# US 2012/0252207 A1 · Post deposition treatments for cvd cobalt films

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2012/0252207 A1
- Document ID: US20120252207A1
- Status: Published application
- Kind: A1
- Application number: 13/174,692
- Filed: 2011-06-30
- Published: 2012-10-04
- Earliest claimed: 2011-03-31
- Assignees: Applied Materials, Inc.
- Inventors: Yu Lei; Xinyu Fu; Anantha Subramani; Seshadri Ganguli; Srinivas Gandikota
- Web page: https://patentgrep.com/patent/US20120252207A1

## CPC

- H10P 14/40: of conductive or resistive materials
- H10P 14/43: Chemical deposition, e.g. chemical vapour deposition [CVD]
- H10P 14/432: {using selective deposition}
- H10W 20/035: {combinations of barrier, adhesion or liner layers, e.g. multi-layered barrier layers}
- H10W 20/038: {covering conductive structures (H10W20/037 takes precedence)}
- H10W 20/048: {by using plasmas or gaseous environments, e.g. by nitriding}
- H10W 20/049: {by diffusing alloying elements}
- H10W 20/0523: {by irradiating with ultraviolet or particle radiation}
- H10W 20/0526: {by thermal treatment thereof}
- H10W 20/056: {by filling conductive material into holes, grooves or trenches}
- H10W 20/063: {by forming conductive members before forming protective insulating material}
- H10W 20/077: {on sidewalls or on top surfaces of conductors (H10W20/076 takes precedence)}
- H10W 20/086: {involving buried masks}
- H10W 20/425: {Barrier, adhesion or liner layers}
- B82Y 40/00: Manufacture or treatment of nanostructures
- H10W 20/043: {for electroplating}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- B82Y: SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES; MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES; MANUFACTURE OR TREATMENT OF NANOSTRUCTURES

## Abstract

Embodiments of the invention provide methods for forming materials on a substrate used for metal gate and other applications. In one embodiment, a method includes forming a cobalt stack over a barrier layer disposed on a substrate by depositing a cobalt layer during a deposition process, exposing the cobalt layer to a plasma to form a plasma-treated cobalt layer during a plasma process, and repeating the cobalt deposition process and the plasma process to form the cobalt stack containing a plurality of plasma-treated cobalt layers. The method further includes exposing the cobalt stack to an oxygen source gas to form a cobalt oxide layer from an upper portion of the cobalt stack during a surface oxidation process and heating the remaining portion of the cobalt stack to a temperature within a range from about 300° C. to about 500° C. to form a crystalline cobalt film during a thermal annealing crystallization process.

## Claims

### Claim 1

A method for depositing materials on a substrate surface, comprising:
forming a cobalt stack over a barrier layer disposed on a substrate by:
depositing a cobalt layer during a deposition process;
exposing the cobalt layer to a plasma to form a plasma-treated cobalt layer during a plasma process; and
repeating the deposition process and the plasma process to form the cobalt stack comprising a plurality of plasma-treated cobalt layers;
exposing the cobalt stack to an oxygen source gas to form a cobalt oxide layer from an upper portion of the cobalt stack during a surface oxidation process; and
heating the cobalt stack to a crystallization temperature within a range from about 300° C. to about 500° C. to form a crystalline cobalt film from the cobalt stack during a thermal annealing crystallization process.

### Claim 2 (depends on 1)

The method of claim 1, wherein the cobalt stack comprises a carbon concentration of about 3 at % or less.

### Claim 3 (depends on 1)

The method of claim 1, wherein the cobalt stack has a thickness within a range from about 80 Å to about 120 Å and has a resistivity within a range from about 20 μΩ-cm to about 40 μΩ-cm.

### Claim 4 (depends on 1)

The method of claim 1, wherein the cobalt stack has a thickness within a range from about 450 Å to about 750 Å and has a resistivity within a range from about 5 μΩ-cm to about 20 μΩ-cm.

### Claim 5 (depends on 1)

The method of claim 1, wherein the plurality of plasma-treated cobalt layers within the cobalt stack contains at least 3 plasma-treated cobalt layers and up to about 30 plasma-treated cobalt layers.

### Claim 6 (depends on 1)

The method of claim 1, wherein the crystallization temperature is within a range from about 300° C. to about 425° C. for a time period within a range from about 5 minutes to about 60 minutes during the thermal annealing crystallization process.

