# US 2012/0251897 A1 · Aluminum Air Battery Including a Composite Anode

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2012/0251897 A1
- Document ID: US20120251897A1
- Status: Published application
- Kind: A1
- Application number: 13/056,476
- Filed: 2010-09-30
- Published: 2012-10-04
- Earliest claimed: 2010-09-30
- Assignees: Empire Technology Development LLC
- Inventors: Thomas A. Yager; Ezekiel Kruglick
- Web page: https://patentgrep.com/patent/US20120251897A1

## CPC

- H01M 12/06: with one metallic and one gaseous electrode
- H01M 4/0438: {by electrochemical processing (electroless electrochemical plating C23C18/54)}
- H01M 4/366: {as layered products}
- H01M 4/38: of elements or alloys
- H01M 4/42: Alloys based on zinc
- H01M 4/628: {Inhibitors, e.g. gassing inhibitors, corrosion inhibitors}
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A method to produce an aluminium air battery, comprising: forming a selectively reactive coating on a surface of an anode core to form a composite anode, the selectively reactive coating comprising a zinc alloy and the anode core comprising aluminium; and storing an electrolyte in contact with the composite anode, wherein the selectively reactive coating is capable of chemically reacting with the electrolyte during discharging of the aluminium air battery the reactive coating may also include an anode corrosion inhibitor material consisting of one or more of indium, gallium, lead, thallium or mercury

## Claims

### Claim 1

A method to produce an aluminum air battery, comprising:
forming a selectively reactive coating on a surface of an anode core to form a composite anode, the selectively reactive coating comprising a zinc alloy and the anode core comprising aluminum; and
storing an electrolyte in contact with the composite anode, wherein the selectively reactive coating is capable of chemically reacting with the electrolyte during discharging of the aluminum air battery.

### Claim 2 (depends on 1)

The method of claim 1, wherein forming comprises forming a selectively reactive coating comprising at least one or more of indium, gallium, lead, thallium, or mercury.

### Claim 3 (depends on 1)

The method of claim 1, wherein the forming of the selectively reactive coating comprises alloying a corrosion resistant material and zinc together to form the selectively reactive coating via heat treatment, wherein the corrosion resistant material comprises one or more of indium, gallium, lead, thallium, or mercury.

### Claim 4 (depends on 1)

The method of claim 1, wherein the forming of the selectively reactive coating comprises alloying a corrosion resistant material and zinc together to form the selectively reactive coating via heat treatment, wherein the corrosion resistant material comprises one or more of indium, gallium, lead, thallium, or mercury, and wherein the selectively reactive coating comprises a ratio of corrosion resistant material to zinc from one hundred parts per million to one thousand parts per million.

### Claim 5 (depends on 1)

The method of claim 1, wherein the forming of the selectively reactive coating comprises:
applying zincate to the anode core to form an initial zinc layer;
depositing zinc on the initial zinc layer;
applying a corrosion resistant material to the zinc, wherein the corrosion resistant material is capable of enhancing the ability of the selectively reactive coating to not chemically react with the electrolyte during storage of the aluminum air battery; and
alloying the corrosion resistant material and zinc to form the selectively reactive coating.

### Claim 6 (depends on 1)

The method of claim 1, wherein the forming of the selectively reactive coating comprises:
applying zincate to the anode core via immersion to form an initial zinc layer;
depositing zinc on the initial zinc layer via an electrochemical zinc plating bath;
applying a corrosion resistant material to the zinc via immersion; and
alloying the corrosion resistant material and zinc to form the selectively reactive coating via heat treatment, wherein the corrosion resistant material is capable of enhancing the ability of the zinc to not chemically react with the electrolyte during storage of the aluminum air battery, wherein the corrosion resistant material comprises one or more of indium, gallium, lead, thallium, or mercury, and wherein the selectively reactive coating comprises a ratio of corrosion resistant material to zinc from one hundred parts per million to one thousand parts per million.

### Claim 7 (depends on 1)

The method of claim 1, wherein the electrolyte comprises an alkaline electrolyte.

### Claim 8

An aluminum air battery, comprising:
a composite anode, wherein the composite anode comprises:
an anode core, wherein the anode core comprises aluminum,
a selectively reactive coating coupled to the surface of the anode core, wherein the selectively reactive coating comprises a zinc alloy;
a battery housing, the battery housing containing the composite anode; and
an electrolyte stored in the battery housing in contact with the composite anode, wherein the selectively reactive coating is capable of chemically reacting with the electrolyte during discharging of the aluminum air battery

### Claim 9 (depends on 8)

The aluminum air battery of claim 8, wherein the zinc alloy of the selectively reactive coating comprises a corrosion resistant material, wherein the corrosion resistant material comprises one or more of indium, gallium, lead, thallium, or mercury, and wherein the selectively reactive coating comprises a ratio of corrosion resistant material to zinc from one hundred parts per million to one thousand parts per million.

### Claim 10 (depends on 8)

The aluminum air battery of claim 8, wherein the electrolyte comprises potassium hydroxide and/or sodium hydroxide.

### Claim 11 (depends on 8)

The aluminum air battery of claim 8, wherein the aluminum air battery does not include a storage tank capable of storing the electrolyte separate from the composite anode.

### Claim 12 (depends on 8)

The aluminum air battery of claim 8, wherein the aluminum air battery does not include a pump system capable of controlling the flow of the electrolyte to the composite anode.

### Claim 13

An aluminum air battery, comprising:
a composite anode, wherein the composite anode comprises:
an anode core, wherein the anode core comprises aluminum,
a zinc coating coupled to the surface of the anode core;
an anode corrosion inhibitor electrically connected to the composite anode, wherein the anode corrosion inhibitor comprises:
an inert substrate core, wherein the inert substrate core is electrically connected to the composite anode,
an anode corrosion inhibitor material coupled to the inert substrate core, wherein the anode corrosion inhibitor material comprises one or more of indium, gallium, lead, thallium, or mercury; and
a battery housing, the battery housing containing the composite anode; and
an electrolyte stored in the battery housing in contact with the composite anode, wherein the anode corrosion inhibitor inhibits a chemical reaction between the composite anode and the electrolyte during storage of the aluminum air battery.

### Claim 14 (depends on 13)

The aluminum air battery of claim 13, wherein the inert substrate core has a positive standard electric potential greater than zinc.

### Claim 15 (depends on 13)

The aluminum air battery of claim 13, wherein inert substrate core comprises one or more of copper, gold, palladium, platinum, cobalt, or nickel.

### Claim 16 (depends on 13)

The aluminum air battery of claim 13, wherein the electrolyte comprises potassium hydroxide and/or sodium hydroxide.

### Claim 17 (depends on 13)

The aluminum air battery of claim 13, wherein the aluminum air battery does not include a storage tank capable of storing the electrolyte separate from the composite anode.

### Claim 18 (depends on 13)

The aluminum air battery of claim 13, wherein the aluminum air battery does not include a pump system capable of controlling the flow of the electrolyte to the composite anode.

### Claim 19

A composite anode, comprising:
an anode core, wherein the anode core comprises aluminum; and
a selectively reactive coating coupled to the surface of the anode core, wherein the selectively reactive coating comprises a zinc alloy,
wherein the zinc alloy of the selectively reactive coating comprises a corrosion resistant material, wherein the corrosion resistant material comprises one or more of indium, gallium, lead, thallium, or mercury.

### Claim 20 (depends on 19)

The composite anode of claim 19, wherein the selectively reactive coating comprises a ratio of corrosion resistant material to zinc from one hundred parts per million to one thousand parts per million.