- Published: 2012-10-04
- Earliest claimed: 2011-03-28
- Assignees: Specialty Minerals (Michigan) Inc.
- Inventors: Angela Rodrigues-Schroer; Ronald Warren Schmidt
- Web page: https://patentgrep.com/patent/US20120252653A1

## CPC

- C04B 14/00: Use of inorganic materials as fillers, e.g. pigments, for mortars, concrete or artificial stone; Treatment of inorganic materials specially adapted to enhance their filling properties in mortars, concrete or artificial stone (expanding or defibrillating materials C04B20/00)
- C04B 28/06: Aluminous cements (monolithic refractories or refractory mortars C04B35/66)
- C04B 35/66: Monolithic refractories or refractory mortars, including those whether or not containing clay {(making or repairing of linings F27D1/16)}
- C04B 40/0039: {Premixtures of ingredients}
- C04B 2103/12: Set accelerators
- C04B 2111/00155: {Sprayable, i.e. concrete-like, materials able to be shaped by spraying instead of by casting, e.g. gunite}
- C04B 2111/28: Fire resistance, i.e. materials resistant to accidental fires or high temperatures
- Y02W 30/91: Use of waste materials as fillers for mortars or concrete
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- Y02W: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO WASTEWATER TREATMENT OR WASTE MANAGEMENT

## Abstract

The present invention relates to a setting agent accelerator for use with an ultra-low cement, low cement and regular castable refractory materials and a method of applying the refractory materials using the setting agent accelerator to form a refractory structure or lining. More particularly, the invention is directed to a setting agent accelerator for use with an ultra-low cement , low cement and regular castable refractory material for preserving or maintaining the safety lining and the working lining of refractory structures or linings from mechanical erosion and/or attack by corrosive materials such as those produced during manufacture of cement, lime, metals or metal alloys including acid and basic slags. The setting agent accelerator has a set accelerating amount of sodium nitrate, sodium nitrite or mixtures thereof, calcium hydroxide and water.

## Claims

### Claim 1

A setting agent accelerator for reducing the set time of a castable refractory comprising:
a first component from the group consisting of a set accelerating amount of sodium nitrate, sodium nitrite and mixtures thereof;
calcium hydroxide; and
water.

### Claim 2 (depends on 1)

The setting agent accelerator for reducing the set time of a castable refractory of claim 1 wherein the first component is sodium nitrate.

### Claim 3 (depends on 1)

The setting agent accelerator for reducing the set time of a castable refractory of claim 1 wherein the first component is sodium nitrite.

### Claim 4 (depends on 1)

The setting agent accelerator for reducing the set time of a castable refractory of claim 1 wherein the first component is a mixture of sodium nitrate and sodium nitrite.

### Claim 5 (depends on 1)

The setting agent accelerator for reducing the set time of a castable refractory of claim 1 wherein:
the first component is present in an amount from 30 to 60 weight percent;
and the calcium hydroxide is present in the amount of 10 to 30 weight percent;
and water is present in the amount of 30 to 60 weight percent.

### Claim 6 (depends on 1)

The setting agent accelerator for reducing the set time of a castable refractory of claim 1 wherein the
first component is present in an amount of from 35 to 45 weight percent;
and the calcium hydroxide is present in the amount of from 12 to 18 weight percent;
and water is present in the amount of from 45 to 55 weight percent.

### Claim 7 (depends on 1)

The setting agent accelerator for reducing the set time of a castable refractory of claim 1 wherein the pH of the setting agent accelerator is from 11 to 13.

### Claim 8 (depends on 5)

The setting agent accelerator for reducing the set time of a castable refractory of claim 5 wherein the pH of the setting agent accelerator is less than 12.4

### Claim 9

A process for placing a castable refractory comprising the steps of:
providing a first composition comprising a castable refractory;
forming an admixture by admixing the first composition with a second composition comprising a setting agent accelerator comprising a first component from the group consisting of a set accelerating amount of sodium nitrate, sodium nitrite and mixtures thereof present in an amount from 30 to 60 weight percent of the second composition,
calcium hydroxide present in the amount of 10 to 30 weight percent of the second composition,
and water present in the amount of 30 to 60 weight percent of the second composition, such that the such that when the admixture is made the setting agent accelerator promotes initial flocculating of the castable refractory ;
projecting the admixture onto a metallurgical vessel or kiln;
permitting the setting agent accelerator to achieve final setting of the admixture to set to form a refractory lining.

