# US 2012/0252955 A1 · Liquid crystal polymer molding and method for producing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2012/0252955 A1
- Document ID: US20120252955A1
- Status: Published application
- Kind: A1
- Application number: 13/425,527
- Filed: 2012-03-21
- Published: 2012-10-04
- Earliest claimed: 2011-03-30
- Assignees: Sumitomo Chemical Company, Limited
- Inventors: Satoshi SEKIMURA; Hiroshi HARADA
- Web page: https://patentgrep.com/patent/US20120252955A1

## CPC

- B29C 45/0025: {Preventing defects on the moulded article, e.g. weld lines, shrinkage marks (preventing defects on the preformed parts or layers B29C45/14836)}
- B29C 45/0013: {using fillers dispersed in the moulding material, e.g. metal particles}
- B29C 45/0046: {Details relating to the filling pattern or flow paths or flow characteristics of moulding material in the mould cavity}
- B29K 2067/00: Use of polyesters {or derivatives thereof}, as moulding material
- B29K 2105/0079: {Liquid crystals}
- B29K 2105/16: Fillers
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS

## Abstract

Provided is a liquid crystal polymer molding in which a weld portion has high strength and also surface properties are satisfactory. A method for producing a liquid crystal polymer molding including a weld portion by injection-molding a liquid crystal polymer composition containing a spherical filler, wherein the spherical filler has a center particle diameter of 60 μm or less, the method including molding so as to satisfy a relation: 20≦[thickness of the weld portion/center particle diameter of the spherical filler]≦55; and a liquid crystal polymer molding obtained by such a method.

## Claims

### Claim 1

A method for producing a liquid crystal polymer molding comprising a weld portion by injection-molding a liquid crystal polymer composition containing a spherical filler, wherein
the spherical filler has a center particle diameter of 60 μm or less, the method comprising molding so as to satisfy a relation:
20≦[thickness of the weld portion/center particle diameter of the spherical filler]≦55.

### Claim 2 (depends on 1)

The method for producing a liquid crystal polymer molding according to claim 1, wherein the liquid crystal polymer is a liquid crystal polyester.

### Claim 3 (depends on 2)

The method for producing a liquid crystal polymer molding according to claim 2, wherein the liquid crystal polyester includes a repeating unit derived from p-hydroxybenzoic acid in the proportion of 30 mol % or more based on the total amount of the whole repeating unit which constitutes the liquid crystal polyester.

### Claim 4 (depends on 1)

The method for producing a liquid crystal polymer molding according to claim 1, wherein injection molding is performed under the conditions that injection acceleration defined by dividing the maximum value of an injection rate by time required to reach the maximum value from initiation of the injection is adjusted to 1,000 to 25,000 mm/sec2, and also the maximum value of injection pressure in a mold inlet is adjusted to 5 to 150 MPa in one injection molding.

### Claim 5 (depends on 1)

The method for producing the liquid crystal polymer molding according to claim 1, wherein injection molding is performed under the conditions that the temperature of the liquid crystal polymer composition at the time of injection is adjusted to [flow initiation temperature of the liquid crystal polymer composition+20° C.] or higher and [flow initiation temperature of the liquid crystal polymer composition+80° C.] or lower.

### Claim 6 (depends on 1)

The method for producing the liquid crystal polymer molding according to claim 1, wherein the temperature of a mold at the time of injection molding is adjusted to 80° C. or higher and [flow initiation temperature of the liquid crystal polymer composition−100° C.] or lower.

### Claim 7 (depends on 1)

A liquid crystal polymer molding obtained by the method according to claim 1.