# US 2012/0252192 A1 · Method of growing heteroepitaxial single crystal or large grained semiconductor films on glass substrates and devices thereon

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2012/0252192 A1
- Document ID: US20120252192A1
- Status: Published application
- Kind: A1
- Application number: 13/495,699
- Filed: 2012-06-13
- Published: 2012-10-04
- Earliest claimed: 2011-07-08
- Assignees: Trustees of Dartmouth College; Solar-Tectic LLC
- Inventors: Praveen Chaudhari; Karin Chaudhari; Ashok Chaudhari; Pia Chaudhari; Jifeng Liu
- Web page: https://patentgrep.com/patent/US20120252192A1

## CPC

- C30B 13/02: Zone-melting with a solvent, e.g. travelling solvent process
- C30B 13/24: using electromagnetic waves
- H10F 71/121: {The active layers comprising only Group IV materials}
- H10F 71/1221: {comprising polycrystalline silicon}
- H10P 14/20: of semiconductor materials
- H10P 14/2922: {being non-crystalline insulating materials, e.g. glass or polymers}
- H10P 14/3411: {Silicon, silicon germanium or germanium}
- Y02E 10/546: Polycrystalline silicon PV cells
- Y02E 10/547: Monocrystalline silicon PV cells
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR
- H10F: INORGANIC SEMICONDUCTOR DEVICES SENSITIVE TO INFRARED RADIATION, LIGHT, ELECTROMAGNETIC RADIATION OF SHORTER WAVELENGTH OR CORPUSCULAR RADIATION
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

Inexpensive semiconductors are produced by depositing a single crystal or large grained silicon on an inexpensive substrate. These semiconductors are produced at low enough temperatures such as temperatures below the melting point of glass. Semiconductors produced are suitable for semiconductor devices such as photovoltaics or displays

## Claims

### Claim 1

A method of growing semiconductor film comprising the steps of:
providing a substrate;
depositing a eutectic alloy film on the substrate;
focusing a heated line source on a surface of said eutectic alloy film; and
scanning, in a direction, said heated line source across the surface of said eutectic alloy thin film,
wherein a semiconductor film is deposited from a solution of said eutectic alloy film onto said substrate during said scanning process,
wherein said semiconductor film nucleates on said substrate and grows along the scanning direction as said heated line source passes across the thin film surface.

### Claim 2 (depends on 1)

The method of claim 1, wherein the eutectic alloy film comprises a metal and a semiconductor.

### Claim 3 (depends on 1)

The method of claim 1, wherein the eutectic alloy film is Au—Si.

### Claim 4 (depends on 3)

The method of claim 3, wherein the Au diffuses onto the top of the Si film during the heated line scanning process and is etched away after the growth of the Si film.

### Claim 5 (depends on 1)

The method of claim 1, wherein the eutectic alloy film is Al—Si.

### Claim 6 (depends on 1)

The method of claim 1, wherein the eutectic alloy film is Ag—Si.

### Claim 7 (depends on 1)

The method of claim 1, wherein the eutectic alloy film is Sn—Si.

### Claim 8 (depends on 1)

The method of claim 1, wherein the heat source is a laser.

### Claim 9 (depends on 8)

The method of claim 8, wherein said laser is a beam and is shaped as a line.

### Claim 10 (depends on 1)

The method of claim 1, wherein a thermal gradient is produced by the passing of the heated line source, said thermal gradient causing the semiconductor grains to continue to grow rather than nucleate a new grain

### Claim 11 (depends on 1)

The method of claim 1, wherein said deposition occurs at a temperature below the softening temperature of glass.

### Claim 12 (depends on 1)

The method of claim 1, wherein said semiconductor growth is in-plane along the scanning direction of said heated line source

### Claim 13 (depends on 1)

The method of claim 1, wherein the semiconductor film is large grained.

### Claim 14 (depends on 1)

The method of claim 1, wherein the substrate is glass.

### Claim 15

A method of growing single crystal semiconductor film comprising the steps of:
providing a substrate;
placing a thin strip of single crystal semiconductor at one end of the substrate;
depositing a eutectic alloy film on a surface of the single crystal strip and the substrate;
directing a heated line source on top of the single crystal strip; and
scanning the heated line source away from the single crystal strip to propagate its crystal orientation across the entire semiconductor thin film.

### Claim 16 (depends on 15)

The method of claim 15, wherein the eutectic alloy film comprises a metal and a semiconductor.

### Claim 17 (depends on 15)

The method of claim 15, wherein the eutectic alloy film is Au—Si.

### Claim 18 (depends on 17)

The method of claim 17, wherein the Au diffuses onto the top of the Si film during the heated line scanning process and is etched away after the growth of the Si film.

### Claim 19 (depends on 15)

The method of claim 15, wherein the eutectic alloy film is Al—Si.

### Claim 20 (depends on 15)

The method of claim 15, wherein the eutectic alloy film is Ag—Si.

### Claim 21 (depends on 15)

The method of claim 15, wherein the eutectic alloy film is Sn—Si.

### Claim 22 (depends on 15)

The method of claim 15, wherein the heat source is a laser.

### Claim 23 (depends on 22)

The method of claim 22, wherein said laser is a beam and is shaped as a line.

### Claim 24 (depends on 15)

The method of claim 15, wherein a thermal gradient is produced by the passing of the heated line source, said thermal gradient causing the semiconductor grains to continue to grow rather than nucleate a new grain

### Claim 25 (depends on 15)

The method of claim 15, wherein said deposition occurs at a temperature below the softening temperature of glass

### Claim 26 (depends on 15)

The method of claim 15, wherein after the heated line scanning process, the semiconductor film is single crystal.

### Claim 27 (depends on 15)

The method of claim 15, wherein the substrate is glass.

### Claim 28 (depends on 15)

The method of claim 15, wherein the single crystal strip is primarily single crystal Si.