### Claim 7 (depends on 1)

The method of claim 1, wherein the cobalt oxide layer is disposed on the cobalt stack and has a thickness within a range from about 5 Å to about 30 Å.

### Claim 8 (depends on 1)

The method of claim 1, wherein the substrate is heated to a temperature within a range from about 20° C. to about 500° C. for a time period of about 60 seconds or less during the surface oxidation process.

### Claim 9 (depends on 8)

The method of claim 8, wherein the temperature is within a range from about 250° C. to about 350° C. and the time period is within a range from about 5 seconds to about 60 seconds during the surface oxidation process.

### Claim 10 (depends on 1)

The method of claim 1, wherein each cobalt layer is deposited from a deposition gas comprising a cobalt source gas and hydrogen gas (H2) during a thermal chemical vapor deposition process.

### Claim 11 (depends on 10)

The method of claim 10, wherein the cobalt source gas is dicobalt hexacarbonyl butylacetylene (CCTBA).

### Claim 12 (depends on 1)

The method of claim 1, wherein each cobalt layer is exposed to the plasma to form each plasma-treated cobalt layer during the plasma process, and the plasma comprises a reagent selected from the group consisting of ammonia (NH3), hydrogen (H2), an ammonia/hydrogen mixture, derivatives thereof, and combinations thereof.

### Claim 13 (depends on 12)

The method of claim 12, wherein each cobalt layer is exposed to a hydrogen plasma for a time period within a range from about 10 seconds to about 180 seconds.

### Claim 14 (depends on 1)

The method of claim 1, further comprising exposing the cobalt oxide layer to a hydrogen plasma to form metallic cobalt layer from the crystalline cobalt film.

### Claim 15 (depends on 1)

The method of claim 1, further comprising depositing a conductive metallic layer comprising a metal on the cobalt oxide layer and thereafter, heating the substrate to diffuse the metal of the conductive metallic layer into the cobalt oxide layer and the crystalline cobalt film.

### Claim 16 (depends on 1)

The method of claim 1, further comprising forming a contact film disposed over the cobalt oxide layer, wherein the contact film comprises at least one conductive material and the conductive material comprises a contact metal selected from the group consisting of copper, aluminum, tungsten, titanium, alloys thereof, and combinations thereof.

### Claim 17

A method for depositing materials on a substrate surface, comprising:
forming a cobalt stack comprising a plurality of plasma-treated cobalt layers over a barrier layer disposed on a substrate by sequentially depositing and treating cobalt layers, wherein each cobalt layer is deposited from a deposition gas comprising a cobalt source gas and hydrogen gas (H2) during a thermal chemical vapor deposition process and subsequently exposed to a plasma to form each of the plasma-treated cobalt layers during a plasma process;
exposing the cobalt stack to an oxygen source gas to form a cobalt oxide layer during a surface oxidation process; and
heating the cobalt stack to a crystallization temperature to form a crystalline cobalt film during a thermal annealing crystallization process.

### Claim 18 (depends on 17)

The method of claim 17, wherein the crystallization temperature is within a range from about 300° C. to about 500° C. during the thermal annealing crystallization process.

### Claim 19

A method for depositing materials on a substrate surface, comprising:
forming a cobalt stack over a barrier layer disposed on a substrate by:
depositing a cobalt layer during a deposition process;
exposing the cobalt layer to a plasma to form a plasma-treated cobalt layer during a plasma process; and
repeating the deposition process and the plasma process to form the cobalt stack comprising a plurality of plasma-treated cobalt layers;
exposing the cobalt stack to an oxygen source gas to form a cobalt oxide layer during a surface oxidation process, wherein the cobalt oxide layer has a thickness within a range from about 5 Å to about 30 Å, and the substrate is heated to a temperature within a range from about 200° C. to about 500° C. for a time period of about 60 seconds or less during the surface oxidation process;
heating the cobalt stack to a crystallization temperature to form a crystalline cobalt film during a thermal annealing crystallization process;
depositing a conductive metallic layer on the crystalline cobalt film, wherein the metal of the conductive metallic layer comprises a metal selected from the group consisting of aluminum, copper, titanium, alloys thereof, and combinations thereof; and
heating the substrate while diffusing the metal of the conductive metallic layer into the crystalline cobalt film.

### Claim 20 (depends on 19)

The method of claim 19, wherein the thickness of the cobalt oxide layer is within a range from about 10 Å to about 20 Å, the temperature is within a range from about 250° C. to about 350° C., and the time period is within a range from about 5 seconds to about 60 seconds during the surface oxidation process.