# US 2012/0252126 A1 · Method for analyzing and detecting calcium element in ore

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2012/0252126 A1
- Document ID: US20120252126A1
- Status: Published application
- Kind: A1
- Application number: 13/504,684
- Filed: 2009-12-30
- Published: 2012-10-04
- Earliest claimed: 2009-10-29
- Assignees: Jiangxi Rare Earth and Rare Metals Tungsten Group Holding Co., Ltd.
- Inventors: Yulan Liang; Ling Peng; Zhijian Zhao
- Web page: https://patentgrep.com/patent/US20120252126A1

## CPC

- G01N 21/79: Photometric titration
- G01N 31/16: using titration
- G01N 33/24: Earth materials (G01N33/42 takes precedence)
- G01N: INVESTIGATING OR ANALYSING MATERIALS BY DETERMINING THEIR CHEMICAL OR PHYSICAL PROPERTIES (measuring or testing apparatus or processes other than immunoassay, involving enzymes or microorganisms C12M, C12Q)

## Abstract

A method for determining the content of calcium element in an ore is provided. It includes: decomposing the ore with hydrochloric acid and nitric acid under heating condition, adding perchloric acid, cooling, adding a small amount of water and boiling the solution to dissolve the salts, then cooling, diluting to the constant volume, filtering into a dry beaker with dry filter-paper, masking interfering ions with triethanolamine, adjusting the pH value of the solution with KOH, using calcein-thymolphthalein as indicator, and determinating the content of calcium with EDTA titrimetry.

## Claims

### Claim 1

A method for analyzing and detecting calcium element in an ore, characterized by the following steps:
(1) adding hydrochloric acid and nitric acid into a sample for heat treatment, adding perchloric acid till smoking, and after cooling, adding a small amount of water to dissolve the salts by boiling;
(2) after cooling the test solution, transferring it to a 100-250 mL volumetric flask and bringing to volume, and filtering into a dry beaker through a dry filter-paper to separate calcium at least in part from impurity elements such as tungsten and molybdenum;
(3) pipetting an appropriate amount of filtrate and adding triethanolamine to mask interfering ions;
(4) adjusting the pH value of the solution with potassium hydroxide;
(5) using calcein-thymolphthalein as a mixed indicator; and
(6) titrating directly for calcium content with a standard EDTA solution and calculating for analysis results.

### Claim 2 (depends on 1)

The method according to claim 1, characterized in that in step (1), the hydrochloric acid is a concentrated hydrochloric acid with a density of 1.19 g/mL, the nitric acid is a concentrated nitric acid with a density of 1.42 g/mL, and the perchloric acid is a concentrated acid with a density of 1.67 g/mL.

### Claim 3 (depends on 1)

The method according to claim 1, characterized in that a part of impurity elements of tungsten and molybdenum are removed in step (2).

### Claim 4 (depends on 1)

The method according to claim 1, characterized in that the concentration of triethanolamine solution in step (3) is 30%-50%.

### Claim 5 (depends on 1)

The method according to claim 1, characterized in that in step (4), the pH value of the solution is adjusted with potassium hydroxide with a concentration of 100-200 g/L.

### Claim 6 (depends on 1)

The method according to claim 1, characterized in that in step (5), calcein-thymolphthalein is used as a mixed indicator.

### Claim 7 (depends on 1)

The method according to claim 1, characterized in that in step (6), the concentration of the standard EDTA solution for titrating calcium element is 0.02-0.03 mol/L.