# US 2012/0251931 A1 · Transfer mask, method of manufacturing a transfer mask, and method of manufacturing a semiconductor device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2012/0251931 A1
- Document ID: US20120251931A1
- Status: Published application
- Kind: A1
- Application number: 13/501,348
- Filed: 2010-10-08
- Published: 2012-10-04
- Earliest claimed: 2009-10-12
- Assignees: Hoya Corporation
- Inventors: Masahiro Hashimoto; Kazuya Sakai; Toshiyuki Suzuki; Kazunori Ono
- Web page: https://patentgrep.com/patent/US20120251931A1

## CPC

- G03F 1/32: Attenuating PSM [att-PSM], e.g. halftone PSM or PSM having semi-transparent phase shift portion,; Preparation thereof
- G03F 1/54: Absorbers, e.g. of opaque materials
- G03F 1/80: Etching
- G03F: PHOTOMECHANICAL PRODUCTION OF TEXTURED OR PATTERNED SURFACES, e.g. FOR PRINTING, FOR PROCESSING OF SEMICONDUCTOR DEVICES; MATERIALS THEREFOR; ORIGINALS THEREFOR; APPARATUS SPECIALLY ADAPTED THEREFOR; (phototypographic composing devices B41B; photosensitive materials or processes for photographic purposes G03C; electrophotography, sensitive layers or processes therefor G03G)

## Abstract

Provided is a transfer mask which has a transfer pattern formed in a pattern-forming thin film provided on a transparent substrate and is adapted to be applied with exposure light having a wavelength of 200 nm or less. The pattern-forming thin film is made of a material containing silicon an a transition metal other than chromium and the chromium content in the film is less than 1.0×1018 atoms/cm3.

## Claims

### Claim 1

A transfer mask having a transfer pattern formed in a pattern-forming thin film which is provided on a transparent substrate,
wherein,
the pattern-forming thin film is made of a material containing silicon and a transition metal other than chromium,
the transfer mask is manufactured using a mask blank in which the pattern-forming thin film and a chromium-based thin film made of a material containing chromium are laminated in this order on the transparent substrate, and
a chromium content in the pattern-forming thin film is less than 1.0×1018 atoms/cm3.

### Claim 2 (depends on 1)

The transfer mask according to claim 1, wherein the transition metal in the pattern-forming thin film is molybdenum.

### Claim 3 (depends on 1)

The transfer mask according to claim 1, wherein the pattern-forming thin film is a light-shielding film having an optical density of 2.5 or more with respect to exposure light.

### Claim 4 (depends on 3)

The transfer mask according to claim 3, wherein the pattern-forming thin film is the light-shielding film having a laminated structure of at least two or more layers comprising a light-shielding layer and a front-surface antireflection layer from the transparent substrate side.

### Claim 5 (depends on 1)

The transfer mask according to claim 1, wherein the pattern-forming thin film has the transfer pattern following a DRAM hp45 nm generation.

### Claim 6 (depends on 1)

The transfer mask according to claim 1, wherein the pattern-forming thin film is a halftone phase shift film;
the chromium-based thin film forming a light-shielding band in a light-shielding band region around a transfer pattern region;
no chromium-based thin film being left on an upper surface of the pattern-forming thin film in the transfer pattern region.

### Claim 7

A method of manufacturing a transfer mask using a mask blank in which a pattern-forming thin film made of a material containing silicon and a transition metal other than chromium and a chromium-based thin film made of a material containing chromium are laminated in this order on a transparent substrate,
wherein the method produces the transfer mask by carrying out in the following order:
a step of forming a resist film having a transfer pattern on the chromium-based thin film;
a step of forming a transfer pattern in the chromium-based thin film using the resist film having the transfer pattern as a mask;
a step of forming a transfer pattern in the pattern-forming thin film using the chromium-based thin film having the transfer pattern as a mask; and
a step of removing the chromium-based thin film by etching, and
wherein the method further comprises a cleaning step of carrying out one or more of alkaline solution cleaning, hot water cleaning, and ozone-containing water cleaning on the produced transfer mask until a chromium content in the transfer pattern of the pattern-forming thin film becomes less than 1.0×1018 atoms/cm3.

