# US 2012/0252910 A1 · Method for Producing Improved Rubberized Concrete using Waste Rubber Tires

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2012/0252910 A1
- Document ID: US20120252910A1
- Status: Published application
- Kind: A1
- Application number: 13/078,913
- Filed: 2011-04-01
- Published: 2012-10-04
- Earliest claimed: 2011-04-01
- Assignees: Chun Well Industry Co., Ltd.
- Inventors: Kuo-Ji Yen; Maw-Tien Lee; Liang-Hsign Chou; Jen-Ray Chang
- Web page: https://patentgrep.com/patent/US20120252910A1

## CPC

- C04B 28/02: containing hydraulic cements other than calcium sulfates
- C04B 18/22: Rubber {, e.g. ground waste tires}
- C08J 11/10: by chemically breaking down the molecular chains of polymers or breaking of crosslinks, e.g. devulcanisation (depolymerisation to the original monomer C07)
- C08J 2319/00: Characterised by the use of rubbers not provided for in groups C08J2307/00 - C08J2317/00
- C08L 19/003: {Precrosslinked rubber; Scrap rubber; Used vulcanised rubber}
- Y02W 30/62: Plastics recycling; Rubber recycling
- Y02W 30/91: Use of waste materials as fillers for mortars or concrete
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- Y02W: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO WASTEWATER TREATMENT OR WASTE MANAGEMENT

## Abstract

Partial oxidation of crumb rubber derived from environmental hazardous waste tires yields surface treated crumb rubber and a gas condensate which are used as blending stocks for making rubberized concrete with substantially improved mechanical strength as compared to the conventional rubberized concrete. The chemically more active rubber surface becomes hydrophilic, so it interacts with the hydrophilic surface of surrounding cement matrix much stronger. The gas condensate co-produced in the partial oxidation reactor consists of mainly active sulfur oxides (R—SOx—R) and serves as an excellent bonding agent to further enhance the bonding strength between the partially oxidized rubber particles and the cement mixes. The mechanically improved rubberized concrete is more versatile than conventional rubberized concrete.

## Claims

### Claim 1

A concrete composition that comprises cement and crumb rubber particles that are partially oxidized and have sulfur-containing, hydrophilic reactive functional groups.

### Claim 2 (depends on 1)

The concrete composition of claim 1 wherein the functional groups are reactive to hydrophilic groups present in cement matrix and are selected from the group consisting of sulfoxides (R—SO—R), sulfones (R—SO2—R), sulfur trioxides (R—SO3) and mixtures thereof, wherein R represents hydrocarbons of the rubber particles.

### Claim 3 (depends on 1)

The concrete composition of claim 1 further comprising a liquid bonding agent that contains a functional group that is selected from the group consisting of sulfoxides, sulfones, sulfur trioxides and mixtures thereof.

### Claim 4 (depends on 3)

The concrete composition of claim 3 wherein the liquid bonding agent comprises at least 0.1 wt % of the concrete composition.

### Claim 5 (depends on 4)

The concrete composition of claim 4 wherein the liquid bonding agent comprises from 0.1 to 1.0 wt % of the concrete composition.

### Claim 6 (depends on 1)

The concrete composition of claim 1 wherein the crumb rubber particles comprises 0.1 to 20 wt % of the concrete composition.

### Claim 7 (depends on 6)

The concrete composition of claim 6 wherein the crumb rubber comprises from 3 wt % to 7.5 wt % of the concrete composition.

### Claim 8 (depends on 1)

The concrete composition of claim 1 wherein the concrete composition when cured has a compressive strength of at least 40 MPa.

### Claim 9 (depends on 1)

The concrete composition of claim 1 wherein the concrete composition when cured has a flexural strength of at least 5.4 MPa.

### Claim 10 (depends on 1)

The concrete composition of claim 1 wherein the concrete composition when cured has a tensile strength of at least 2.9 MPa.

### Claim 11

A concrete composition comprising cement, rubber particles that are partially oxidized and having surface-active functional groups that are selected group the group consisting of sulfoxides (R—SO—R), sulfones (R—SO2—R), sulfur trioxides (R—SO3) and mixtures thereof, and a bonding agent that is gas condensate that is formed by partially oxidizing crumb rubber in the presence of oxygen gas, wherein R represents hydrocarbons of the rubber particles.

