# US 2012/0252939 A1 · Asphaltic compositions, filled asphaltic materials, and methods for making asphaltic compositions

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2012/0252939 A1
- Document ID: US20120252939A1
- Status: Published application
- Kind: A1
- Application number: 13/434,711
- Filed: 2012-03-29
- Published: 2012-10-04
- Earliest claimed: 2011-04-04
- Assignees: Honeywell International Inc.
- Inventors: Scott Hacker; Yonghong Ruan; Ho-Nan Sung; Richard Heath
- Web page: https://patentgrep.com/patent/US20120252939A1

## CPC

- C08L 95/00: Compositions of bituminous materials, e.g. asphalt, tar, pitch
- C08L 23/0853: Ethylene vinyl acetate copolymers
- C08L 2205/03: containing three or more polymers in a blend
- C08L 2555/22: Asphalt produced above 140°C, e.g. hot melt asphalt
- C08L 2555/52: Aggregate, e.g. crushed stone, sand, gravel or cement
- C08L 2555/80: Macromolecular constituents
- C08L 2555/84: Polymers comprising styrene, e.g. , polystyrene, styrene-diene copolymers or styrene-butadiene-styrene copolymers
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)

## Abstract

An asphaltic composition comprises base asphalt and a low molecular weight ethylene vinyl acetate copolymer. The low molecular weight ethylene vinyl acetate copolymer is present in an amount of from about 0.1 to about 5 wt. % of the base asphalt.

## Claims

### Claim 1

An asphaltic composition comprising:
base asphalt; and
a low molecular weight ethylene vinyl acetate copolymer present in an amount of from about 0.1 to about 5 wt. % of the base asphalt.

### Claim 2 (depends on 1)

The asphaltic composition according to claim 1, wherein the low molecular weight ethylene vinyl acetate copolymer is present in an amount of from about 0.5 to about 2 wt. % of the base asphalt.

### Claim 3 (depends on 1)

The asphaltic composition according to claim 1, wherein the low molecular weight ethylene vinyl acetate copolymer has a vinyl acetate content of from about 1 to about 40 wt. % of the low molecular weight ethylene vinyl acetate copolymer.

### Claim 4 (depends on 1)

The asphaltic composition according to claim 1, wherein the low molecular weight ethylene vinyl acetate copolymer has a vinyl acetate content of from about 5 to about 15 wt. % of the low molecular weight ethylene vinyl acetate copolymer.

### Claim 5 (depends on 1)

The asphaltic composition according to claim 1, wherein the low molecular weight ethylene vinyl acetate copolymer has a molecular weight of from about 1,000 to about 200,000 Daltons.

### Claim 6 (depends on 1)

The asphaltic composition according to claim 1, wherein the low molecular weight ethylene vinyl acetate copolymer has a molecular weight of from about 1,000 to about 50,000 Daltons.

### Claim 7 (depends on 1)

The asphaltic composition according to claim 1, wherein the low molecular weight ethylene vinyl acetate copolymer has a molecular weight of from about 5,000 to about 20,000 Daltons.

### Claim 8 (depends on 1)

The asphaltic composition according to claim 1, further comprising a high temperature performance additive that is present in an amount of from about 0.5 to about 12 wt. % of a base asphalt.

### Claim 9 (depends on 8)

The asphaltic composition according to claim 8, wherein the high temperature performance additive comprises an elastomers, a plastomers, or a combination thereof.

### Claim 10

A filled asphaltic material comprising:
an asphaltic composition present in an amount of about 3 to about 99 wt. % of the filled asphaltic material, the asphaltic composition comprising base asphalt and a low molecular weight ethylene vinyl acetate copolymer that is present in an amount of from about 0.1 to about 5 wt. % of the base asphalt; and
an inorganic filler present in an amount of from about 1 to about 97 wt. % of the filled asphaltic material.

### Claim 11 (depends on 10)

The filled asphaltic material according to claim 10, wherein the asphaltic composition is present in an amount of from about 3 to about 8 wt. % of the filled asphaltic material, and the inorganic filler is aggregate that is present in an amount of from about 92 to about 97 wt. % of the filled asphaltic material.

### Claim 12 (depends on 11)

The filled asphaltic material according to claim 11, wherein the asphaltic composition further comprises one or more high temperature performance additives that are present in an amount of from about 0.5 to about 5 wt. % of a base asphalt.

### Claim 13 (depends on 10)

The filled asphaltic material according to claim 10, wherein the asphaltic composition is present in an amount of from about 30 to about 99 wt. % of the filled asphaltic material, and the inorganic filler is mineral filler that is present in an amount of from about 1 to about 70 wt. % of the filled asphaltic material.

### Claim 14 (depends on 13)

The filled asphaltic material according to claim 13, wherein the asphaltic composition further comprises one or more high temperature performance additives that are present in an amount of from about 4 to about 12 wt. % of a base asphalt.

### Claim 15

A method for making an asphaltic composition, the method comprising the step of combining a low molecular weight ethylene vinyl acetate copolymer and base asphalt at an elevated temperature to form the asphaltic composition, wherein the low molecular weight ethylene vinyl acetate copolymer is present in an amount of from about 0.1 to about 5 wt. % of the base asphalt.

### Claim 16 (depends on 15)

The method according to claim 15, further comprising the step of combining a high temperature performance additive and the base asphalt, wherein the high temperature performance additive is present in an amount of from about 0.5 to about 12 wt. % of a base asphalt.

### Claim 17 (depends on 16)

The method according to claim 16, wherein the high temperature performance additive and the low molecular weight ethylene vinyl acetate copolymer are combined together to form a low and high end temperature performance blend prior to the steps of combining the low molecular weight ethylene vinyl acetate copolymer and combining the high temperature performance additive, and wherein the steps of combining the low molecular weight ethylene vinyl acetate copolymer and combining the high temperature performance additive both include mixing the low and high end temperature performance blend with the base asphalt.

### Claim 18 (depends on 17)

The method according to claim 17, wherein the low and high end temperature performance blend is a physical mixture, a melt blend, or a cooled shaped melt blend.

### Claim 19 (depends on 16)

The method according to claim 16, wherein step of combining the high temperature performance additive begins prior to the step of combining the low molecular weight ethylene vinyl acetate copolymer.

### Claim 20 (depends on 16)

The method according to claim 16, wherein the step of combining the low molecular weight ethylene vinyl acetate copolymer begins prior to the step of combining a high temperature performance additive.