# US 2012/0252988 A1 · Process for preparing a bimodal polyethylene product in a single loop reactor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2012/0252988 A1
- Document ID: US20120252988A1
- Status: Published application
- Kind: A1
- Application number: 13/514,087
- Filed: 2010-12-17
- Published: 2012-10-04
- Earliest claimed: 2009-12-18
- Assignees: Total Petrochemicals Research Feluy
- Inventors: Martine Slawinski
- Web page: https://patentgrep.com/patent/US20120252988A1

## CPC

- C08F 210/16: Copolymers of ethene with alpha-alkenes, e.g. EP rubbers
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS

## Abstract

The present invention relates to a process for preparing a bimodal polyethylene product in a single loop reactor, comprising polymerizing ethylene monomer and optionally one or more olefin co-monomers in the presence of a single heterogeneous polymerization catalyst consisting of a metallocene-alumoxane catalyst immobilized on a porous support wherein said metallocene comprises only one transition metal. Said polymerization catalyst consists of two physically different fractions of support particles onto which said metallocene-alumoxane catalyst is immobilized.

## Claims

### Claim 1

A process for preparing a bimodal polyethylene product in a single loop reactor, comprising polymerizing ethylene monomer and optionally one or more olefin co-monomers in the presence of a single heterogeneous polymerization catalyst consisting of a metallocene-alumoxane catalyst immobilized on a particulate porous support,
wherein said metallocene comprises only one transition metal,
wherein said particulate porous support consists of a first fraction support and a second fraction support, and
wherein said first fraction support differs from said second fraction support in at least one physical parameter.

### Claim 2 (depends on 1)

Process according to claim 1, wherein said support is a particulate porous silica support.

### Claim 3 (depends on 1, 2)

Process according to claim 1 or 2, wherein said first fraction support differs from said second fraction support in at least one physical parameter selected from the group comprising median particle diameter, average pore diameter, average pore volume, and surface area.

### Claim 4 (depends on 1, 2, 3)

Process according to any of claims 1 to 3, wherein the difference between the median particle diameter of said first fraction support and the median particle diameter of said second fraction support is at least 15 μm.

### Claim 5 (depends on 3, 4)

Process according to claim 3 or 4, wherein the difference between the average pore diameter of said first fraction support and the average pore diameter of said second fraction support is at least 30 Angstrom.

### Claim 6 (depends on 3, 4, 5)

Process according to any of claims 3 to 5, wherein the difference between the average pore volume of said first fraction support and the average pore volume of said second fraction support is at least 0.2 ml/g.

### Claim 7 (depends on 3, 4, 5, 6)

Process according to any of claims 3 to 6, wherein the difference between the surface area of said first fraction support and the surface area of said second fraction support is at least 100 m2/g.

### Claim 8 (depends on 1, 2, 3, 4, 5, 6, 7)

Process according to any of claims 1 to 7, wherein said polymerization catalyst consists of a first fraction catalyst and a second fraction catalyst and wherein said first fraction catalyst differs from said second fraction catalyst in median particle diameter.

### Claim 9 (depends on 8)

Process according to claim 8, wherein the difference between the median particle diameter of said first fraction catalyst and the median particle diameter of said second fraction catalyst is at least 15 μm.

### Claim 10 (depends on 1, 2, 3, 4, 5, 6, 7, 8, 9)

Process according to any of claims 1 to 9, wherein said polymerization catalyst, is prepared by a process comprising the steps of:
preparing said particulate porous support comprising a first fraction support and a second fraction support wherein said first fraction support differs from said second fraction support in at least one physical parameter, preferably selected from the group comprising median particle diameter, average pore diameter; average pore volume, and surface area;
activating said particulate porous support by reacting said particulate porous support with alumoxane; and
reacting said activated particulate porous support with a metallocene.

### Claim 11 (depends on 1, 2, 3, 4, 5, 6, 7, 8, 9, 10)

Process according to any of claims 1 to 10, wherein said metallocene has formula (I) or (II)
for non-bridged metallocenes;
(Ar)2MQ2 (I)
or
for bridged metallocenes
R″(Ar)2MQ2 (II)
wherein each Ar is independently selected from the group consisting of cyclopentadienyl, indenyl, tetrahydroindenyl, and fluorenyl; and wherein Ar is optionally substituted with one or more substituents each independently selected from the group consisting of halogen, a hydrosilyl, a SiR3 group wherein R is a hydrocarbyl having 1 to 20 carbon atoms, and a hydrocarbyl having 1 to 20 carbon atoms, and wherein said hydrocarbyl optionally contains one or more atoms selected from the group comprising B, Si, S, O, F, Cl, and P;
wherein M is a transition metal selected from the group consisting of titanium, zirconium, hafnium and vanadium;
wherein each Q is independently selected from the group consisting of halogen; a hydrocarboxy having 1 to 20 carbon atoms; and a hydrocarbyl having 1 to 20 carbon atoms wherein said hydrocarbyl optionally contains one or more atoms selected from the group comprising B, Si, S, O, F, Cl and P;
wherein R″ is a bridge between the two Ar and selected from the group consisting of a C1-C20 alkylene, a germanium, a silicon, a siloxane, an alkylphosphine and an amine, wherein said R″ is optionally substituted with one or more substituents each independently selected from the group consisting of halogen, a hydrosilyl, a SiR3 group wherein R is a hydrocarbyl having 1 to 20 carbon atoms, and a hydrocarbyl having 1 to 20 carbon atoms, and wherein said hydrocarbyl optionally contains one or more atoms selected from the group comprising B, Si, S, O, F, Cl and P.

### Claim 12 (depends on 1, 2, 3, 4, 5, 6, 7, 8, 9, 10, 11)

Process according to any of claims 1 to 11, wherein said alumoxane has formula (III) or (IV)
for oligomeric, linear alumoxanes;
R—(Al(R)—O)x—AlR2 (III)
or
for oligomeric, cyclic alumoxanes
(—Al(R)—O—)y (IV)
wherein x is 1-40, y is 3-40, and each R is independently selected from a C1-C8 alkyl.

### Claim 13 (depends on 1, 2, 3, 4, 5, 6, 7, 8, 9, 10, 11, 12)

Process according to any of claims 1 to 12, wherein said metallocene comprises the transition metal zirconium.

### Claim 14 (depends on 1, 2, 3, 4, 5, 6, 7, 8, 9, 10, 11, 12, 13)

Process according to any of claims 1 to 13 wherein said alumoxane is methylalumoxane.