# US 2012/0251888 A1 · Mixed Carbon Material and Negative Electrode for Nonaqueous Secondary Battery

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2012/0251888 A1
- Document ID: US20120251888A1
- Status: Published application
- Kind: A1
- Application number: 13/247,433
- Filed: 2011-09-28
- Published: 2012-10-04
- Earliest claimed: 2009-03-30
- Assignees: Chuo Denki Kogyo Co., Ltd.; Sumitomo Metal Industries, Ltd.
- Inventors: Hiroshi Yamamoto; Tatsuo Nagata; Tooru Fujiwara
- Web page: https://patentgrep.com/patent/US20120251888A1

## CPC

- H01M 4/587: for inserting or intercalating light metals
- C01B 32/05: Preparation or purification of carbon not covered by groups C01B32/15, C01B32/20, C01B32/25, C01B32/30
- C01B 32/21: After-treatment
- H01M 4/131: Electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- H01M 4/1393: of electrodes based on carbonaceous material, e.g. graphite-intercalation compounds or CFx
- H01M 4/364: {as mixtures}
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

The present invention provides a mixed carbon material which comprises carbon material A and carbon material B and which is a carbon material suitable for a negative electrode material which can provide a nonaqueous secondary battery having a low irreversible capacity and having a negative electrode with a high capacity and high charge acceptance. Carbon material A and carbon material B both have cores made of graphite powder and a surface carbon material in the form of at least one of amorphous carbon and turbostratic carbon adhered to or coated on at least a portion of the surface of the graphite powder. The compressed density is 1.80-1.90 g/cm3 for carbon material A alone, 1.45-1.65 g/cm3 for carbon material B alone, and 1.75-1.84 g/cm3 for the mixed carbon material.

## Claims

### Claim 1

A mixed carbon material comprising carbon material A and carbon material B, wherein
carbon material A and carbon material B both have cores made of graphite powder and a surface carbon material adhered to and/or coated on at least a portion of the surface of the graphite powder,
the surface carbon material is at least one of amorphous carbon and turbostratic carbon,
the compressed density which is defined below is 1.80-1.90 g/cm3 for carbon material A alone, 1.45-1.65 g/cm3 for carbon material B alone, and 1.75-1.84 g/cm3 for the mixed carbon material,
the average particle diameter of carbon material B is at most 14 μm and is smaller than the average particle diameter of carbon material A, and
the specific surface areas of carbon material A and carbon material B are at most 4 m2/g and at most 6 m2/g, respectively,
the compressed density being the density of a powder when 1.00 grams of the powder are packed into a cylindrical mold with a diameter of 15 mm, a pressing force of 8.7 kN is applied to the powder, and then the pressing force is reduced to 0.15 kN.

### Claim 2 (depends on 1)

A mixed carbon material as set forth in claim 1 wherein the mixing ratio of carbon material A to carbon material B is from 90:10 to 60:40 as a mass ratio.

### Claim 3

A negative electrode for a nonaqueous secondary battery having a negative electrode material including a mixed carbon material comprising carbon material A and carbon material B, wherein
carbon material A and carbon material B both have cores made of graphite powder and a surface carbon material adhered to and/or coated on at least a portion of the surface of the graphite powder,
the surface carbon material is at least one of amorphous carbon and turbostratic carbon,
the compressed density which is defined below is 1.80-1.90 g/cm3 for carbon material A alone, 1.45-1.65 g/cm3 for carbon material B alone, and 1.75-1.84 g/cm3 for the mixed carbon material,
the average particle diameter of carbon material B is at most 14 μm and is smaller than the average particle diameter of carbon material A, and
the specific surface areas of carbon material A and carbon material B are at most 4 m2/g and at most 6 m2/g, respectively,
the compressed density being the density of a powder when 1.00 grams of the powder are packed into a cylindrical mold with a diameter of 15 mm, a pressing force of 8.7 kN is applied to the powder, and then the pressing force is reduced to 0.15 kN.

### Claim 4 (depends on 3)

A negative electrode for a nonaqueous secondary battery as set forth in claim 3 wherein the mixing ratio of carbon material A to carbon material B is from 90:10 to 60:40 as a mass ratio.