# US 2012/0258250 A1 · Extrusion-based additive manufacturing process with part annealing

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2012/0258250 A1
- Document ID: US20120258250A1
- Status: Published application
- Kind: A1
- Application number: 13/081,956
- Filed: 2011-04-07
- Published: 2012-10-11
- Earliest claimed: 2011-04-07
- Assignees: Stratasys, Inc.
- Inventors: Luke M.B. Rodgers
- Web page: https://patentgrep.com/patent/US20120258250A1

## CPC

- B29C 64/118: using filamentary material being melted, e.g. fused deposition modelling [FDM]
- B29C 64/106: using only liquids or viscous materials, e.g. depositing a continuous bead of viscous material
- B33Y 10/00: Processes of additive manufacturing
- B33Y 40/00: Auxiliary operations or equipment, e.g. for material handling
- B33Y 40/20: Post-treatment, e.g. curing, coating or polishing
- B33Y 70/00: Materials specially adapted for additive manufacturing
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- B33Y: ADDITIVE MANUFACTURING, i.e. MANUFACTURING OF THREE-DIMENSIONAL [3D] OBJECTS BY ADDITIVE DEPOSITION, ADDITIVE AGGLOMERATION OR ADDITIVE LAYERING, e.g. BY 3D PRINTING, STEREOLITHOGRAPHY OR SELECTIVE LASER SINTERING

## Abstract

A method for building a three-dimensional part, the method comprising providing a printed three-dimensional part and support structure, where the support structure comprises at least two polymers having different glass transition temperatures. The method also comprises annealing the three-dimensional part.

## Claims

### Claim 1

A method for printing a three-dimensional part with an extrusion-based additive manufacturing system, the method comprising:
printing a support structure from a support material with the extrusion-based additive manufacturing system using a layer-based additive manufacturing technique, wherein the support material comprises at least two polymers having different glass transition temperatures and that are substantially immiscible with each other;
in coordination with the printing of the support structure, printing the three-dimensional part from a part material with the extrusion-based additive manufacturing system using the layer-based additive manufacturing technique;
heating the printed support structure and the printed three-dimensional part to at least one temperature that is above a glass transition temperature of the part material, and that is below a glass transition temperature of at least one of the polymers of the support material; and
cooling the heated support structure and the heated three-dimensional part.

### Claim 2 (depends on 1)

The method of claim 1, wherein the at least two polymers of the support material comprise:
a first polymer having a first glass transition temperature; and
a second polymer having a second glass transition temperature that is greater than the first glass transition temperature of the first polymer by at least about 10° C.

### Claim 3 (depends on 2)

The method of claim 2, wherein the second glass transition temperature of the second polymer is at least about 20° C. greater than the first glass transition temperature of the first polymer.

### Claim 4 (depends on 1)

The method of claim 1, wherein the at least two polymers of the support material comprise:
at least one first polymer having a first average glass transition temperature; and
at least one second polymer having a second average glass transition temperature that is greater than the first average glass transition temperature of the at least one first polymer by at least about 10° C., wherein a weight ratio of the at least one second polymer to the at least one first polymer ranges from about 3:2 to about 3:1.

### Claim 5 (depends on 1)

The method of claim 1, wherein the support structure is printed to have a sprue hole; and wherein the method further comprises depositing additional part material through the sprue hole after at least a portion of the three-dimensional part is cooled.

### Claim 6 (depends on 1)

The method of claim 1, wherein the at least two polymers comprise a copolymer polymerized from monomers selected from the group consisting of acrylic acid, ionic salts of acrylic acid, methacrylic acid, ionic salts of methacrylic acid, alkyl acrylates, alkyl methacrylates, and combinations thereof.

### Claim 7 (depends on 1)

The method of claim 1, wherein the printing of the support structure using the layer-based additive manufacturing technique and the printing of the three-dimensional part using the layer-based additive manufacturing technique are performed to provide layers for the support structure and the three-dimensional part having substantially the same layer thicknesses.

