# US 2012/0252208 A1 · Method of forming metal interconnections of semiconductor device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2012/0252208 A1
- Document ID: US20120252208A1
- Status: Published application
- Kind: A1
- Application number: 13/431,446
- Filed: 2012-03-27
- Published: 2012-10-04
- Earliest claimed: 2011-03-28
- Assignees: Samsung Electronics Co., Ltd.
- Inventors: WooJin Jang; KyoungWoo Lee
- Web page: https://patentgrep.com/patent/US20120252208A1

## CPC

- H10W 20/425: {Barrier, adhesion or liner layers}
- H10W 20/0261: {characterised by the filling method or the material of the conductive fill}
- H10W 20/037: {the barrier, adhesion or liner layers being on top of a main fill metal}
- H10W 20/056: {by filling conductive material into holes, grooves or trenches}
- H10W 20/077: {on sidewalls or on top surfaces of conductors (H10W20/076 takes precedence)}
- H10W 20/20: Interconnections within wafers or substrates, e.g. through-silicon vias [TSV]
- H10W 20/42: Vias, e.g. via plugs
- H10W 20/43: Layouts of interconnections
- H10W 20/4421: {the principal metal being copper}
- H10W 72/20: Bump connectors, e.g. solder bumps or copper pillars; Dummy bumps; Thermal bumps
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

A method of forming a metal interconnection of semiconductor device is provided. The method includes forming a low-k dielectric layer including an opening; forming a barrier metal pattern conformally covering a bottom surface and an inner sidewall of the opening; forming a metal pattern exposing a part of the inner sidewall of the barrier metal pattern in the opening; forming a metal capping layer on the top surfaces of the metal pattern and the low-k dielectric layer using a selective chemical vapor deposition process, wherein the thickness of the metal capping layer on the metal pattern is greater than the thickness of the metal capping layer on the low-k dielectric layer; and forming a metal capping pattern covering the top surface of the metal pattern by planarizing the metal capping layer down to the top surface of the low-k dielectric layer.

## Claims

### Claim 1

A method of forming a metal interconnection of a semiconductor device comprising:
forming a low-k dielectric layer including an opening, the low-k dielectric layer having a top surface;
forming a barrier metal pattern conformally covering a bottom surface and an inner sidewall of the opening;
forming a metal pattern exposing a part of the inner sidewall of the barrier metal pattern in the opening, the metal pattern having a top surface;
forming a metal capping layer having a first thickness on the top surface of the metal pattern and forming a metal capping layer having a second thickness on the low-k dielectric layer using a selective chemical vapor deposition process, wherein the first thickness is greater than the second thickness; and
forming a metal capping pattern covering the top surface of the metal pattern by planarizing the metal capping layer down to the top surface of the low-k dielectric layer.

### Claim 2 (depends on 1)

The method of claim 1, wherein a top surface of the metal capping pattern is coplanar with the top surface of the low-k dielectric layer. 20

### Claim 3 (depends on 1)

The method of claim 1, wherein the top surface of the metal capping pattern is disposed to be lower than the top surface of the low-k dielectric layer.

### Claim 4 (depends on 1)

The method of claim 1, wherein the metal pattern comprises copper and the metal capping pattern comprises ruthenium.

### Claim 5 (depends on 1)

The method of claim 1, wherein in the selective chemical vapor deposition process, the metal capping layer is formed on the metal pattern at a first rate and the metal capping layer on the low-k dielectric layer is formed at a second rate; the first rate being higher than the second rate.

### Claim 6 (depends on 1)

The method of claim 1, further comprising the steps of performing a thermal treatment process and a plasma treatment process before forming the metal capping layer.

### Claim 7 (depends on 1)

The method of claim 1, wherein forming the metal pattern comprises:
forming a metal layer filling the opening in which the barrier metal pattern is formed on the low-k dielectric layer;
planarizing the metal layer down to the top surface of the low-k dielectric layer to provide a top surface of the planarized metal layer ; and
recessing the top surface of the planarized metal layer by performing an isotropic etching process on the metal layer.

