# US 2012/0253498 A1 · Method for producing metal ingot, method for controlling liquid surface, and ultrafine copper alloy wire

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2012/0253498 A1
- Document ID: US20120253498A1
- Status: Published application
- Kind: A1
- Application number: 13/499,908
- Filed: 2011-09-12
- Published: 2012-10-04
- Earliest claimed: 2011-03-31
- Assignees: Furukawa Electronic Co., Ltd.
- Inventors: Shuji Tommatsu; Daisuke Nishide
- Web page: https://patentgrep.com/patent/US20120253498A1

## CPC

- B22D 11/005: {of wire (casting on wire B22D19/14)}
- B22D 46/00: Controlling, supervising, not restricted to casting covered by a single main group, e.g. for safety reasons (controlling or regulating in general G05)
- B22D 11/004: {Copper alloys}
- B22D 11/06: into moulds with travelling walls, e.g. with rolls, plates, belts, caterpillars
- B22D 11/161: {for automatic starting the casting process}
- B22D 11/185: {by using optical means}
- B22D: CASTING OF METALS; CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES (shaping of plastics or substances in a plastic state B29C; metallurgical processing, selection of substances to be added to metal C21, C22)

## Abstract

Surface 27 of molten metal within a mold is constantly monitored by camera 25. Camera 25 records the surface from an obliquely upward position of the mold in an area that does not affect the casting process. Various analyzing frames such as analysis band 35, molten metal pattern 37, and injection monitoring part 43, are set with respect to the information recorded by the camera 25. The analysis band 35 includes the surface (molten metal part 31c), and is set to a predetermined width so that the direction of surface change is in the longitudinal direction. The width of the analysis band 35 is set as wide as possible in a range that does not block the discharge part (molten metal part 31a). Inside the analysis band 35, the rate of change of the binary data is calculated by the analyzing part.

## Claims

### Claim at position 1

1: A method for producing metal ingot, which comprises the use of a production apparatus comprising:
a mold;
a spout that pours molten metal in a tundish to said mold;
a stopper that adjusts opening of said spout;
a camera that records image of surface of molten metal within said mold;
an analyzing part that analyzes image recorded by said camera; and
a controlling part that adjusts the opening of said spout based on information analyzed by said analyzing part;
wherein said analyzing part sets an analysis band along a direction of change of said surface on the surface image recorded by said camera, and said analysis band has a predetermined width and includes said surface, binarizes image within said analysis band to a molten metal part and a non molten metal part, obtains rate of change of the binary data for the longitudinal direction of said analysis band, and identifies the lowest position among the positions where the peak of the calculated rate of change is equal to or above a predetermined standard value as the surface height; and
wherein said controlling part adjusts the opening of said spout by comparing said surface height with a standard surface height.

### Claim at position 2 (depends on 1)

2: The method for producing metal ingot of claim 1, wherein said analyzing part analyzes image data at a regular interval, averages multiple image data within a predetermined time, and calculates said peak.

### Claim at position 3 (depends on 1)

3: The method for producing metal ingot of claim 1, wherein said analyzing part recognizes partial shape of the binarized molten metal part within the recording field of said camera, compares pattern shape corresponding to said shape of molten metal part with said shape of molten metal part, and constantly corrects position so that said shape of molten metal part and said pattern shape overlap, thereby revising the position of said analyzing part within the recording field of said camera.

### Claim at position 4 (depends on 1)

4: The method for producing metal ingot of claim 1, wherein said analyzing part monitors width of molten metal poured from a molten metal injection part to said mold within the recording field of said camera, corrects opening of said spout according to the width of molten metal at said injection part, and gives off an abnormal signal when the width of molten metal at said injection part becomes 0.

### Claim at position 5 (depends on 1)

5: The method for producing metal ingot of claim 1, wherein said analyzing part controls said spout to a closing direction when it is determined that the surface of molten metal has reached the upper limit of said analysis band, and gives off an abnormal signal when it is not determined that the surface has declined within a predetermined time.

### Claim at position 6 (depends on 1)

6: The method for producing metal ingot of claim 1, wherein for said peak, the boundary between the molten metal part and the non molten metal part is formed along the longitudinal direction of the analysis band, and the rate of change is to be 100% when there is no inclination in the rate of change between black and white at said boundary, and the rate of change is to be 0% when there is no change in black or white at parts other than said boundary, and said standard value is set in the range of 50% to 80%.

### Claim at position 7 (depends on 1)

7: The method for producing metal ingot of claim 1, wherein an upper limit is set for the opening of said spout.

### Claim at position 8 (depends on 1)

8: The method for producing metal ingot of claim 1, wherein the opening of said spout is corrected according to the molten metal surface height within said tundish.

### Claim at position 9

9: A method for controlling liquid surface, which comprises the use of a liquid transfer apparatus, comprising:
a liquid holding part in to which liquid is poured;
an injection part for pouring liquid in to said liquid holding part;
an opening adjustment part for adjusting opening of said injection part;
a camera for recording surface of liquid within said liquid holding part;
an analyzing part for analyzing image recorded by said camera;
a controlling part for adjusting opening of said injection part, based on information analyzed by said analyzing part;
wherein said analyzing part sets an analysis band along a direction of change of said surface on the surface image recorded by said camera, and said analysis band has a predetermined width and includes said surface, binarizes image within said analysis band to a liquid part and a non liquid part, obtains rate of change of the binary data for the longitudinal direction of said analysis band, and identifies the lowest position among the positions where the peak of the calculated rate of change is equal to or above a predetermined standard value as the surface height; and
wherein said controlling part adjusts the opening of said injection part by comparing said surface height with a standard surface height.

### Claim at position 10 (depends on 1)

10: An ultrafine copper alloy wire with a diameter of less than or equal to 0.03 mm diameter, which is obtained by rolling and wire drawing a copper alloy ingot produced by the method for producing metal ingot defined in claim 1, wherein the amount of wire drawing per one break is more than or equal to 15 kg.