# US 2012/0252954 A1 · Method for producing a two-dimensional rubber covering and two-dimensional rubber covering

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2012/0252954 A1
- Document ID: US20120252954A1
- Status: Published application
- Kind: A1
- Application number: 13/514,500
- Filed: 2010-10-25
- Published: 2012-10-04
- Earliest claimed: 2009-12-22
- Assignees: Nora Systems GmbH
- Inventors: Gregor Grun; Mario Kroeger
- Web page: https://patentgrep.com/patent/US20120252954A1

## CPC

- C08K 5/0025: {Crosslinking or vulcanising agents; including accelerators}
- C08J 3/203: {Solid polymers with solid and/or liquid additives}
- C08K 3/013: Fillers, pigments or reinforcing additives
- C08J 2321/00: Characterised by the use of unspecified rubbers
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)

## Abstract

A method for producing a two-dimensional rubber covering, in particular a floor covering, comprising the following steps: preparing an unvulcanised rubber material, mixing a filler into the unvulcanised rubber material, converting the rubber material into a two-dimensional state, and crosslinking the rubber material in the two-dimensional state. The method includes that the filler contains particles of glass, porcelain, earthenware and/or stoneware. Also, a covering produced in the described manner.

## Claims

### Claim at position 1

1-13. (canceled)

### Claim 14

A method for producing a two-dimensional rubber covering, in particular a floor covering, comprising the steps:
providing an unvulcanized rubber material,
mixing a filler into the unvulcanized rubber material,
rendering the rubber material into a two-dimensional state, and
crosslinking the rubber material in the two-dimensional state,
wherein the filler contains particles of at least one of glass, porcelain, earthenware and stoneware.

### Claim 15 (depends on 14)

The method according to claim 14, wherein the Mooney viscosity of the unvulcanized rubber material is less than 160 ML (1+4) 100° C. as measured according to DIN standard 53523 after the filler has been admixed into it.

### Claim 16 (depends on 15)

The method according to claim 15, wherein the Mooney viscosity of the unvulcanized rubber material is less than 145 ML (1+4) 100° C. as measured according to DIN standard 53523 after the filler has been admixed into it.

### Claim 17 (depends on 16)

The method according to claim 16, wherein the Mooney viscosity of the unvulcanized rubber material is less than 120 ML (1+4) 100° C. as measured according to DIN standard 53523 after the filler has been admixed into it.

### Claim 18 (depends on 14)

The method according claim 14, wherein the particles of at least one of glass, porcelain, earthenware and stoneware are recycled materials.

### Claim 19 (depends on 14)

The method according to claim 14, wherein the particles of at least one of glass, porcelain, earthenware and/or stoneware are mixed in as a ground-up product.

### Claim 20 (depends on 19)

The method according to claim 19, wherein the d50 value of a grain size of the particles is between 1 μm and 200 μm.

### Claim 21 (depends on 19)

The method according to claim 19, wherein the d50 value of a grain size of the particles is between 1 μm and 20 μm.

### Claim 22 (depends on 14)

The method according to claim 14, wherein the particles of at least one of glass, porcelain, earthenware and stoneware are admixed in a proportion of 10% by weight to 80% by weight, relative to the two-dimensional rubber covering.

### Claim 23 (depends on 14)

The method according to claim 14, wherein the rubber covering is crosslinked with at least one of peroxides, sulfur and additives.

### Claim 24 (depends on 23)

The method according to claim 23, wherein crosslinking with sulfur is accelerated by using crosslinking accelerators or combinations thereof.

### Claim 25 (depends on 24)

The method according to claim 24, wherein, the accelerators contain substances belonging to one or more of the classes of dithiocarbamates, metal salts of dithiocarbamates, thiurams, mercapto accelerators, sulfenamides and guanidines.

### Claim 26 (depends on 14)

The method according to claim 14, wherein the particles have basic properties.

### Claim 27 (depends on 14)

The method according to claim 14, wherein the crosslinking with sulfur is accelerated by using particles of glass.

### Claim 28 (depends on 14)

The method according to claim 14, wherein the rubber material contains at least one of SBR (styrene butadiene rubber), NBR (nitrile butadiene rubber), HNBR (hydrogenated nitrile butadiene rubber), EPDM (ethylene propylene diene rubber), EPM (ethylene propylene rubber), EVA (ethylene vinyl acetate), CSM (chlorosulfonyl polyethylene rubber), CR (chloroprene rubber), VSI (silicone rubber) and AEM (ethylene acrylate rubber).

### Claim 29

A two-dimensional rubber covering into which particles of at least one of glass, porcelain, earthenware and stoneware have been admixed as the filler.