# US 2012/0252225 A1 · Semiconductor fabrication method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2012/0252225 A1
- Document ID: US20120252225A1
- Status: Published application
- Kind: A1
- Application number: 13/140,549
- Filed: 2011-04-11
- Published: 2012-10-04
- Earliest claimed: 2011-03-29
- Inventors: Chunlong Li; Junfeng Li
- Web page: https://patentgrep.com/patent/US20120252225A1

## CPC

- H10P 14/6309: {of silicon in uncombined form, i.e. pure silicon}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A semiconductor fabrication method is provided, in which a protective layer is deposited on the dummy wafer such that the protective layer fully encases the dummy wafer. Therefore, the dummy wafer will not be oxidized during thermal oxidation, thereby reducing dummy wafer consumption, decreasing production cost, avoiding particulate matter produced due to oxidation of the dummy wafer, and preventing the wafer to be oxidized from contamination.

## Claims

### Claim 1

A semiconductor fabrication method, comprising:
providing a wafer to be oxidized;
providing a dummy wafer; and
arranging the wafer to be oxidized and the dummy wafer in a thermal oxidation tool, to perform thermal oxidation,
wherein the method further comprises, before performing the thermal oxidation, depositing a protective layer on an outer surface of the dummy wafer such that the protective layer fully encases the dummy wafer.

### Claim 2 (depends on 1)

The semiconductor fabrication method according to claim 1, wherein the thermal oxidation tool is a thermal oxidation furnace.

### Claim 3 (depends on 1)

The semiconductor fabrication method according to claim 1, wherein the protective layer is a silicon nitride film.

### Claim 4 (depends on 3)

The semiconductor fabrication method according to claim 3, wherein the silicon nitride film is formed by chemical vapor deposition (CVD), physical vapor deposition (PVD), or atomic layer deposition (ALD).

### Claim 5 (depends on 3)

The semiconductor fabrication method according to claim 3, wherein the silicon nitride film is formed by Low-pressure CVD (LPCVD) at the temperature of 760° C.

### Claim 6 (depends on 1)

The semiconductor fabrication method according to claim 1, wherein the protective layer has a thickness ranging from 500 Å to 1000 Å.