# US 2012/0252202 A1 · Semiconductor memory devices and method of manufacturing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2012/0252202 A1
- Document ID: US20120252202A1
- Status: Published application
- Kind: A1
- Application number: 13/244,203
- Filed: 2011-09-23
- Published: 2012-10-04
- Earliest claimed: 2010-11-24
- Inventors: Federica Zanderigo; Maria Gabriella Righini; Giulio Albini; Francesca Sammiceli
- Web page: https://patentgrep.com/patent/US20120252202A1

## CPC

- H10D 30/69: IGFETs having charge trapping gate insulators, e.g. MNOS transistors
- H10B 43/30: characterised by the memory core region
- H10D 30/0413: {of FETs having charge-trapping gate insulators, e.g. MNOS transistors}
- H10D 64/68: characterised by the insulator, e.g. by the gate insulator
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10B: ELECTRONIC MEMORY DEVICES

## Abstract

The semiconductor memory devices include an interfacial improvement resistance layer is formed between a polysilicon layer and a conductive layer in order to improve interfacial resistance between the polysilicon layer and the conductive layer. The method of manufacturing semiconductor memory devices includes forming a polysilicon layer over a semiconductor substrate, amorphizing the polysilicon layer, and stacking an interfacial improvement resistance layer and conductive layers over the amorphized polysilicon layer.

## Claims

### Claim 1

A method of manufacturing semiconductor memory devices, comprising:
forming a polysilicon layer over a semiconductor substrate;
amorphizing the polysilicon layer; and
stacking an interfacial improvement resistance layer and conductive layers over the amorphized polysilicon layer.

### Claim 2 (depends on 1)

The method of claim 1, wherein the polysilicon layer is amorphized using a pre-amorphization implant (PAT) method.

### Claim 3 (depends on 1)

The method of claim 1, wherein the interfacial improvement resistance layer is made of titanium (Ti), tantalum (Ta), or tungsten (W).

### Claim 4 (depends on 1)

The method of claim 1, wherein the conductive layers comprise:
a back tunneling improvement layer formed of a metal nitride layer having a high work function, and
a resistance improvement layer formed of a metal layer.

### Claim 5 (depends on 4)

The method of claim 4, wherein the back tunneling improvement layer is a tantalum nitride (TaN) layer or a titanium nitride (TiN) layer.

### Claim 6 (depends on 4)

The method of claim 4, wherein the resistance improvement layer is a tungsten (W) layer.

### Claim 7 (depends on 6)

The method of claim 6, wherein an anti-diffusion layer is formed of a tungsten nitride (WN) layer and is further formed under the resistance improvement layer.

### Claim 8 (depends on 1)

The method of claim 1, further comprising:
stacking a hard mask layer and photoresist patterns over the conductive layers;
patterning the hard mask layer by an etch process using the photoresist patterns as an etch mask;
removing exposed regions of the conductive layers and the interfacial improvement resistance layer by using the patterned hard mask layer as an etch mask;
removing the photoresist patterns; and
removing exposed regions of the amorphized polysilicon layer.

### Claim 9 (depends on 8)

The method of claim 8, further comprising forming spacers on sidewalls of the patterned hard mask layer, the conductive layers, and the interfacial improvement resistance layer before removing the exposed regions of the amorphized polysilicon layer.

### Claim 10 (depends on 9)

The method of claim 9, wherein the spacers are formed of a nitride layer.

### Claim 11 (depends on 9)

The method of claim 9, wherein the amorphized polysilicon layer is recrystallized when forming the spacers.

### Claim 12

A method of manufacturing semiconductor memory devices, comprising:
forming a polysilicon layer over a semiconductor substrate;
amorphizing the polysilicon layer by a process including implanting impurities into the polysilicon layer;
stacking an interfacial improvement resistance layer over the amorphized polysilicon layer; and
recrystallizing the amorphized polysilicon layer.

### Claim 13 (depends on 12)

The method of claim 12, wherein the polysilicon layer is crystalline before performing the amorphizing of the polysilicon layer.

### Claim 14

A semiconductor memory device, comprising:
a polysilicon layer formed over a semiconductor substrate, wherein the polysilicon layer includes injected impurities;
an interfacial improvement resistance layer formed on the polysilicon layer; and
conductive layers formed over the interfacial improvement resistance layer.

### Claim 15 (depends on 14)

The semiconductor memory device of claim 14, wherein the interfacial improvement resistance layer is made of titanium (Ti), tantalum (Ta), or tungsten (W).

### Claim 16 (depends on 14)

The semiconductor memory device of claim 14, wherein the conductive layers comprise:
a back tunneling improvement layer formed of a metal nitride layer having a high work function, and
a resistance improvement layer formed of a metal layer.

### Claim 17 (depends on 16)

The semiconductor memory device of claim 16, wherein the back tunneling improvement layer is a tantalum nitride (TaN) layer or a titanium nitride (TiN) layer.

### Claim 18 (depends on 16)

The semiconductor memory device of claim 16, wherein the resistance improvement layer is a tungsten (W) layer.

### Claim 19 (depends on 18)

The semiconductor memory device of claim 18, wherein an anti-diffusion layer is formed of a tungsten nitride (WN) layer and is further formed under the resistance improvement layer.