# US 2012/0252209 A1 · Plasma nitriding method, plasma nitriding apparatus and method of manufacturing semiconductor device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2012/0252209 A1
- Document ID: US20120252209A1
- Status: Published application
- Kind: A1
- Application number: 13/433,746
- Filed: 2012-03-29
- Published: 2012-10-04
- Earliest claimed: 2011-03-31
- Assignees: Tokyo Electron Limited
- Inventors: Yoshiro Kabe; Yoshihiro Sato
- Web page: https://patentgrep.com/patent/US20120252209A1

## CPC

- H10P 95/00: Generic processes or apparatus for manufacture or treatments not covered by the other groups of this subclass
- C23C 8/36: using ionised gases, e.g. ionitriding
- H10D 64/01338: {with a treatment, e.g. annealing, after the formation of the conductor}
- H10D 64/01354: {passivation or protection of the electrode, e.g. using re-oxidation}
- H10D 64/664: {the additional layers comprising a barrier layer between the layer of silicon and an upper metal or metal silicide layer}
- H10W 20/038: {covering conductive structures (H10W20/037 takes precedence)}
- H10D 64/693: {the insulator comprising nitrogen, e.g. nitrides, oxynitrides or nitrogen-doped materials}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

A plasma nitriding method includes placing, in a processing chamber, a target object having a structure including a first portion containing a metal and a second portion containing silicon to expose surfaces of the first and the second portion; and performing a plasma process on the target object to selectively nitride the surface of the first portion such that a metal nitride film is selectively formed on the surface of the first portion. Further, the first portion contains tungsten, and a nitrogen-containing plasma is generated by supplying a nitrogen-containing gas into the processing chamber and setting an internal pressure of the processing chamber in a range from 133 Pa to 1333 Pa. The surface of the first portion is selectively nitrided without nitriding the surface of the second portion by the nitrogen-containing plasma such that a tungsten nitride film is formed on the surface of the first portion.

## Claims

### Claim 1

A plasma nitriding method comprising:
placing, in a processing chamber, a target object having a structure including a first portion containing a metal and a second portion containing silicon to expose surfaces of the first and the second portion; and
performing a plasma process on the target object to selectively nitride the surface of the first portion such that a metal nitride film is selectively formed on the surface of the first portion,
wherein the first portion contains tungsten, and
wherein a nitrogen-containing plasma is generated by supplying a nitrogen-containing gas into the processing chamber and setting an internal pressure of the processing chamber in a range from 133 Pa to 1333 Pa, and the surface of the first portion is selectively nitrided without nitriding the surface of the second portion by the nitrogen-containing plasma such that a tungsten nitride film is formed on the surface of the first portion.

### Claim 2 (depends on 1)

The plasma nitriding method of claim 1, wherein the internal pressure of the processing chamber is set in a range from 267 Pa to 1333 Pa.

### Claim 3 (depends on 1)

The plasma nitriding method of claim 1, wherein the second portion includes a silicon substrate made of silicon, and
the first portion is disposed on a portion of an upper surface of the silicon substrate.

### Claim 4 (depends on 2)

The plasma nitriding method of claim 2, wherein the second portion includes a silicon substrate made of silicon, and
the first portion is disposed on a portion of an upper surface of the silicon substrate.

### Claim 5 (depends on 1)

The plasma nitriding method of claim 1, wherein the structure includes a silicon substrate made of silicon and a laminating body disposed on a portion of an upper surface of the silicon substrate,
wherein the laminating body includes an insulating layer made of silicon oxynitride, a first electrode layer stacked on the insulating layer and made of polysilicon, a barrier layer stacked on the first electrode layer and made of tungsten nitride, and a second electrode layer stacked on the barrier layer and made of tungsten,
wherein the first portion includes the barrier layer and the second electrode layer, and
wherein the second portion includes the silicon substrate, the insulating layer, and the first electrode layer.