### Claim 8 (depends on 1)

The method of claim 1, wherein the printing of the support structure and the printing of the three-dimensional part are performed in a build chamber of the extrusion-based additive manufacturing system, and wherein heating the printed support structure and the printed three-dimensional part is performed in the build chamber.

### Claim 9

A method for building a three-dimensional part, the method comprising:
providing a three-dimensional part and a support structure, wherein the three-dimensional part is printed from a part material using a layer-based additive manufacturing technique, and wherein the support structure is printed from a support material in coordination with the three-dimensional part using the layer-based additive manufacturing technique, the support material comprising:
a first polymer having a first glass transition temperature; and
a second polymer that is substantially immiscible with the first polymer, the second polymer having a second glass transition temperature that is higher than the first glass transition temperature of the first polymer;
heating the provided three-dimensional part and the support structure to at least one temperature that is above a glass transition temperature of the part material, that is above the first glass transition temperature of the first polymer of the support material, and that is below the second glass transition temperature of the second polymer of the support material; and
cooling the heated three-dimensional part and the heated support structure.

### Claim 10 (depends on 9)

The method of claim 9, wherein the second glass transition temperature of the second polymer is greater than the first glass transition temperature of the first polymer by at least about 10° C.

### Claim 11 (depends on 10)

The method of claim 10, wherein the second glass transition temperature of the second polymer is at least about 20° C. greater than the first glass transition temperature of the first polymer.

### Claim 12 (depends on 9)

The method of claim 9, and further comprising maintaining the heating for a duration ranging from about 2 hours to about 5 hours.

### Claim 13 (depends on 9)

The method of claim 9, wherein the second polymer comprises a copolymer polymerized from monomers selected from the group consisting of acrylic acid, ionic salts of acrylic acid, methacrylic acid, ionic salts of methacrylic acid, alkyl acrylates, alkyl methacrylates, and combinations thereof.

### Claim 14 (depends on 9)

The method of claim 9, wherein the first polymer comprises a terpolymer having a plurality of carboxyl groups, a plurality of phenyl groups, and a plurality of carboxylate ester groups.

### Claim 15

A method for printing a three-dimensional part with an extrusion-based additive manufacturing system, the method comprising:
providing a support material to the extrusion-based additive manufacturing system, the support material comprising a first polymer having a first glass transition temperature and a second polymer having a second glass transition temperature;
providing a part material to the extrusion-based additive manufacturing system, the part material having a glass transition temperature that is less than the second glass transition temperature of the second polymer of the support material;
heating a build environment of the extrusion-based additive manufacturing system to at least one temperature that is above the glass transition temperature of the part material, that is above the first glass transition temperature of the first polymer of the support material, and that is below the second glass transition temperature of the second polymer of the support material;
printing a support structure in the heated build environment from the support material in coordination with printing the three-dimensional part in the heated build environment from the part material; and
cooling the printed support structure and the printed three-dimensional part.

### Claim 16 (depends on 15)

The method of claim 15, wherein the second glass transition temperature of the second polymer is greater than the first glass transition temperature of the first polymer by at least about 10° C.

### Claim 17 (depends on 16)

The method of claim 16, wherein the second glass transition temperature of the second polymer is at least about 20° C. greater than the first glass transition temperature of the first polymer.

### Claim 18 (depends on 15)

The method of claim 15, and further comprising at least partially dissolving the cooled support structure in an aqueous alkaline solution.

### Claim 19 (depends on 15)

The method of claim 15, wherein the second polymer comprises a copolymer polymerized from monomers selected from the group consisting of acrylic acid, ionic salts of acrylic acid, methacrylic acid, ionic salts of methacrylic acid, alkyl acrylates, alkyl methacrylates, and combinations thereof.

### Claim 20 (depends on 15)

The method of claim 15, wherein the first polymer of the support structure and the second polymer of the support structure are substantially immiscible with each other.