# US 2012/0252977 A1 · Polylactic acid compositions, polylactic acid materials and methods of preparing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2012/0252977 A1
- Document ID: US20120252977A1
- Status: Published application
- Kind: A1
- Application number: 13/432,858
- Filed: 2012-03-28
- Published: 2012-10-04
- Earliest claimed: 2011-03-30
- Assignees: BYD Company Limited
- Inventors: Xueyuan Zhu; Jianghong DOU; Xiaobin HE; Jianghui LI
- Web page: https://patentgrep.com/patent/US20120252977A1

## CPC

- C08L 67/04: Polyesters derived from hydroxycarboxylic acids, e.g. lactones (C08L67/06 takes precedence)
- B29C 48/04: Particle-shaped (making granules B29B9/00)
- B29C 48/92: Measuring, controlling or regulating
- C08L 55/02: ABS [Acrylonitrile-Butadiene-Styrene] polymers
- B29C 2948/9259: Angular velocity
- B29C 2948/92704: Temperature
- B29C 2948/92885: Screw or gear
- B29C 2948/92895: Barrel or housing
- C08L 2205/03: containing three or more polymers in a blend
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)

## Abstract

A polylactic acid composition is provided having a polymer matrix and a compatibilizer. The polymer matrix includes polylactic acids and acrylonitrile-butadiene-styrenes. The compatibilizer is at least one compound selected from the group consisting of: a poly (styrene-ethylene-butadiene-styrene) copolymer grafted with maleic anhydrides, an acrylonitrile-butadiene-styrene copolymer grafted with maleic anhydrides, a polystyrene grafted with maleic anhydrides, and an ethylene-ethyl acrylate-glycidyl methacrylate.

## Claims

### Claim 1

A polylactic acid composition comprising:
a polymer matrix and a compatibilizer,
wherein the polymer matrix includes at least one polylactic acid and at least one acrylonitrile-butadiene-styrene;
wherein the compatibilizer is at least one compound selected from the group consisting of:
a poly (styrene-ethylene-butadiene-styrene) copolymer grafted with maleic anhydrides;
an acrylonitrile-butadiene-styrene copolymer grafted with maleic anhydrides;
a polystyrene grafted with maleic anhydrides; and
an ethylene-ethyl acrylate-glycidyl methacrylate.

### Claim 2 (depends on 1)

The polylactic acid composition according to claim 1, wherein the acylonitrile-butadiene-styrene ranges from about 91 wt. % to about 171 wt. % of the polylactic acid, and the compatibilizer ranges from about 10 wt. % to about 22.2 wt. % of the polylactic acid, based on the total weight of the polylactic acid.

### Claim 3 (depends on 1)

The polylactic acid composition according to claim 1, wherein the polylactic acid composition has a viscometric average molecular weight ranging from about 100,000 to about 750,000, a melting temperature ranging from about 150° C. to about 175° C., and a moisture content of less than about 0.025 wt. %.

### Claim 4 (depends on 2)

The polylactic acid composition according to claim 2, wherein the polylactic acid composition has a viscometric average molecular weight ranging from about 100,000 to about 750,000, a melting temperature ranging from about 150° C. to about 175° C., and a moisture content of less than about 0.025 wt. %.

### Claim 5 (depends on 1)

The polylactic acid composition according to claim 1, wherein the acrylonitrile-butadiene-styrene has a weight average molecular weight ranging from about 50,000 to about 150,000.

### Claim 6 (depends on 1)

The polylactic acid composition according claim 1, wherein the compatibilizer is at least one compound selected from the group consisting of:
a poly (styrene-ethylene-butadiene-styrene) copolymer grafted with maleic anhydrides,
wherein the maleic anhydrides range from about 3 wt. % to about 10 wt. % of the poly (stylene-ethylene-butadiene-stylene) copolymer grafter with maleic anhydrides;
an acrylonitrile-butadiene-styrene copolymer grafted with maleic anhydrides,
wherein the maleic anhydrides range from about 3 wt. % to about 10 wt. % of the acrylonitrile-butadiene-styrene copolymer grafted with maleic anhydrides;
a polystyrene grafted with maleic anhydrides,
wherein the maleic anhydrides range from about 3 wt. % to about 10 wt. % of the polystyrene grafted with maleic anhydrides; and
an ethylene-ethyl acrylate-glycidyl methacrylate.

### Claim 7 (depends on 2)

The polylactic acid composition of claim 2, wherein the compatibilizer is ethylene-ethyl acrylate-glycidyl methacrylate.

### Claim 8 (depends on 7)

The polylactic acid composition of claim 7, wherein the glycidyl methacrylate ranges from about 6 wt. % to about 15 wt. % of the ethylene-ethyl acrylate-glycidyl methacrylate.

### Claim 9 (depends on 1)

The polylactic acid composition according to claim 1, wherein the polylactic acid composition further comprises at least one additive selected from the group consisting of: an antioxidant in an amount ranging from about 0.3 wt. % to about 2 wt. % of the polylactic acids, a hydrolysis resistance agent in an amount ranging from about 0.2 wt. % to about 1.68 wt. % of the polylactic acids, and a shock resistance agent in an amount ranging from about 6.8 wt. % to about 50 wt. % of the polylactic acids.