### Claim 8 (depends on 7)

The method of manufacturing a transfer mask according to claim 7, wherein the cleaning step carries out the alkaline solution cleaning, the hot water cleaning, and the ozone-containing water cleaning in this order.

### Claim 9 (depends on 7)

The method of manufacturing a transfer mask according to claim 7, wherein the alkaline solution is an aqueous solution containing ammonia and hydrogen peroxide.

### Claim 10 (depends on 7)

The method of manufacturing a transfer mask according to claim 7, wherein the transition metal in the pattern-forming thin film is molybdenum.

### Claim 11 (depends on 7)

The method of manufacturing a transfer mask according to claim 7, wherein the pattern-forming thin film is a light-shielding film having an optical density of 2.5 or more with respect to exposure light, and
the chromium-based thin film is entirely removed in the step of removing by etching.

### Claim 12 (depends on 11)

The method of manufacturing a transfer mask according to claim 11, wherein the pattern-forming thin film is the light-shielding film having a laminated structure of at least two or more layers comprising a light-shielding layer and a front-surface antireflection layer from the transparent substrate side.

### Claim 13 (depends on 7)

The method of manufacturing a transfer mask according to claim 7, wherein the pattern-forming thin film has the transfer pattern following a DRAM hp45 nm generation.

### Claim 14 (depends on 7)

The method of manufacturing a transfer mask according to claim 7, wherein the pattern-forming thin film is a halftone phase shift film,
a laminated structure of the chromium-based thin film and the pattern-forming thin film has an optical density of 2.5 or more with respect to exposure light, and
the chromium-based thin film is removed in its region other than a light-shielding band region around a transfer pattern region in the step of removing the chromium-based thin film by etching, thereby forming a light-shielding band.

### Claim 15 (depends on 1)

A method of manufacturing a semiconductor device, comprising forming a circuit pattern on a semiconductor wafer using the transfer mask according to claim 1.

### Claim 16 (depends on 7)

A method of manufacturing a semiconductor device, comprising forming a circuit pattern on a semiconductor wafer using the transfer mask manufactured by the method of manufacturing a transfer mask according to claim 7.

### Claim 17 (depends on 15)

The method of manufacturing a semiconductor device according to claim 15, wherein the circuit pattern formed on the semiconductor wafer includes a circuit pattern following a DRAM hp45 nm generation.

### Claim 18 (depends on 1)

The transfer mask according to claim 1, wherein the transfer mask is adapted to be applied with exposure light having a wavelength of 200 nm or less.

### Claim 19 (depends on 1)

The transfer mask according to claim 1, wherein the chromium-based thin film is not left on an upper surface of the pattern-forming thin film.

### Claim 20 (depends on 6)

The transfer mask according to claim 6, wherein a laminated constitution of the chromium-based thin film and the pattern-forming thin film has an optical density of 2.5 or more with respect to exposure light.

### Claim 21

A transfer mask having a transfer pattern formed in a pattern-forming thin film which is provided on a transparent substrate, wherein:
the pattern-forming thin film in a transfer pattern region is a halftone phase shift film;
the pattern-forming thin film in the transfer pattern region being made of a material containing silicon and a transition metal other than chromium, the chromium content in the pattern-forming thin film being less than 1.0×1018 atoms/cm3;
the chromium-based thin film, made of a material containing chromium, forming a light-shielding band on an upper surface of the pattern-forming thin film in a light-shielding band region around the transfer pattern region;
no chromium-based thin film being present on the upper surface of the pattern-forming thin film in the transfer pattern region.

### Claim 22 (depends on 21)

The transfer mask according to claim 21, wherein the transfer mask is adapted to be applied with exposure light having a wavelength of 200 nm or less.

### Claim 23 (depends on 7)

The transfer mask according to claim 7, wherein the transfer mask is adapted to be applied with exposure light having a wavelength of 200 nm or less.

### Claim 24 (depends on 21)

A method of manufacturing a semiconductor device, comprising forming a circuit pattern on a semiconductor wafer using the transfer mask according to claim 21.

### Claim 25 (depends on 16)

The method of manufacturing a semiconductor device according to claim 16, wherein the circuit pattern formed on the semiconductor wafer includes a circuit pattern following a DRAM hp45 nm generation.