# US 2012/0252932 A1 · Composite forming material

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2012/0252932 A1
- Document ID: US20120252932A1
- Status: Published application
- Kind: A1
- Application number: 13/486,173
- Filed: 2012-06-01
- Published: 2012-10-04
- Earliest claimed: 2010-03-08
- Assignees: Mag-Isover K.K.
- Inventors: Shuji SANO; Masaya TSUKAMOTO; Kenichiro TERAGAMI; Toru MURAKAMI
- Web page: https://patentgrep.com/patent/US20120252932A1

## CPC

- B29C 45/0005: {using fibre reinforcements}
- C08J 5/043: {with glass fibres}
- C08K 7/20: Glass
- C08K 9/06: with silicon-containing compounds
- B29K 2309/08: Glass
- C08K 9/04: Ingredients treated with organic substances {(treated with macromolecular compounds C08K9/08)}
- C08K 2201/003: Additives being defined by their diameter
- C08K 2201/004: Additives being defined by their length
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS

## Abstract

A composite forming material of the present invention in which a fiberglass and a thermoplastic resin are compounded, where the fiberglass is a glass wool and a surface treatment is performed on the glass wool by spraying a solution which includes a silane coupling agent and/or a film former, a weight percent of the silane coupling agent to the glass wool is 0.24 wt %, and a weight percent of the film former to the glass wool is 2.4 wt %, the mean length of the glass wool is 600 μm, and the diameter is 3.4 μm.

## Claims

### Claim 1

A composite forming material characterized that a fiberglass and a thermoplastic resin are mixed, and the fiberglass is glass wool.

### Claim 2 (depends on 1)

A composite forming material according to claim 1, a surface treatment is performed on the glass wool by spraying a solution which includes a silane coupling agent and/or a film former.

### Claim 3 (depends on 2)

A composite forming material according to claim 2, the weight percent of the silane coupling agent to the glass wool is 0.24 wt %, and the weight percent of the film former to the glass wool is 2.4 wt %.

### Claim 4 (depends on 1)

A composite forming material according to claim 1, the mean length of the glass wool is 600 μm, and the diameter is 3.4 μm.

### Claim 5 (depends on 2)

A composite forming material according to claim 2, the mean length of the glass wool is 600 μm, and the diameter is 3.4 μm.

### Claim 6 (depends on 3)