# US 2012/0252224 A1 · Method of depositing silicon oxide film and silicon nitride film, film forming apparatus, and method of manufacturing semiconductor device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2012/0252224 A1
- Document ID: US20120252224A1
- Status: Published application
- Kind: A1
- Application number: 13/432,611
- Filed: 2012-03-28
- Published: 2012-10-04
- Earliest claimed: 2011-03-30
- Assignees: Tokyo Electron Limited
- Inventors: Atsushi ENDO; Masaki KUROKAWA; Hiroki IRIUDA
- Web page: https://patentgrep.com/patent/US20120252224A1

## CPC

- H10P 14/69215: {the material being a silicon oxide, e.g. SiO2}
- C23C 16/345: {Silicon nitride}
- C23C 16/402: {Silicon dioxide}
- H10P 14/6334: {using decomposition or reaction of gaseous or vapour phase compounds, i.e. chemical vapour deposition (deposition by physical ablation of a target H10P14/6329)}
- H10P 14/662: {Laminate layers, e.g. stacks of alternating high-k metal oxides (adhesion layers or buffer layers H10P14/6508, H10P14/6548)}
- H10P 14/69433: {the material being a silicon nitride not containing oxygen, e.g. SixNy or SixByNz}
- H10W 42/121: {protecting against mechanical damage (H10W76/00, H10W74/00 take precedence)}
- H10P 72/127: {characterised by the substrate support}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

A method of depositing a silicon oxide film and a silicon nitride film includes depositing the silicon oxide film and the silicon nitride film on a substrate, and a gas for forming the silicon nitride film further includes boron.

## Claims

### Claim 1

A method of depositing a silicon oxide film and a silicon nitride film, the method comprising depositing the silicon oxide film and the silicon nitride film on a substrate,
wherein boron is added in a gas for forming the silicon nitride film.

### Claim 2

A method of depositing a silicon oxide film and a silicon nitride film on a substrate, the method comprising:
accommodating a plurality of substrates, on each of which a deposited film of the silicon oxide film and the silicon nitride film is to be formed, in a processing chamber wherein a side portion of each of the substrates is held;
supplying a silicon oxide material gas and an oxidizing agent into the processing chamber, when the silicon oxide film is formed;
supplying a silicon material gas, a nitrating agent, and a boron-containing gas into the processing chamber, when the silicon nitride film is formed; and
forming the deposited films of the silicon oxide films and the silicon nitride films on a surface and a rear surface of each of the plurality of substrates by repeating the supplying of the silicon oxide material gas and the oxidizing agent and the supplying of the silicon material gas, the nitrating agent, and the boron-containing gas.

### Claim 3 (depends on 2)

The method of claim 2, wherein a difference between a film forming temperature when the silicon oxide film is formed and a film forming temperature when the silicon nitride film is formed is within a range of 50° C. to 150° C.

### Claim 4 (depends on 2)

The method of claim 2, wherein a film forming temperature when the silicon oxide film is formed and a film forming temperature when the silicon nitride film is formed are equal to each other.

### Claim 5 (depends on 2)

The method of claim 2, wherein the boron-containing gas is boron trichloride.

### Claim 6 (depends on 2)

The method of claim 2, wherein the silicon material gas is dichlorosilane and the nitrating agent is ammonia.

### Claim 7 (depends on 1)

The method of claim 1, wherein the silicon nitride film is a film formed of SiaBbNc, and an atomic composition ratio of the SiaBbNc is controlled within ranges of a=25 to 17 atm %, b=22 to 32 atm %, and c=53 to 51 atm %.

### Claim 8 (depends on 7)

The method of claim 7, wherein the substrate is a silicon wafer, and a stress applied to the silicon wafer from the film formed of the SiaBbNc is controlled within a range of 100 to 600 MPa.

### Claim 9 (depends on 1)

The method of claim 1, wherein the silicon nitride film is a SiBN film, in which the number of silicon atoms is less than the number of boron atoms.

### Claim 10 (depends on 9)

The method of claim 9, wherein the silicon nitride film is a film formed of SiaBbNc, and an atomic composition ratio of the SiaBbNc is controlled within ranges of a=20 to 17 atm %, b=28 to 32 atm %, and c=52 to 51 atm %.

### Claim 11 (depends on 10)

The method of claim 10, wherein the substrate is a silicon wafer, and a stress applied to the silicon wafer from the film formed of the SiaBbNc is controlled within a range of 100 to 300 MPa.

### Claim 12 (depends on 1)

The method of claim 1, wherein the silicon nitride film is a SiBN film, in which the number of silicon atoms is equal to or greater than the number of boron atoms.

### Claim 13 (depends on 12)

The method of claim 12, wherein the silicon nitride film is a film formed of SiaBbNc, and an atomic composition ratio of the SiaBbNc is controlled within ranges of a=25 to 24 atm %, b=22 to 24 atm %, and c=53 to 52 atm %.

### Claim 14 (depends on 13)

The method of claim 13, wherein the substrate is a silicon wafer, and a haze level of the film formed of the SiaBbNc is controlled within a range of 0.005 ppm to 0.01 ppm.

### Claim 15 (depends on 2)

A film forming apparatus forming a deposited film of a silicon oxide film and a silicon nitride film on a substrate, the film forming apparatus comprising:
a processing chamber which accommodates a plurality of substrates, on which the deposited film of the silicon oxide film and the silicon nitride film is to be formed, wherein a side portion of each of the substrates is held;
a gas supply mechanism which supplies a gas used in a process into the processing chamber;
an exhauster which evacuates an inside of the processing chamber; and
a controller which controls the gas supply mechanism and the exhauster,
wherein the controller controls the gas supply mechanism and the exhauster to execute the supplying of the silicon oxide material gas and the oxidizing agent, the supplying of the silicon material gas, the nitrating agent, and the boron-containing gas, and the forming of the deposited films of the silicon oxide films and the silicon nitride films, of claim 2.

### Claim 16

A method of manufacturing a semiconductor device including a deposited film, in which a silicon oxide film and a silicon nitride film are repeatedly deposited, the method comprising:
accommodating a plurality of substrates, on each of which the deposited film of the silicon oxide film and the silicon nitride film is to be formed, in a processing chamber wherein a side portion of each of the substrates is held;
supplying a silicon oxide material gas and an oxidizing agent into the processing chamber, when the silicon oxide film is formed;
supplying a silicon material gas, a nitrating agent, and a boron-containing gas into the processing chamber, when the silicon nitride film is formed;
forming the deposited films of the silicon oxide films and the silicon nitride films on a surface and a rear surface of each of the plurality of substrates by repeating the supplying of the silicon oxide material gas and the oxidizing agent and the supplying of the silicon material gas, the nitrating agent, and the boron-containing gas; and
removing the deposited film formed on the rear surface of each of the plurality of substrates, after finishing the forming of the deposited film.

### Claim 17 (depends on 16)

The method of claim 16, wherein a difference between a film forming temperature when the silicon oxide film is formed and a film forming temperature when the silicon nitride film is formed is within a range of 50° C. to 150° C.

### Claim 18 (depends on 16)

The method of claim 16, wherein a film forming temperature when the silicon oxide film is formed and a film forming temperature when the silicon nitride film is formed are equal to each other.