# US 2012/0252319 A1 · Polishing method, manufacturing method of piezoelectric vibrating piece, piezoelectric vibrator, oscillator, electronic apparatus and radio-controlled timepiece

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2012/0252319 A1
- Document ID: US20120252319A1
- Status: Published application
- Kind: A1
- Application number: 13/431,301
- Filed: 2012-03-27
- Published: 2012-10-04
- Earliest claimed: 2011-03-28
- Inventors: Youichi Fujihira
- Web page: https://patentgrep.com/patent/US20120252319A1

## CPC

- G04R 20/10: Tuning or receiving; Circuits therefor
- B24B 37/042: {operating processes therefor}
- B24B 37/08: for double side lapping
- H03H 9/1021: {the BAW device being of the cantilever type}
- H03H 9/215: consisting of quartz
- H03H 2003/0492: {during the manufacture of a tuning-fork}
- G04R: RADIO-CONTROLLED TIME-PIECES
- B24B: MACHINES, DEVICES, OR PROCESSES FOR GRINDING OR POLISHING (grinding of gear teeth B23F, of screw-threads B23G1/36; by electro-erosion B23H; abrasive or related blasting B24C; tools for grinding, buffing or sharpening B24D; polishing compositions C09G1/00; abrasives C09K3/14; electrolytic etching or polishing C25F3/00; grinding arrangements for use on assembled railway tracks E01B31/17); DRESSING OR CONDITIONING OF ABRADING SURFACES; FEEDING OF GRINDING, POLISHING, OR LAPPING AGENTS
- H03H: IMPEDANCE NETWORKS, e.g. RESONANT CIRCUITS; RESONATORS (waveguides, resonators, lines or other devices of the waveguide type H01P)

## Abstract

Provided is a polishing method which can enhance thickness accuracy of a wafer at the time of polishing the wafer. In a polishing method of a crystal wafer (tuning fork substrate) which is held on a carrier between an upper platen and a lower platen, an AT cut wafer for thickness measurement is arranged on the carrier, the AT cut wafer is polished together with the crystal wafer (tuning fork substrate), resonance frequency of the AT cut wafer is detected, and a thickness of the crystal wafer (tuning fork substrate) is controlled based on a detection result.

## Claims

### Claim 1

A method for polishing a wafer mounted on a polishing device that comprises a lower platen, an upper platen above the lower platen, a wafer carrier mounted on the lower platen, a probe mounted on the upper platen, the method comprising:
mounting a first wafer and an AT cut wafer on the wafer carrier;
applying a polishing agent to upper and lower surfaces of the first wafer and the AT cut wafer;
rotating the upper platen and the lower platen while applying the polishing agent, thereby polishing the first wafer and the AT cut wafer by the rotating;
detecting a resonant frequency of the AT cut wafer, wherein the resonant frequency of the AT cut wafer corresponds to a thickness of the first wafer; and
continue rotating the upper and lower platens until a resonant frequency corresponding to a predetermined thickness of the first wafer is detected a predetermined number of times.

### Claim 2 (depends on 1)

The method of claim 1, wherein the upper and lower platens are rotated until the resonant frequency corresponding to a predetermined thickness of the first wafer is detected a predetermined number of times within the predetermined period of time.

### Claim 3 (depends on 2)

The method of claim 2, wherein the upper and lower platens are rotated until the resonant frequency corresponding to a predetermined thickness of the first wafer is detected at least three times within the predetermined period of time.

### Claim 4 (depends on 2)

The method of claim 2, wherein the predetermined period of time comprises the range of 0.5 seconds to 1.0 seconds.

### Claim 5 (depends on 1)

The method of claim 1, wherein the upper and lower platens are rotated until the resonant frequency corresponding to a predetermined thickness of the first wafer is detected at least once.

### Claim 6 (depends on 1)

The method of claim 1, wherein the AT cut wafer is mounted at a center of the carrier.

### Claim 7 (depends on 1)

The method of claim 1, further comprising mounting a second wafer on the carrier.

### Claim 8 (depends on 7)

The method of claim 7, wherein the AT cut wafer is mounted between the first and second wafers.

### Claim 9 (depends on 1)

The method of claim 1, wherein the AT cut wafer is mounted on the carrier at a position such that when the lower and upper platens rotate, the AT cut wafer periodically passes under the probe.

### Claim 10 (depends on 1)

The method of claim 1, wherein the upper and lower platens are rotated in opposite directions.

### Claim 11

A method for polishing a wafer mounted on a polishing device that comprises a lower platen, an upper platen above the lower platen, a wafer carrier mounted on the lower platen, a probe mounted on the upper platen, the method comprising:
mounting a first wafer and an AT cut wafer on the wafer carrier;
rotating the upper platen and the lower platen, thereby polishing the first wafer and the AT cut wafer by the rotating;
detecting a resonant frequency of the AT cut wafer, wherein the resonant frequency of the AT cut wafer corresponds to a thickness of the first wafer; and
continue rotating the upper and lower platens until a resonant frequency corresponding to a predetermined thickness of the first wafer is detected a predetermined number of times within a predetermined period of time.

### Claim 12 (depends on 11)

The method of claim 11, further comprising applying a polishing agent to upper and lower surfaces of the first wafer and the AT cut wafer.

### Claim 13 (depends on 11)

The method of claim 11, wherein the upper and lower platens are rotated until the resonant frequency corresponding to a predetermined thickness of the first wafer is detected at least three times within the predetermined period of time.

### Claim 14 (depends on 11)

The method of claim 11, wherein the predetermined period of time comprises the range of 0.5 seconds to 1.0 seconds.

### Claim 15 (depends on 11)

The method of claim 11, wherein the upper and lower platens are rotated until the resonant frequency corresponding to a predetermined thickness of the first wafer is detected at least once.

### Claim 16 (depends on 11)

The method of claim 11, wherein the AT cut wafer is mounted at a center of the carrier.

### Claim 17 (depends on 11)

The method of claim 11, wherein the AT cut wafer is mounted on the carrier at a position such that when the lower and upper platens rotate, the AT cut wafer periodically passes under the probe.

### Claim 18 (depends on 11)

The method of claim 11, wherein the upper and lower platens are rotated in opposite directions.

### Claim 19

A method for polishing a wafer mounted on a polishing device that comprises a lower platen, an upper platen above the lower platen, multiple wafer carriers mounted on the lower platen, a probe mounted on the upper platen, the method comprising:
mounting a first wafer and an AT cut wafer on each of the wafer carriers;
rotating the upper platen and the lower platen, thereby polishing the first wafer and the AT cut wafer mounted on each of the wafer carriers by the rotating;
detecting a resonant frequency of each of the AT cut wafers, wherein the resonant frequency of each AT cut wafer corresponds to a thickness of the corresponding first wafer; and
continue rotating the upper and lower platens until a resonant frequency corresponding to a predetermined thickness of one or more of the first wafers is detected a predetermined number of times within a predetermined period of time.

### Claim 20 (depends on 19)

The method of claim 19, wherein the AT cut wafers are each mounted on the corresponding wafer carrier at a position such that when the lower and upper platens rotate, each AT cut wafer periodically passes under the probe.