### Claim 10 (depends on 9)

The process for placing a castable refractory according to claim 9 wherein the setting agent accelerator is present in an amount of from 0.1 to 3.0 weight percent of the total dry weight of the admixture.

### Claim 11 (depends on 9)

The process for placing a castable refractory according to claim 9 wherein the setting agent accelerator is present in an amount of from 0.01 to 5.0 weight percent of the total wetted weight of the admixture.

### Claim 12 (depends on 9)

The process for placing a castable refractory according to claim 9 wherein the first component comprises sodium nitrate wherein the sodium nitrate is present in an amount of from 35 to 45 weight percent of the second composition.

### Claim 13 (depends on 12)

The process for placing a castable refractory according to claim 12 wherein the calcium hydroxide is present in an amount of 12 to 18 weight percent of the second composition,

### Claim 14 (depends on 9)

The process for placing a castable refractory according to claim 9 wherein the first component comprises sodium nitrite.

### Claim 15 (depends on 9)

The process for placing a castable refractory of claim 9 wherein the castable refractory is an ultra-low cement castable refractory,

### Claim 16 (depends on 9)

The process for placing a castable refractory of claim 9 wherein the castable refractory is a low cement castable refractory.

### Claim 17 (depends on 9)

The process for placing a castable refractory of claim 9 wherein the castable refractory is a regular castable refractory.

### Claim 18

A refractory composition comprising an admixture of a first composition comprising
a castable refractory;
a second composition comprising a setting agent accelerator comprising a first component from the group consisting of a set accelerating amount of sodium nitrate, sodium nitrite and mixtures thereof present in an amount from 30 to 60 weight percent of the second composition,
calcium hydroxide present in the amount of 10 to 30 weight percent of the second composition,
and water present in the amount of 30 to 60 weight percent of the second composition, such that when the admixture is made the setting agent accelerator promotes initial flocculating and later promotes final setting of the castable refractory.

### Claim 19 (depends on 18)

The refractory composition according to claim 18 wherein the setting agent accelerator is present in an amount of from 0.1 to 3.0 weight percent of the total dry weight of the refractory composition.

### Claim 20 (depends on 18)

The refractory composition according to claim 18 wherein the setting agent accelerator is present in an amount of from 0.01 to 5.0 weight percent of the total dry weight of the refractory composition.

### Claim 21 (depends on 18)

The refractory composition according to claim 18 wherein the first component comprises sodium nitrate wherein the sodium nitrate is present in an amount of from 35 to 45 weight percent of the second composition.

### Claim 22 (depends on 21)

The refractory composition according to claim 21 wherein the calcium hydroxide is present in an amount of 12 to 18 weight percent of the second composition.

### Claim 23 (depends on 18)

The refractory composition according to claim 18 wherein the first component comprises sodium nitrite.

### Claim 24 (depends on 18)

The refractory composition according to claim 18 wherein the refractory castable is an ultra-low cement refractory castable.

### Claim 25 (depends on 18)

The refractory composition according to claim 18 wherein the refractory castable is a low cement refractory castable.

### Claim 26 (depends on 18)

The refractory composition according to claim 18 wherein the refractory castable is a regular refractory castable.

### Claim 27

An admixture for a setting agent accelerator for a refractory castable comprising: 60 to 80 weight percent sodium nitrate, sodium nitrite or mixtures thereof and 20 to 40 weight percent calcium hydroxide.

### Claim 28 (depends on 20)

The admixture for a setting agent accelerator for a refractory castable of claim 20 comprising 69 to 75 weight percent sodium nitrate, sodium nitrite or mixtures thereof and 25 to 31 weight percent calcium hydroxide.