure at the second temperature for a second predetermined time, which is longer than the first predetermined time, to form a Group IBIIIAVIA absorber layer.

## Claims

### Claim 1

A method of forming a Group IBIIIAVIA absorber layer for manufacturing photovoltaic cells, comprising:
providing a workpiece having a precursor layer formed over a substrate, the precursor layer including copper, indium, gallium, selenium and a dopant including a Group IA material;
heating the precursor layer to a first temperature;
reacting the precursor layer in selenium vapor at the first temperature for a first predetermined time to transform the precursor layer to a partially formed absorber structure;
removing the selenium vapor after the step of reacting the precursor layer at the first temperature;
cooling down the partially formed absorber structure to a second temperature,
wherein the first temperature and the second temperature are each above 400° C., and the first temperature is greater than the second temperature; and
reacting the partially formed absorber structure in an inert gas atmosphere at the second temperature for a second predetermined time, which is longer than the first predetermined time, to form a Group IBIIIAVIA absorber layer.

### Claim 2 (depends on 1)

The method of claim 1 wherein the Group IA dopant material is provided in an amount that ranges from 0.03 to 3 atomic percent of the copper in the precursor layer.

### Claim 3 (depends on 1)

The method of claim 1, wherein the Group IA material comprises one of Li and K.

### Claim 4 (depends on 3)

The method of claim 3 further comprising a Group VA material.

### Claim 5 (depends on 4)

The method of claim 4, wherein the Group VA material comprises one of Bi, As and Sb.

### Claim 6 (depends on 1)

The method of claim 1 further comprising a Group VA material.

### Claim 7 (depends on 6)

The method of claim 6, wherein the Group VA material comprises one of Bi, As and Sb.

### Claim 8 (depends on 1)

The method of claim 1, wherein the first temperature is above 620° C.

### Claim 9 (depends on 8)

The method of claim 8, wherein the second temperature is in the range of 450-525° C.

### Claim 10 (depends on 9)

The method of claim 9, wherein the first predetermined time is in the range of 2-7 minutes and the second predetermined time is in the range of 15-25 minutes.

### Claim 11 (depends on 10)

The method of claim 10, wherein the step of heating includes a ramp rate of at least 5° C./second.

### Claim 12 (depends on 1)

The method of claim 1, wherein the method of forming the Group IBIIIAVIA absorber layer is performed in a roll to roll reactor.

### Claim 13 (depends on 12)

The method of claim 12, wherein the step of providing comprises advancing the workpiece into the roll to roll reactor through an entrance opening.

### Claim 14 (depends on 13)

The method of claim 13, wherein the workpiece is released from a supply spool adjacent the entrance opening by unwrapping the workpiece from the supply spool before the step of providing.

### Claim 15 (depends on 14)

The method of claim 14, wherein the workpiece is received from an exit opening of the roll to roll reactor and wrapped around a receiving spool adjacent the entrance opening after the step of reacting the partially formed absorber structure.

### Claim 16 (depends on 1)

The method of claim 1, wherein the step of reacting the precursor layer at the second temperature is carried out in an inert gas atmosphere.

### Claim 17 (depends on 1)

The method of claim 1, wherein the first temperature is in the range of 525-650° C. and the second temperature is in the range of 450-525° C.

### Claim 18 (depends on 17)

The method of claim 17, wherein the first predetermined time is in the range of 2-7 minutes and the second predetermined time is in the range of 15-25 minutes.

### Claim 19 (depends on 1)

The method of claim 1, wherein the step of heating includes a ramp rate of at least 5° C./second.

### Claim 20

A method of forming a Group IBIIIAVIA absorber layer for manufacturing photovoltaic cells, comprising:
providing a workpiece having a precursor formed over a substrate, the precursor including copper, indium, gallium, selenium and a dopant including a Group IA material, wherein the dopant material is formed on a first stack layer of the precursor that is disposed directly on the substrate;
heating the precursor to a first temperature;
reacting the precursor in a selenium vapor to form a Group IBIIIAVIA absorber layer.

### Claim 21 (depends on 20)

The method of claim 20 wherein the Group IA dopant material is provided in an amount that ranges from 0.03 to 3 atomic percent of the copper in the precursor layer.

### Claim 22 (depends on 20)

The method of claim 20, wherein the Group IA material comprises one of Na, Li and K.

### Claim 23 (depends on 22)

The method of claim 22 further comprising a Group VA material.

### Claim 24 (depends on 23)

The method of claim 23, wherein the Group VA material comprises one of Bi, As and Sb.

### Claim 25 (depends on 29)

The method of claim 29 further comprising a Group VA material.

### Claim 26 (depends on 25)

The method of claim 25, wherein the Group VA material comprises one of Bi, As and Sb.