# US 2012/0252203 A1 · Controlled electroplated solder bumps

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2012/0252203 A1
- Document ID: US20120252203A1
- Status: Published application
- Kind: A1
- Application number: 13/076,881
- Filed: 2011-03-31
- Published: 2012-10-04
- Earliest claimed: 2011-03-31
- Assignees: Globalfoundries Inc.
- Inventors: Christian Schroiff
- Web page: https://patentgrep.com/patent/US20120252203A1

## CPC

- H10W 72/012: {of bump connectors, dummy bumps or thermal bumps}
- H10W 72/0112: {Apparatus for manufacturing bump connectors}
- H10W 72/0198: {batch processes}
- H10W 72/01235: {by plating, e.g. electroless plating or electroplating}
- H10W 72/252: {comprising solid metals or solid metalloids, e.g. PbSn, Ag or Cu}
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

The uniformity of the composition of plated solder bumps from one batch of wafers to another is improved by controlling the rotational speed of the wafers based on the particular solder bump pattern. Embodiments include sequentially horizontal fountain electroplating a pattern of solder bumps, e.g., SnAg solder bumps, on a plurality batches of wafers and controlling the rotational speed of each batch of wafers during electroplating based on a calibration plot of the concentration of a solder bump component, e.g., Ag, as a function of rotational speed for each solder bump pattern, such that the uniformity of the Ag concentration in the patterns of solder bumps is greater than 95%, e.g., greater than 98%. Embodiments further include electroplating in the same plater sequential batches of wafers having both different patterns and different solder bump compositions at the same high throughput.

## Claims

### Claim 1

A method comprising:
forming a solder bump pattern on a batch of wafers by horizontal fountain electroplating;
rotating the wafers during electroplating at a rotational speed; and
controlling the rotational speed of the wafers during electroplating to regulate the concentration of a solder bump component in the solder bump pattern.

### Claim 2 (depends on 1)

The method according to claim 1, comprising controlling the rotational speed depending on the pattern of solder bumps.

### Claim 3 (depends on 1)

The method according to claim 1, comprising:
electroplating a first pattern of solder bumps on a first batch of wafers in a horizontal fountain plater while rotating the first batch of wafers at a first rotational speed;
providing a second batch of wafers to be plated with a second pattern of solder bumps;
adjusting the first rotational speed to a second rotational speed determined by the second pattern of solder bumps; and
electroplating the second pattern of solder bumps on the second batch of wafers while rotating the second batch of wafers at the second rotational speed.

### Claim 4 (depends on 3)

The method according to claim 3, comprising electroplating the first and second batches of wafers at substantially the same throughput and at substantially the same plating rate.

### Claim 5 (depends on 4)

The method according to claim 4, wherein the solder comprises silver (Ag).

### Claim 6 (depends on 5)

The method according to claim 5, wherein the solder also comprises tin (Sn).

### Claim 7 (depends on 4)

The method according to claim 4, comprising controlling the first and second rotational speeds such that the composition of the solder bumps does not vary by more than 5.0% from the first batch of wafers to the second batch of wafers.

### Claim 8 (depends on 6)

The method according to claim 6, comprising controlling the first and second rotational speeds such that the concentration of Ag in the solder bumps does not vary by more than 5.0% from the first batch of wafers to the second batch of wafers.

### Claim 9 (depends on 6)

The method according to claim 6, comprising rotating the first and second batches of wafers at different rotational speeds between 40 and 150 rpm.

### Claim 10 (depends on 8)

The method according to claim 8, comprising rotating the first and second batches of wafers at different rotational speeds between 40 and 150 rpm.

### Claim 11 (depends on 3)

The method according to claim 3, wherein the first and second patterns are different in the arrangement, number, pitch, and/or diameter of the solder bumps.

### Claim 12

A method comprising:
preparing a first calibration plot of the concentration of a solder component in a solder bump as a function of rotational speed for a wafer electroplated with a first pattern of solder bumps;
providing a first batch of wafers to be electroplated with the first pattern of solder bumps;
determining a first rotational speed from the first calibration plot for a predetermined concentration of the solder component; and
electroplating the first pattern of solder bumps on the first batch of wafers in a horizontal fountain plater while rotating the first wafer at the first rotational speed, whereby the composition of the solder bumps in the first pattern is substantially constant.

### Claim 13 (depends on 12)

The method according to claim 12, further comprising:
preparing a second calibration plot of the concentration of the solder component in a solder bump as a function of rotational speed for a wafer electroplated with a second pattern of solder bumps;
providing a second batch of wafers to be electroplated with the second pattern of solder bumps;
determining a second rotational speed from the second calibration plot for the predetermined concentration of the solder component; and
electroplating the second pattern of solder bumps on the second batch of wafers in the same horizontal fountain plater while rotating the second wafer at the second rotational speed.

### Claim 14 (depends on 13)

The method according to claim 13, whereby the composition of the solder bumps does not vary by more than 5.0% from the first wafer to the second wafer.

### Claim 15 (depends on 14)

The method according to claim 14, wherein the solder comprises silver (Ag), and the Ag concentration in the solder bumps does not vary by more than 5.0% from the first batch of wafers to the second batch of wafers.

### Claim 16 (depends on 14)

The method according to claim 14, comprising electroplating the first and second batches of wafers at substantially the same plating rate and at substantially the same throughput.

### Claim 17 (depends on 13)

The method according to claim 13, wherein the first and second patterns are the same or different, the method comprising rotating the first and second batches of wafers such that the solder bumps in the first pattern have a first predetermined composition and the solder bumps in the second pattern have a second predetermined composition different from the first predetermined composition.

### Claim 18 (depends on 16)

The method according to claim 16, comprising rotating the first and second batches of wafers at different rotational speeds between 40 and 150 rpm.

### Claim 19

A method of sequentially electroplating a first pattern of solder bumps on a first batch of wafers and a second pattern of solder bumps on a second batch of wafers in a horizontal fountain plater, the method comprising:
rotating the first batch of wafers at a first rotational speed determined by the first pattern; and
rotating the second batch of wafers at a second rotational speed, different from the first rotational speed, determined by the second pattern.

### Claim 20 (depends on 19)

The method according to claim 19, wherein the first and second patterns are different in the arrangement, number, pitch, and/or diameter of the solder bumps.