# US 2012/0253030 A1 · Process for manufacturing low-fibrillating cellulosic fiber

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2012/0253030 A1
- Document ID: US20120253030A1
- Status: Published application
- Kind: A1
- Application number: 13/440,076
- Filed: 2012-04-05
- Published: 2012-10-04
- Earliest claimed: 2009-10-07
- Assignees: Grasim Industries Limited
- Inventors: Bir KAPOOR; Preeti LODHA; Parag PATIL; Aditya SHRIVASTAVA; Kishore SHOUCHE; Eric UERDINGEN; Michael SIEMER; Thomas WISNIEWSKI; Uwe VAGT; Massonne KLEMENS
- Web page: https://patentgrep.com/patent/US20120253030A1

## CPC

- C08B 1/003: {Preparation of cellulose solutions, i.e. dopes, with different possible solvents, e.g. ionic liquids (solutions used in the manufacture of monocomponent artificial filaments or cellulose or derivatives thereof D01F2/02)}
- D01D 5/06: Wet spinning methods {(D01D5/0046 takes precedence)}
- D01F 2/02: from solutions of cellulose in acids, bases or salts
- Y02P 20/54: using solvents, e.g. supercritical solvents or ionic liquids
- C08B: POLYSACCHARIDES; DERIVATIVES THEREOF (polysaccharides containing less than six saccharide radicals attached to each other by glycosidic linkages C07H; fermentation or enzyme-using processes C12P19/00; sugar industry C13; production of cellulose D21)
- D01D: MECHANICAL METHODS OR APPARATUS IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS, THREADS, FIBRES, BRISTLES OR RIBBONS
- D01F: CHEMICAL FEATURES IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS, THREADS, FIBRES, BRISTLES OR RIBBONS; APPARATUS SPECIALLY ADAPTED FOR THE MANUFACTURE OF CARBON FILAMENTS
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A process for manufacturing low-fibrillating cellulosic fibers by a dry-jet-wet spinning process is provided. The cellulose is treated with a specific ionic liquid based solvent to produce the said fibers with fibrillating index less than or equal to (3).

## Claims

### Claim 1

A process for producing low fibrillating cellulose fibers by a dry-jet-wet spinning process comprising following steps:
a. dissolving cellulose in a solvent system containing at least 50% of at least one ionic liquid to form a polymer solution of 100 to 1000000 Poise zero shear viscosity wherein the ionic liquid has cations with heterocyclic ring system containing one or two nitrogen atoms, each such nitrogen atom substituted by an alkyl group having 1 to 20 carbon atoms, and anions being at least one selected from the group consisting of a carboxylate anion of formula Ra-COO− wherein Ra is a alkyl group having 1 to 20 carbon atoms, preferably 5 to 0.9 carbon atoms, and phosphate anion of formula Rb-Rc-P04−, Rb and Rc are alkyl groups having 1 to 20 carbon atoms, preferably having 1 to 5 carbon atoms, and total number of carbon atoms i the alkyl groups in the anion and cation being at least 5, preferably 7, most preferably at least 9;
b. spinning fibres from said solution in a spinneret through an air gap of 2 mm to 50 mm into a coagulation bath comprising 0.01% to 70% by weight of said ionic liquid, maintained at a temperature between −5° C. to 60° C.; and
c. washing and drying the fibers obtained in step (b).

### Claim 2 (depends on 1)

The process as claimed in claim 1, wherein the ionic liquid is at least one selected from the group consisting of Dibutyl imidazolium acetate, Dipentyl imidazolium acetate, Dihexyl imidazolium acetate, Dibutyl imidazolium octanoate, 1-Ethyl-3-methyl imidazolium heptanoate, Dipropyl imidazolium octanoate, 1-Ethyl-3-methyl imidazolium octanoate, 1-Ethyl-3-methyl imidazolium nonanoate, 1-Ethy 1-3-methyl imidazolium decanoate, 1-Ethyl-3-methyl imidazolium undecanoate, 1-Ethyl-3-methyl imidazolium dodecanoate, 1-Ethyl-3-methyl immidazolium diethyl phosphate, Diethyl imidazolium octanoate and 1-Decy-1-3-methyl imidazolium acetate.

### Claim 3 (depends on 1)

The process as claimed in claim 1, where in the total number of carbon atoms in the alkyl groups of the anion and cation being at the most 30, preferably below 26, most preferably below 22.

### Claim 4 (depends on 1)

The process as claimed in claim 1, wherein the concentration of the ionic liquid is at least 70% by weight of the solvent system.

### Claim 5 (depends on 1)

The process as claimed in claim 1, wherein the solvent system further comprises at least one solvent selected from the group consisting of water, dimethyl sulfoxide, dimethyl acetamide, dimethyl formamide, N-methylpyrrolidone and mixtures thereof.

### Claim 6 (depends on 1)

The process as claimed in claim 1, wherein the coagulation bath further comprises at least 40% by weight of a protic solvent selected from the group consisting of water, methanol, ethanol, glycerol, n-propanol, iso-propanol and mixtures thereof.

### Claim 7

The process for producing low fibrillating cellulose fibers by a dry-jet-wet spinning process comprising following steps:
a. dissolving cellulose in a solvent system containing at least 50% of at least one 1,3-disubstituted imidazolium salt of the formula I
where,
R1 and R3 are each, independently of one another, an organic group having 1 to 20 carbon atoms, preferably 1 to 4 carbon atoms;
R2, R4 and R5 are each, independently of one another, an H atom or an organic group having from 1 to 20 carbon atoms, preferably R2, R4 and R5 are each H atom;
X is an anion, anion being at least one selected from the group consisting of a carboxylate anion of formula Ra-COO− wherein Ra is a alkyl group having 1 to 20 carbon atoms, preferably 5 to 9 carbon atoms and phosphate anion of formula Rb-Rc-P04−, Rb and Rc are alkyl groups having 1 to 20 carbon atoms, preferably having 1 to 5 carbon atoms; and n is 1, 2 or 3 to form a polymer solution of 100 to 1000000 Poise zero shear viscosity wherein the ionic liquid has cations with heterocyclic ring system containing one or two nitrogen atoms, each such nitrogen atom substituted by an alkyl group having 1 to 20 carbon atoms, and anions being at least one selected from the group consisting of a carboxylate anion of formula Ra-COO− wherein Ra is an alkyl group having 1 to 20 carbon atoms, preferably 5 to 9 carbon atoms, and phosphate anion of formula Rb-Rc-PO4−, Rb and Rc are alkyl groups having 1 to 20 carbon atoms, preferably having 1 to 5 carbon atoms, and total number of carbon atoms i the alkyl groups in the anion and cation being at least 5, preferably 7, most preferably at least 9;
b. spinning fibres from said solution in a spinneret through an air gap of 2 mm to 50 mm into a coagulation bath comprising 0.01% to 70% by weight of said ionic liquid, maintained at a temperature between −5° C. to 60° C.; and
c. washing and drying the fibers obtained in step (b).

### Claim 8 (depends on 7)

The process as claimed in claim 7, wherein R1 and R3 are same.

### Claim 9 (depends on 7)

The process as claimed in claim 7, wherein X is diethyl phosphate.

### Claim 10 (depends on 1)

The fibres produced in accordance with the claim 1 having fibrillation index less than or equal to 3.

### Claim 11 (depends on 7)

The fibers produced in accordance with claim 7 having fibrillation index less than or equal to 3.