### Claim 8 (depends on 7)

The method of claim 7, wherein the isotropic etching process uses a mixed solution comprising a corrosion inhibitor and one of dilute sulfuric acid solution and a solution of HF:HNO3(25:1).

### Claim 9 (depends on 1)

The method of claim 1, wherein the low-k dielectric layer is formed from a material having a dielectric constant of from about 2.0 to about 3.5.

### Claim 10 (depends on 1)

The method of claim 1, further comprising forming a solder ball or a solder bump on a surface of the metal capping pattern.

### Claim 11 (depends on 1)

The method of claim 1, further comprising forming a capping insulating layer extending from a top surface of the metal capping pattern to a top surface of the low-k dielectric layer.

### Claim 12 (depends on 11)

The method of claim 11, wherein the capping insulating layer on the metal capping pattern has a first thickness and the capping insulating layer on the low-k dielectric layer has a second thickness, wherein the first thickness is greater than the second thickness.

### Claim 13

A method of forming a metal interconnection of a semiconductor device comprising:
forming a low-k dielectric layer including an opening;
conformally forming a barrier metal layer on the low-k dielectric layer including the opening;
forming a metal layer filling the opening on the barrier metal layer;
forming a barrier metal pattern and a metal pattern locally in the opening by planarizing the metal layer and the barrier metal layer down to a top surface of the low-k dielectric layer;
exposing a part of an inner wall of the barrier metal pattern by recessing a top surface of the metal pattern;
selectively depositing a metal capping layer on a top surface of the recessed metal pattern and a top surface of the low-k dielectric layer, wherein the metal capping layer on the top surface of the recessed metal pattern has a first thickness and the metal capping layer on the top surface of the low-k dielectric layer has a second thickness, wherein the first thickness is greater than the second thickness; and
forming a metal capping pattern covering a top surface of the metal pattern by planarizing the metal capping layer down to the top surface of the low-k dielectric layer.

### Claim 14 (depends on 13)

The method of claim 13, wherein forming the metal capping layer is forming a ruthenium layer by performing a selective chemical deposition process.

### Claim 15 (depends on 13)

The method of claim 13, wherein the low-k dielectric layer is formed from material having a dielectric constant of from about 2.0 to about 3.5.

### Claim 16

A method of forming a metal interconnection of a semiconductor device comprising:
forming a low-k dielectric layer on an etch-stop layer, the low-k dielectric layer having a top surface comprising an opening having a bottom surface and an inner sidewall;
forming a barrier metal pattern conformally covering the bottom surface and an inner sidewall of the opening, wherein the opening is coated but not filled;
planarizing the metal barrier pattern to expose the low-k dielectric layer and an upper surface of the barrier metal pattern on the inner sidewall of the opening;
forming a second metal layer on the planarized metal barrier pattern and the exposed low-k dielectric layer;
planarizing the second metal layer to expose the low-k dielectric layer and recess the level of the second metal layer in the opening;
forming a metal capping layer on the exposed low-k dielectric layer and filling the opening;
planarizing the metal capping layer to expose the low-k dielectric layer, an upper surface of the barrier metal pattern on the inner sidewall of the opening and the metal capping layer in the opening; and
forming a capping insulator layer and an insulating layer on the exposed low-k dielectric layer and the opening.

### Claim 17 (depends on 16)

The method of claim 16, wherein a top surface of the metal capping pattern is coplanar with the top surface of the low-k dielectric layer.

### Claim 18 (depends on 16)

The method of claim 16, wherein the planarizing of the metal capping pattern planarizes the metal capping pattern to be lower than the top surface of the low-k dielectric layer.

### Claim 19 (depends on 16)

The method of claim 16, wherein the metal pattern comprises copper and the metal capping pattern comprises ruthenium.

### Claim 20 (depends on 16)

The method of claim 16, wherein the capping insulating layer on the metal capping pattern has a first thickness and the capping insulating layer on the low-k dielectric layer has a second thickness, wherein the first thickness is greater than the second thickness.