# US 2012/0252945 A1 · Reinforced flame retardant resin composition and molded article

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2012/0252945 A1
- Document ID: US20120252945A1
- Status: Published application
- Kind: A1
- Application number: 13/428,661
- Filed: 2012-03-23
- Published: 2012-10-04
- Earliest claimed: 2011-03-29
- Assignees: Asahi Kasei Chemicals Corporation
- Inventors: Toru YAMAGUCHI; Tomohiro KONDO
- Web page: https://patentgrep.com/patent/US20120252945A1

## CPC

- C08L 69/00: Compositions of polycarbonates; Compositions of derivatives of polycarbonates
- C08K 3/22: of metals
- C08K 3/346: {Clay}
- C08K 3/36: Silica
- C08K 5/523: with hydroxyaryl compounds
- C08L 25/12: with unsaturated nitriles
- C08L 71/12: Polyphenylene oxides
- C08L 25/06: Polystyrene
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)

## Abstract

A reinforced flame retardant resin composition including 20 to 87% by mass of an (A) thermoplastic resin, 3 to 20% by mass of a (B) aromatic phosphoric acid ester-based flame retardant agent, 5 to 40% by mass of (C) mica powder, and 0.5 to 30% by mass of (D) hydrous mineral powder having a dehydration starting temperature for crystallization water in a range of 400 to 600° C.

## Claims

### Claim 1

A reinforced flame retardant resin composition comprising:
20 to 87% by mass of an (A) thermoplastic resin;
3 to 20% by mass of a (B) aromatic phosphoric acid ester-based flame retardant agent;
5 to 40% by mass of (C) mica powder; and
0.5 to 30% by mass of (D) hydrous mineral powder having a dehydration starting temperature for crystallization water in a range of 400 to 600° C.

### Claim 2 (depends on 1)

The reinforced flame retardant resin composition according to claim 1 comprising:
30 to 87% by mass of the (A) component;
3 to 20% by mass of the (B) component;
5 to 30% by mass of the (C) component; and
0.5 to 20% by mass of the (D) component, wherein
a total amount of the (C) component and the (D) component is 10 to 50% by mass.

### Claim 3 (depends on 1)

The reinforced flame retardant resin composition according to claim 1 further comprising:
0.01 to 2 parts by mass of an (E) fluorine-containing dripping preventing agent with respect to 100 parts by mass of a combination of the (A) component, the (B) component, the (C) component, and the (D) component.

### Claim 4 (depends on 1)

The reinforced flame retardant resin composition according to claim 1, wherein the (C) mica powder has an average particle diameter of 10 to 150 μm.

### Claim 5 (depends on 1)

The reinforced flame retardant resin composition according to claim 1, wherein the (D) hydrous mineral powder having a dehydration starting temperature for crystallization water in a range of 400 to 600° C. has an average particle diameter of 0.01 to 100 μm.

### Claim 6 (depends on 1)

The reinforced flame retardant resin composition according to claim 1, wherein the (D) hydrous mineral powder having a dehydration starting temperature for crystallization water in a range of 400 to 600° C. is a chlorite group mineral powder having a dehydration starting temperature for crystallization water in a range of 400 to 600° C.

### Claim 7 (depends on 6)

The reinforced flame retardant resin composition according to claim 6, wherein the (D) hydrous mineral powder having a dehydration starting temperature for crystallization water in a range of 400 to 600° C. is chlorite.

### Claim 8 (depends on 1)

The reinforced flame retardant resin composition according to claim 1, wherein the (D) hydrous mineral powder having a dehydration starting temperature for crystallization water in a range of 400 to 600° C. is boehmite (hydrated alumina).

### Claim 9 (depends on 1)

The reinforced flame retardant resin composition according to claim 1, wherein the (A) component contains 50 to 100% by mass of an (A1) aromatic polycarbonate and 50 to 0% by mass of an (A2) styrene-based resin.

### Claim 10 (depends on 1)

The reinforced flame retardant resin composition according to claim 1, wherein the (A) component contains 50 to 100% by mass of an (A3) polyphenylene ether and 50 to 0% by mass of an (A2) styrene-based resin.

### Claim 11 (depends on 1)

A molded article molded from the reinforced flame retardant resin composition according to claim 1.

### Claim 12 (depends on 1)

A molded chassis molded from the reinforced flame retardant resin composition according to claim 1.

### Claim 13 (depends on 12)

The molded chassis according to claim 12 wherein the molded chassis is a molded chassis for a device having an optical system unit.

### Claim 14

A method of increasing the flame retardance of a resin composition comprising:
combining (D) a hydrous mineral powder having a dehydration starting temperature for crystallization water in a range of 400 to 600° C. with (A) a thermoplastic resin, (B) an aromatic phosphoric acid ester-based flame retardant agent, and (C) mica powder, wherein the flame retardance of the composition of (A), (B), (C), and (D) exhibits a higher flame retardance than a composition of (A), (B), and (C) that excludes (D).

### Claim 15 (depends on 14)

The method according to claim 14, wherein the mass ratio of the (D) hydrous mineral powder to the amount of the (C) mica powder ranges from 1:80 to 6:1.

### Claim 16 (depends on 14)

The method according to claim 14, wherein the (C) mica powder and (D) hydrous mineral powder together comprise less than 60% by mass of the resin composition.