# US 2012/0252676 A1 · Extremely Low Resistance Compositions and Methods for Creating Same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2012/0252676 A1
- Document ID: US20120252676A1
- Status: Published application
- Kind: A1
- Application number: 13/076,188
- Filed: 2011-03-30
- Published: 2012-10-04
- Earliest claimed: 2011-03-30
- Assignees: Ambature, Inc.
- Inventors: Douglas J. Gilbert; Timothy S. Cale
- Web page: https://patentgrep.com/patent/US20120252676A1

## CPC

- H10N 60/858: {having multilayered structures, e.g. superlattices}
- H10N 60/0296: {Processes for depositing or forming copper oxide superconductor layers}
- H10N 60/0661: {Processes performed after copper oxide formation, e.g. patterning}
- Y10T 428/31678: Of metal
- H10N: ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

The invention pertains to creating new extremely low resistance (“ELR”) materials, which may include high temperature superconducting (“HTS”) materials. In some implementations of the invention, an ELR material may be modified by depositing a layer of modifying material unto the ELR material to form a modified ELR material. The modified ELR material has improved operational characteristics over the ELR material alone. Such operational characteristics may include operating at increased temperatures or carrying additional electrical charge or other operational characteristics. In some implementations of the invention, the ELR material is a cuprate-perovskite, such as, but not limited to BSSCO. In some implementations of the invention, the modifying material is a conductive material that bonds easily to oxygen, such as, but not limited to, chromium.

## Claims

### Claim 1

A composition comprising:
a first layer comprising BSSCO; and
a second layer comprising a modifying material, wherein the modifying material of the second layer is bonded to the BSSCO of the first layer, wherein the modifying material comprises an element selected from the group consisting of: chromium, copper, bismuth, cobalt, vanadium, titanium, rhodium, beryllium, gallium, selenium, and silver.

### Claim 2 (depends on 1)

The composition of claim 1, wherein the modifying material of the second layer is bonded to a face of the BSSCO of the first layer, wherein the face is not substantially perpendicular to a c-axis of the BSSCO.

### Claim 3 (depends on 1)

The composition of claim 1, wherein the modifying material of the second layer is bonded to a face of the BSSCO of the first layer, wherein the face is substantially perpendicular to any line in an “a-b” face of the BSSCO.

### Claim 4 (depends on 1)

The composition of claim 1, wherein the modifying material of the second layer is bonded to a face of the BSSCO of the first layer, wherein the face is substantially perpendicular to a b-axis of the BSSCO.

### Claim 5 (depends on 1)

The composition of claim 1, wherein the modifying material of the second layer is bonded to a face of the BSSCO of the first layer, wherein the face is substantially perpendicular to an a-axis of the BSSCO.

### Claim 6 (depends on 1)

The composition of claim 1, wherein the modifying material of the second layer is bonded to a face of the BSSCO of the first layer, wherein the face is substantially parallel to the c-axis.

### Claim 7 (depends on 1)

The composition of claim 1, wherein the composition has improved operating characteristics over those of BSSCO.

### Claim 8 (depends on 1)

The composition of claim 1, wherein the composition operates at a higher temperature than that of BSSCO.

### Claim 9 (depends on 8)

The composition of claim 8, wherein the composition demonstrates extremely low resistance at a higher temperature than that of BSSCO.

### Claim 10 (depends on 8)

The composition of claim 8, wherein the composition transitions from a non-ELR state to a ELR state at a temperature higher than that of BSSCO.

### Claim 11 (depends on 1)

The composition of claim 1, wherein the composition has a transition temperature greater than that of BSSCO.

### Claim 12 (depends on 8)

The composition of claim 8, wherein the composition operates at a temperature greater than any one of the following temperatures: 100K, 150K, 200K, 250K, or 300K.

### Claim 13 (depends on 1)

The composition of claim 1, wherein the composition carries a greater amount of current in an ELR state than that carried by BSSCO in its ELR state.

### Claim 14 (depends on 1)

The composition of claim 1, wherein the second layer is deposited onto the first layer.

### Claim 15 (depends on 1)

The composition of claim 1, wherein the first layer is deposited onto the second layer.

### Claim 16 (depends on 1)

The composition of claim 1, wherein the BSSCO of the first layer is formed on the second layer.

### Claim 17

A method comprising:
bonding a modifying material to a face of BSSCO, wherein the modifying material comprises an element selected from the group consisting of: chromium, copper, bismuth, cobalt, vanadium, titanium, rhodium, beryllium, gallium, selenium, and silver.

### Claim 18 (depends on 17)

The method of claim 17, wherein the face of the BSSCO is not substantially perpendicular to a c-axis of the BSSCO.

### Claim 19 (depends on 17)

The method of claim 17, wherein bonding a modifying material to a face of BSSCO comprises depositing the modifying material onto the BSSCO.

### Claim 20 (depends on 17)

The method of claim 17, wherein bonding a modifying material to a face of BSSCO comprises forming the BSSCO on the modifying material.

### Claim 21 (depends on 17)

The method of claim 17, wherein bonding a modifying material to a face of BSSCO comprises bonding a first layer comprising the modifying material to a second layer comprising the BSSCO.

### Claim 22

A composition comprising:
a first layer comprising BSSCO; and
a second layer comprising a modifying material, wherein the modifying material of the second layer is bonded to the BSSCO of the first layer, wherein the modifying material is a conductive material that bonds easily with oxygen.

### Claim 23 (depends on 22)

The composition of claim 22, wherein the modifying material is an element selected from the group consisting of: chromium, copper, bismuth, cobalt, vanadium, titanium, rhodium, beryllium, gallium, selenium, and silver.

### Claim 24

A method comprising:
bonding a modifying material to a face of an HTS perovskite material, wherein the HTS perovskite is BSSCO, wherein the modifying material comprises an element selected from the group consisting of: chromium, copper, bismuth, cobalt, vanadium, titanium, rhodium, beryllium, gallium, selenium, and silver.

### Claim 25

A composition comprising:
a first layer comprising an extremely low resistance material, wherein the extremely low resistance material is BSSCO;
a second layer comprising a modifying material, wherein the second layer is bonded to the first layer;
a third layer comprising the extremely low resistance material; and
a fourth layer of the modifying material, wherein the third layer is bonded to the fourth layer.