# US 2012/0252940 A1 · System and Method for High Throughput Preparation of Rubber-Modified Asphalt Cement

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2012/0252940 A1
- Document ID: US20120252940A1
- Status: Published application
- Kind: A1
- Application number: 13/493,557
- Filed: 2012-06-11
- Published: 2012-10-04
- Earliest claimed: 2008-09-24
- Assignees: Wright Asphalt Products Company
- Inventors: Theodore P. Flanigan
- Web page: https://patentgrep.com/patent/US20120252940A1

## CPC

- C08L 95/00: Compositions of bituminous materials, e.g. asphalt, tar, pitch
- B28C 7/003: {Heating, e.g. using steam}
- C08J 3/005: {Processes for mixing polymers}
- C08L 21/00: Compositions of unspecified rubbers
- C09D 195/00: Coating compositions based on bituminous materials, e.g. asphalt, tar, pitch
- C08J 2395/00: Bituminous materials, e.g. asphalt, tar or pitch
- C08L 19/003: {Precrosslinked rubber; Scrap rubber; Used vulcanised rubber}
- C08L 2555/22: Asphalt produced above 140°C, e.g. hot melt asphalt
- C08L 2555/34: Recycled or waste materials, e.g. reclaimed bitumen, asphalt, roads or pathways, recycled roof coverings or shingles, recycled aggregate, recycled tires, crumb rubber, glass or cullet, fly or fuel ash, or slag
- C08L 2555/86: Polymers containing aliphatic hydrocarbons only, e.g. polyethylene, polypropylene or ethylene-propylene-diene copolymers
- C08L 2666/08: Homopolymers or copolymers according to C08L7/00 - C08L21/00; Derivatives thereof
- Y02W 30/91: Use of waste materials as fillers for mortars or concrete
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- B28C: PREPARING CLAY; PRODUCING MIXTURES CONTAINING CLAY OR CEMENTITIOUS MATERIAL, e.g. PLASTER (preparing material for foundry moulds B22C5/00)
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)
- Y02W: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO WASTEWATER TREATMENT OR WASTE MANAGEMENT

## Abstract

This invention encompasses rubber modified asphalt cement compositions, as well as systems, apparatuses, methods for preparing, as well as methods for using rubber-modified asphalt cement compositions.

## Claims

### Claim 1

A method for preparing a rubber-modified asphalt cement composition, comprising:
contacting asphalt with rubber granules to form a mixture;
heating the mixture; and
passing the heated mixture through at least one high shear mixer;
wherein the rubber-modified asphalt cement composition comprises an integration value of at least 90.

### Claim 2 (depends on 1)

The method of claim 1, wherein the heating step comprises heating the mixture to a temperature of at least about 500° F.

### Claim 3 (depends on 1)

The method of claim 1, wherein the passing step comprises passing the heated mixture through the at least one high shear mixer for greater than 30 minutes.

### Claim 4

A method for preparing a rubber-modified asphalt cement composition, comprising:
contacting asphalt with rubber granules to form a mixture;
heating the mixture to a temperature of at least about 500° F.; and
passing the heated mixture through at least one high shear mixer for greater than 30 minutes.

### Claim 5 (depends on 5)

The method of claim 5, wherein the rubber-modified asphalt cement composition comprises an integration value of at least 95.

### Claim 6

A method for high throughput preparation of a rubber-modified asphalt cement composition, comprising:
contacting asphalt with at least 40,000 pounds of rubber granules to form a mixture;
heating the mixture; and
passing the heated mixture through at least one high shear mixer;
wherein the rubber-modified asphalt cement composition comprises an integration value of at least 95, and
wherein the method is performed in less than 24 hours.

### Claim 7 (depends on 6)

The method of claim 6, wherein the rubber-modified asphalt cement composition comprising about 65-95 wt. % of asphalt and about 5-35 wt. % of rubber granules.

### Claim 8 (depends on 6)

The method of claim 6, wherein the heating step comprises heating the mixture to a temperature of at least about 500° F.

### Claim 9 (depends on 6)

The method of claim 6, wherein the passing step comprises passing the heated mixture through the at least one high shear mixer for greater than 30 minutes.

### Claim 10

A rubber-modified asphalt cement composition prepared by:
contacting asphalt with rubber granules to form a mixture;
heating the mixture; and
passing the heated mixture through at least one high shear mixer;
wherein the rubber-modified asphalt cement composition comprises an integration value of at least 95.

### Claim 11 (depends on 10)

The composition of claim 10, wherein the mixture is heated to a temperature greater than 500° F.

### Claim 12 (depends on 10)

The composition of claim 10, wherein the heated mixture is passed through the at least one high shear mixer for greater than 30 minutes.

### Claim 13 (depends on 10)

The composition of claim 10, wherein the rubber-modified asphalt cement composition comprises about 65-95 wt. % of asphalt and about 5-35 wt. % of rubber granules.

### Claim 14

A system for preparing a rubber-modified asphalt cement composition, comprising:
an asphalt charging device for charging asphalt into the system;
a rubber charging device for charging rubber granules into the system;
at least one heater for heating the charged asphalt, the charged rubber granules, or a mixture thereof;
at least one high shear mixer for mixing the charged asphalt and charged rubber granules into a rubber-modified asphalt cement composition; and
a controller for controlling the asphalt charging device, the rubber charging device, and/or the at least one high shear mixer, in a manner such that the rubber-modified asphalt cement composition has an integration factor of at least 95.

### Claim 15 (depends on 14)

The system of claim 14, wherein the system is capable of high throughput production in less than 24 hours of a rubber-modified asphalt cement composition comprising at least 40,000 pounds of rubber granules, wherein the composition has an integration value of at least 95.

### Claim 16 (depends on 14)

The system of claim 14, wherein the controller is a semi-automatic controller.

### Claim 17 (depends on 14)

The system of claim 14, wherein the controller is an automatic controller.