### Claim 6 (depends on 2)

The plasma nitriding method of claim 2, wherein the structure includes a silicon substrate made of silicon and a laminating body disposed on a portion of an upper surface of the silicon substrate,
wherein the laminating body includes an insulating layer made of silicon oxynitride, a first electrode layer stacked on the insulating layer and made of polysilicon, a barrier layer stacked on the first electrode layer and made of tungsten nitride, and a second electrode layer stacked on the barrier layer and made of tungsten,
wherein the first portion includes the barrier layer and the second electrode layer, and
wherein the second portion includes the silicon substrate, the insulating layer, and the first electrode layer.

### Claim 7 (depends on 1)

The plasma nitriding method of claim 1, wherein the nitrogen-containing plasma is a microwave-excited plasma formed by converting the nitrogen-containing gas supplied to the processing chamber into a plasma by a microwave introduced into the processing chamber through a planar antenna having a plurality of slots.

### Claim 8 (depends on 2)

The plasma nitriding method of claim 2, wherein the nitrogen-containing plasma is a microwave-excited plasma formed by converting the nitrogen-containing gas supplied to the processing chamber into a plasma by a microwave introduced into the processing chamber through a planar antenna having a plurality of slots.

### Claim 9 (depends on 4)

The plasma nitriding method of claim 4, wherein the nitrogen-containing plasma is a microwave-excited plasma formed by converting the nitrogen-containing gas supplied to the processing chamber into a plasma by a microwave introduced into the processing chamber through a planar antenna having a plurality of slots.

### Claim 10 (depends on 6)

The plasma nitriding method of claim 6, wherein the nitrogen-containing plasma is a microwave-excited plasma formed by converting the nitrogen-containing gas supplied to the processing chamber into a plasma by a microwave introduced into the processing chamber through a planar antenna having a plurality of slots.

### Claim 11

A plasma nitriding apparatus which performs a plasma process on a target object having a structure including a first portion containing a metal and a second portion containing silicon to expose surfaces of the first and the second portion, and selectively nitrides the surface of the first portion by the plasma process such that a metal nitride film is selectively formed on the surface of the first portion, wherein the first portion contains tungsten, the apparatus comprising:
a processing chamber in which the target object is loaded and a specific process is performed;
a gas supply unit which supplies a nitrogen-containing gas as a processing gas into the processing chamber;
an exhaust unit which vacuum evacuates the processing chamber;
a plasma generating unit which generates a plasma in the processing chamber; and
a control unit which controls such that the nitrogen-containing gas is supplied into the processing chamber by the gas supply unit, an internal pressure of the processing chamber is set in a range from 133 Pa to 1333 Pa by the exhaust unit, a nitrogen-containing plasma is generated in the processing chamber by the plasma generating unit, and the surface of the first portion is selectively nitrided without nitriding the surface of the second portion by the nitrogen-containing plasma such that a tungsten nitride film is formed on the surface of the first portion.

### Claim 12

A method of manufacturing a semiconductor device having a structure including a first portion containing a metal and a second portion containing silicon, wherein the first portion contains tungsten, the method comprising:
forming an initial laminated film, to become at least a part of the first and the second portion, on a semiconductor substrate;
etching the initial laminated film to form the structure such that surfaces of the first and the second portions are exposed;
transferring the semiconductor substrate having the structure into a processing chamber;
supplying a nitrogen-containing gas into the processing chamber;
setting an internal pressure of the processing chamber in a range from 133 Pa to 1333 Pa;
generating a nitrogen-containing plasma in the processing chamber; and
plasma nitriding to selectively nitride the surface of the first portion without nitriding the surface of the second portion by the nitrogen-containing plasma such that a tungsten nitride film is formed on the surface of the first portion.

### Claim 13 (depends on 12)

The method of claim 12, further comprising forming an insulating layer made of silicon oxide to cover the structure after the plasma nitriding.