### Claim 12 (depends on 11)

The concrete composition of claim 11 wherein the bonding agent comprises at least 0.1 wt % of the concrete composition.

### Claim 13 (depends on 12)

The concrete composition of claim 12 wherein the liquid bonding agent comprises from 0.1 to 1.0 wt % of the concrete composition.

### Claim 14 (depends on 11)

The concrete composition of claim 11 wherein the crumb rubber particles comprise 0.1 to 20 wt % of the concrete composition.

### Claim 15 (depends on 14)

The concrete composition of claim 14 wherein the liquid bonding agent comprises from 3 wt % to 7.5 wt % of the concrete composition.

### Claim 16 (depends on 11)

The concrete composition of claim 11 wherein the concrete composition when cured has a compressive strength of at least 40 MPa.

### Claim 17 (depends on 11)

The concrete composition of claim 11 wherein the concrete composition when cured has a flexural strength of at least 5.4 MPa.

### Claim 18 (depends on 11)

The concrete composition of claim 11 wherein the concrete composition when cured has a tensile strength of at least 2.9 MPa.

### Claim 19 (depends on 11)

The concrete composition of claim 11 that does not include a superplastizer.

### Claim 20

A method of producing partially oxidized rubber particles and binding agents, which are suitable for use as concrete components, that comprises heating rubber particles in the presence of oxygen to partially oxidize the rubber particles such that the surface of the particles form functional groups that are selected from the group consisting of the sulfoxides (R—SO—R), sulfones (R—SO2—R), sulfur trioxides (R—SO3) and mixtures thereof, wherein R represents hydrocarbons of the rubber particles, and to form a gas condensate that serves a binding agent for the concrete.

### Claim 21 (depends on 20)

The method of claim 20 comprising the steps of:
(a) heating the rubber particles in a mixture of oxygen and an inert gas to a temperature and for a sufficient length of time to partially oxidize the rubber particles and generate a gaseous by-product; and
(b) cooling the oxidized rubber particles and gaseous by-product; and
(c) recovering the oxidized rubber particles and a gas condensate.

### Claim 22 (depends on 20)

The method of claim 20 comprising the steps of:
(a) introducing a feed containing crumb rubber particles into an upper portion of a continuous reactor at or near the top at a rate sufficient to establish a desired residence time within the reactor;
(b) preheating a gas mixture of air and an inert gas to a temperature sufficient to initiate and maintain partial oxidation of the rubber particles;
(c) introducing the preheated gas mixture into a lower portion of the reactor;
(d) withdrawing partially oxidized rubber particles from the reactor; and
(e) collecting the gas condensate from an overhead cooler of the reactor.

### Claim 23 (depends on 20)

The method of claim 20 wherein the rubber particles are recovered from waste tires, mechanically grounded and screened into irregular particles with desirable sizes in the range of 100 to 1,000 μm.

### Claim 24 (depends on 20)

The method of claim 20 wherein the size of the rubber particles ranges from 300 to 600 μm.

### Claim 25 (depends on 20)

The method of claim 20 comprising heating the rubber particles in a mixture of air and nitrogen that has a volume ratio of air to nitrogen (A/N) in the range of 5/1 to 1/7.

### Claim 26 (depends on 25)

The method of claim 25 wherein the A/N is in the range of 1/2 to 1/5.

### Claim 27 (depends on 20)

The method of claim 20 comprising heating the rubber particles to a temperature in the ranges from 100 to 500° C.

### Claim 28 (depends on 27)

The method of claim 27 wherein the temperature ranges from 200 to 300° C.

### Claim 29 (depends on 20)

The method of claim 20 comprising heating the rubber particles for 30 minutes to 3 hours.

### Claim 30 (depends on 29)

The method of claim 29 comprising heating the rubber particles for 45 minutes to 2 hours.

### Claim 31 (depends on 20)

The method of claim 20 wherein the gas condensate comprises a water-soluble component and a water-insoluble component.