# US 2012/0252934 A1 · Microcapsule Corrosion Control In Reinforced Concrete

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2012/0252934 A1
- Document ID: US20120252934A1
- Status: Published application
- Kind: A1
- Application number: 13/139,583
- Filed: 2011-03-29
- Published: 2012-10-04
- Earliest claimed: 2011-03-29
- Assignees: Empire Technology Development LLC
- Inventors: Seth Miller; Thomas A. Yager
- Web page: https://patentgrep.com/patent/US20120252934A1

## CPC

- C04B 40/0633: {Chemical separation of ingredients, e.g. slowly soluble activator}
- B01J 13/043: {Drying and spraying}
- C04B 20/1033: {obtained by reactions only involving carbon-to-carbon unsaturated bonds}
- C04B 28/02: containing hydraulic cements other than calcium sulfates
- C04B 2103/0094: {Agents for altering or buffering the pH; Ingredients characterised by their pH}
- C04B 2111/00112: {Mixtures characterised by specific pH values}
- C04B 2111/26: Corrosion of reinforcement resistance
- Y10T 428/2998: including synthetic resin or polymer
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

Corrosion control in reinforced concrete is generally disclosed. Some example embodiments may include concrete including aggregate, cement, and/or microcapsules distributed within the cement, where the individual microcapsules may include a high pH salt substantially contained within an acid-soluble shell. If the pH of the concrete decreases, the acid soluble shell may swell and/or dissolve, such as below a pH of about 11, which may release the high pH salt. The high pH salt may locally increase the pH of the concrete. By increasing the pH above about pH 11, corrosion of steel rebar may be prevented and/or reduced.

## Claims

### Claim 1

A concrete structure comprising:
aggregate;
cement interposing and bonding the aggregate; and
a plurality of microcapsules distributed within the cement, individual microcapsules comprising a high pH salt substantially contained within an acid-soluble shell.

### Claim 2 (depends on 1)

The structure of claim 1, wherein the high pH salt comprises one or more of a hydroxide, a phosphate, and a carbonate.

### Claim 3 (depends on 1)

The structure of claim 1, wherein the high pH salt comprises one or more of sodium hydroxide and sodium carbonate.

### Claim 4 (depends on 1)

The structure of claim 1, wherein the shell comprises an acid-soluble polymer.

### Claim 5 (depends on 1)

The structure of claim 1, wherein the shell comprises a polymer comprising imidazoline subunits.

### Claim 6 (depends on 5)

The structure of claim 5, wherein the polymer comprising imidazoline subunits comprises about 20% to about 30% imidazoline and about 70% to about 80% styrene.

### Claim 7 (depends on 1)

The structure of claim 1, wherein the shell is substantially insoluble in water above about pH 12 and is at least partially soluble in water below about pH 11.

### Claim 8 (depends on 1)

The structure of claim 1, wherein the microcapsules comprise about 0.1% to about 10% of the cement by volume.

### Claim 9 (depends on 1)

The structure of claim 1, wherein the microcapsules comprise about 1% to about 5% of the cement by volume.

### Claim 10 (depends on 1)

The structure of claim 1, wherein a ratio by weight of the high pH salt to the cement is about 0.0001:1 to about 0.0020:1.

### Claim 11 (depends on 1)

The structure of claim 1, wherein a ratio by weight of the high pH salt to the cement is about 0.0001:1.

### Claim 12 (depends on 1)

The structure of claim 1, wherein a ratio by weight of the high pH salt to the cement is about 0.0005:1.

### Claim 13 (depends on 1)

The structure of claim 1, wherein a ratio by weight of the high pH salt to the cement is about 0.0010:1.

### Claim 14 (depends on 1)

The structure of claim 1, further comprising one or more steel reinforcing bars.

### Claim 15

An additive for concrete, the additive comprising:
a plurality of microcapsules, individual microcapsules comprising an acid-soluble shell substantially enclosing a core comprising a pH adjustment material.

### Claim 16 (depends on 15)

The additive of claim 15, wherein the acid-soluble shell is substantially insoluble in water above about pH 12 and is at least partially soluble in water below about pH 11.

### Claim 17 (depends on 15)

The additive of claim 15, wherein the pH adjustment material comprises a high pH salt.

### Claim 18 (depends on 15)

The additive of claim 15, wherein individual microcapsules are about 10 μm to about 500 μm in size.

### Claim 19 (depends on 15)

The additive of claim 15, wherein individual microcapsules are about 100 μm to about 250 μm in size.

### Claim 20 (depends on 15)

The additive of claim 15, wherein the high pH salt comprises one or more of a hydroxide, a phosphate, and a carbonate.

### Claim 21 (depends on 15)

The additive of claim 15, wherein the high pH salt comprises one or more of sodium hydroxide and sodium carbonate.

### Claim 22 (depends on 15)

The additive of claim 15, wherein the shell comprises an acid-soluble polymer.

### Claim 23 (depends on 15)

The additive of claim 15, wherein the shell comprises poly(imidazoline).

### Claim 24

A method of preparing concrete, the method comprising:
combining cement, aggregate, and a plurality of microcapsules;
wherein individual microcapsules comprise a shell substantially enclosing a core comprising a high pH salt, the shell being substantially insoluble in water above about pH 12 and at least partially soluble in water below about pH 11.

### Claim 25 (depends on 24)

The method of claim 24, wherein combining the cement, the aggregate, and the plurality of microcapsules includes combining the cement, the aggregate, and the plurality of microcapsules with water to form a pourable mixture.

### Claim at position 26

26-27. (canceled)

### Claim 28 (depends on 24)

The method of claim 24, wherein combining the cement, the aggregate, and the plurality of microcapsules comprises combining the cement, the aggregate, and the plurality of microcapsules such that the plurality of microcapsules comprise about 1% to about 5% of the total volume of the cement, the aggregate, and the plurality of microcapsules.

### Claim 29 (depends on 24)

The method of claim 24, wherein combining the cement, the aggregate, and the plurality of microcapsules comprises combining the cement, the aggregate, and the plurality of microcapsules such that a ratio by weight of the high pH salt to the cement is about 0.0001:1 to about 0.0020:1.

### Claim at position 29

30-32. (canceled)

### Claim 33

A cement mixture comprising:
a hydraulic cement; and
a plurality of microcapsules dispersed in the hydraulic cement;
wherein individual microcapsules comprise a shell substantially enclosing a core comprising a high pH salt, the shell being substantially insoluble in water above about pH 12 and at least partially soluble in water below about pH 11.

### Claim 34 (depends on 33)

The cement mixture of claim 33, wherein the high pH salt comprises one or more of a hydroxide, a phosphate, and a carbonate.

### Claim 35 (depends on 33)

The cement mixture of claim 33, wherein the shell comprises an acid-soluble polymer.