# US 2012/0252188 A1 · Plasma processing method and device isolation method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2012/0252188 A1
- Document ID: US20120252188A1
- Status: Published application
- Kind: A1
- Application number: 13/432,151
- Filed: 2012-03-28
- Published: 2012-10-04
- Earliest claimed: 2011-03-31
- Assignees: Tokyo Electron Limited
- Inventors: Ryota YONEZAWA; Kazuyoshi Yamazaki; Masaki Sano
- Web page: https://patentgrep.com/patent/US20120252188A1

## CPC

- H10P 14/6316: {Formation by nitridation, e.g. nitridation of the substrate}
- C23C 8/36: using ionised gases, e.g. ionitriding
- H10P 14/6309: {of silicon in uncombined form, i.e. pure silicon}
- H10P 14/6522: {introduced into a nitride material, e.g. changing SiN to SiON}
- H10P 14/6526: {introduced into an oxide material, e.g. changing SiO to SiON}
- H10W 10/014: {using trench refilling with dielectric materials, e.g. shallow trench isolations}
- H10W 10/17: formed using trench refilling with dielectric materials, e.g. shallow trench isolations
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

A plasma processing method for use in device isolation by shallow trench isolation in which an insulating film is embedded in a trench formed in silicon and the insulating film is planarized to form a device isolation film, the method includes a plasma nitriding the silicon of an inner wall surface of the trench by using a plasma before embedding the insulating film in the trench. The plasma nitriding is performed by using a plasma of a processing gas containing a nitrogen-containing gas under conditions in which a processing pressure ranges from 1.3 Pa to 187 Pa and a ratio of a volumetric flow rate of the nitrogen-containing gas to a volumetric flow rate of the entire processing gas ranges from 1% to 80% such that a silicon nitride film is formed on the inner wall surface of the trench to have a thickness of 1 to 10 nm.

## Claims

### Claim 1

A plasma processing method for use in device isolation by shallow trench isolation in which an insulating film is embedded in a trench formed in silicon and the insulating film is planarized to form a device isolation film, the method comprising:
a plasma nitriding the silicon of an inner wall surface of the trench by using a plasma before embedding the insulating film in the trench,
wherein the plasma nitriding is performed by using a plasma of a processing gas containing a nitrogen-containing gas under conditions in which a processing pressure ranges from 1.3 Pa to 187 Pa and a ratio of a volumetric flow rate of the nitrogen-containing gas to a volumetric flow rate of the entire processing gas ranges from 1% to 80% such that a silicon nitride film is formed on the inner wall surface of the trench to have a thickness of 1 to 10 nm.

### Claim 2 (depends on 1)

The plasma processing method of claim 1, wherein the processing pressure in said plasma nitriding ranges from 1.3 Pa to 40 Pa.

### Claim 3 (depends on 1)

The plasma processing method of claim 1, further comprising, after said plasma nitriding, oxidizing the silicon nitride film by using a plasma of a processing gas containing an oxygen-containing gas to modify the silicon nitride film into a silicon oxynitride film.

### Claim 4 (depends on 2)

The plasma processing method of claim 2, further comprising, after said plasma nitriding, oxidizing the silicon nitride film by using a plasma of a processing gas containing an oxygen-containing gas to modify the silicon nitride film into a silicon oxynitride film.

### Claim 5 (depends on 3)

The plasma processing method of claim 3, wherein in said plasma oxidation, a processing pressure ranges from 1.3 Pa to 1000 Pa, and a ratio of a volumetric flow rate of the oxygen-containing gas to a volumetric flow rate of the entire processing gas ranges from 1% to 80%.

### Claim 6 (depends on 4)

The plasma processing method of claim 4, wherein in said plasma oxidation, a processing pressure ranges from 1.3 Pa to 1000 Pa, and a ratio of a volumetric flow rate of the oxygen-containing gas to a volumetric flow rate of the entire processing gas ranges from 1% to 80%.

### Claim 7 (depends on 3)

The plasma processing method of claim 3, wherein said plasma nitriding and said plasma oxidation are performed by using a plasma processing apparatus which generates a plasma by introducing a microwave into a processing chamber through a planar antenna having holes.

### Claim 8 (depends on 6)

The plasma processing method of claim 6, wherein said plasma nitriding and said plasma oxidation are performed by using a plasma processing apparatus which generates a plasma by introducing a microwave into a processing chamber through a planar antenna having holes.

### Claim 9

A device isolation method comprising:
forming a trench in silicon;
embedding an insulating film in the trench;
planarizing the insulating film to form an device isolation film; and
before said embedding the insulating film in the trench, a plasma nitriding an inner wall surface of the trench by using a plasma of a processing gas containing a nitrogen-containing gas under conditions in which a processing pressure ranges from 1.3 Pa to 187 Pa and a ratio of a volumetric flow rate of the nitrogen-containing gas to a volumetric flow rate of the entire processing gas ranges from 1% to 80% such that a silicon nitride film is formed to have a thickness of 1 to 10 nm.

### Claim 10 (depends on 9)

The device isolation method of claim 9, wherein the processing pressure in said plasma nitriding ranges from 1.3 Pa to 40 Pa.

### Claim 11 (depends on 9)

The device isolation method of claim 9, further comprising, after said plasma nitriding, a plasma oxidation step of oxidizing the silicon nitride film by using a plasma of a processing gas containing an oxygen-containing gas to modify the silicon nitride film into a silicon oxynitride film.

### Claim 12 (depends on 11)

The device isolation method of claim 11, wherein in said plasma oxidation, a processing pressure ranges from 1.3 Pa to 1000 Pa, and a ratio of a volumetric flow rate of the oxygen-containing gas to a volumetric flow rate of the entire processing gas ranges from 1% to 80%.

### Claim 13 (depends on 11)

The device isolation method of claim 11, wherein said plasma nitriding and said plasma oxidation are performed by using a plasma processing apparatus which generates a plasma by introducing a microwave into a processing chamber through a planar antenna having holes.

### Claim 14 (depends on 10)

The device isolation method of claim 10, further comprising, after said plasma nitriding, oxidizing the silicon nitride film by using a plasma of a processing gas containing an oxygen-containing gas to modify the silicon nitride film into a silicon oxynitride film.

### Claim 15 (depends on 14)

The device isolation method of claim 14, wherein in said plasma oxidation, a processing pressure ranges from 1.3 Pa to 1000 Pa, and a ratio of a volumetric flow rate of the oxygen-containing gas to a volumetric flow rate of the entire processing gas ranges from 1% to 80%.

### Claim 16 (depends on 15)