### Claim 10 (depends on 9)

The polylactic acid composition according to claim 9, wherein the antioxidant is at least one selected compound from the group consisting of: a butyl hydroxy anisd, a dibutyl hydroxyl toluene, a tert-butylhydroquinone, a phenyl diisodecyl phosphate, a pentaerythritol diphosphite, [3-(3,5-dit-butyl-4-hydroxyphenyl)propionic acid]pentaerythriotol, a tri-(2,4-dit-butyl phenyl)phosphate, [β-(3,5-dit-butyl-4-hydroxy phenyl)propionic acid]octadecanoate, tetra[β-(3,5-dit-butyl-4-hydroxy phenyl)propionic acid]pentaerythriotol; the hydrolysis resistance agent is at least one compound selected from the group consisting of: a carbodiimide compound, a isocyanate compound, and a oxazoline compound; and the shock resistance agent is at least one compound selected from the group consisting of a silicon-acrylic resin, and a methyl methacrylate-ethyl acrylate-butyl acrylate copolymer.

### Claim 11 (depends on 1)

A method of preparing a polylactic acid material comprising the steps of:
melting and extruding the polylactic acid composition of claim 1 at a temperature ranging from about 140° C. to about 200° C. to form an extruded polylactic acid composition, and then
granulating and injection molding the extruded polylactic acid composition to form the polylactic acid material.

### Claim 12 (depends on 11)

The method of claim 11 further comprising: drying the polylactic acid material under a pressure ranging from about 0.04 MPa to about 0.08 MPa at a temperature ranging from about 30° C. to about 95° C. before the polyalactic; then melting and extruding the polylactic acid material using a screw having a ratio of length to diameter ranging from about 20 to about 40, the screw having a rotating speed ranging from about 180 to about 230 r/min and under a temperature zone selected from the group consisting of: about 140° C. to about 160° C., about 140° C. to about 170° C., about 140° C. to about 180° C., about 150° C. to about 180° C., about 160° C. to about 180° C., about 170° C. to about 190° C., about 180° C. to about 195° C., about 180° C. to about 195° C., about 190° C. to about 200° C., about 195° C. to about 200° C., and each temperature zone operated under a vacuum degree ranging from about 0.02 MPa to about 0.06 MPa.

### Claim 13 (depends on 11)

A method of claim 11, wherein the acylonitrile-butadiene-styrene ranges from about 91 wt. % to about 171 wt. % of the polylactic acid, and the compatibilizer ranges from about 10 wt. % to about 22.2 wt. % of the polylactic acid, based on the total weight of the polylactic acid.

### Claim 14 (depends on 11)

A method of claim 11, wherein the polylactic acid composition has a viscometric average molecular weight ranging from about 100,000 to about 750,000, a melting temperature ranging from about 150° C. to about 175° C., and a moisture content of less than about 0.025 wt. %.

### Claim 15 (depends on 11)

A method of claim 11, wherein the acrylonitrile-butadiene-styrene has a weight average molecular weight ranging from about 50,000 to about 150,000.

### Claim 16 (depends on 11)

A method of claim 11, wherein the compatibilizer is at least one compound selected from the group consisting of:
a poly (styrene-ethylene-butadiene-styrene) copolymer grafted with maleic anhydrides,
wherein the maleic anhydrides range from about 3 wt. % to about 10 wt. % of the poly (stylene-ethylene-butadiene-stylene) copolymer grafter with maleic anhydrides;
an acrylonitrile-butadiene-styrene copolymer grafted with maleic anhydrides,
wherein the maleic anhydrides range from about 3 wt. % to about 10 wt. % of the acrylonitrile-butadiene-styrene copolymer grafted with maleic anhydrides;
a polystyrene grafted with maleic anhydrides,
wherein the maleic anhydrides range from about 3 wt. % to about 10 wt. % of the polystyrene grafted with maleic anhydrides; and
an ethylene-ethyl acrylate-glycidyl methacrylate.

### Claim 17 (depends on 13)

A method of claim 13, wherein the compatibilizer is ethylene-ethyl acrylate-glycidyl methacrylate.

### Claim 18 (depends on 17)

A method of claim 17, wherein the glycidyl methacrylate ranges from about 6 wt. % to about 15 wt. % of the ethylene-ethyl acrylate-glycidyl methacrylate.

### Claim 19 (depends on 11)

A method of claim 11, wherein the polylactic acid composition further comprises at least one additive selected from the group consisting of: an antioxidant in an amount ranging from about 0.3 wt. % to about 2 wt. % of the polylactic acids, a hydrolysis resistance agent in an amount ranging from about 0.2 wt. % to about 1.68 wt. % of the polylactic acids, and a shock resistance agent in an amount ranging from about 6.8 wt. % to about 50 wt. % of the polylactic acids.

### Claim 20 (depends on 19)

A method of claim 19, wherein the antioxidant is at least one selected compound from the group consisting of: a butyl hydroxy anisd, a dibutyl hydroxyl toluene, a tert-butylhydroquinone, a phenyl diisodecyl phosphate, a pentaerythritol diphosphite, [3-(3,5-dit-butyl-4-hydroxyphenyl)propionic acid]pentaerythriotol, a tri-(2,4-dit-butyl phenyl)phosphate, [β-(3,5-dit-butyl-4-hydroxy phenyl)propionic acid]octadecanoate, tetra[β-(3,5-dit-butyl-4-hydroxy phenyl)propionic acid]pentaerythriotol; the hydrolysis resistance agent is at least one compound selected from the group consisting of: a carbodiimide compound, a isocyanate compound, and a oxazoline compound; and the shock resistance agent is at least one compound selected from the group consisting of: a silicon-acrylic resin, and a methyl methacrylate-ethyl acrylate-butyl acrylate copolymer.