# US 2012/0251882 A1 · Composite, electrode active material for secondary lithium battery including the composite, method of preparing the composite, anode for secondary lithium battery including the electrode active material, and secondary lithium battery including the anode

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2012/0251882 A1
- Document ID: US20120251882A1
- Status: Published application
- Kind: A1
- Application number: 13/243,851
- Filed: 2011-09-23
- Published: 2012-10-04
- Earliest claimed: 2011-03-30
- Assignees: Samsung SDI Co., Ltd.
- Inventors: Sung-Hwan Moon; Yury Matulevich; Jae-Hyuk Kim; Hee-Young Chu; Myung-Hwan Jeong; Chang-Ui Jeong; Jong-Seo Choi
- Web page: https://patentgrep.com/patent/US20120251882A1

## CPC

- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 4/366: {as layered products}
- H01M 4/485: of mixed oxides or hydroxides for inserting or intercalating light metals, e.g. LiTi2O4 or LiTi2OxFy (H01M4/505, H01M4/525 take precedence)
- Y02E 60/10: Energy storage using batteries
- Y02E 60/50: Fuel cells
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A composite includes a compound selected from the group consisting of a lithium lanthanum zirconium oxide and a lithium lanthanum tantalum oxide; a lanthanum oxide; and an oxide selected from the group consisting of a lanthanum zirconium oxide and a lanthanum tantalum oxide. An electrode active material for a secondary lithium battery may include such composite. Methods of preparing the composite, an electrode for a secondary lithium battery including the electrode active material, and a secondary lithium battery including the electrode are disclosed.

## Claims

### Claim 1

A composite, comprising:
a compound selected from the group consisting of a compound represented by Formula 1 below and a compound represented by Formula 2 below;
a lanthanum oxide (La2O3); and
an oxide selected from the group consisting of a lanthanum zirconium oxide (La2Zr2O7) and a lanthanum tantalum oxide (La2Ta2O7):
L7+xM3−xZr2O12 [Formula 1]
wherein, in Formula 1, L is an alkali metal,
M is a tri-valent metal, and
x is a number of 0 to 3, and
L5+aMbTa2O12 [Formula 2]
wherein, in Formula 2, L is an alkali metal,
M is a tri-valent metal,
a is a number that is greater than 0 and equal to or less than 3, and
b is a number that is greater than 0 and equal to or less than 3.

### Claim 2 (depends on 1)

The composite of claim 1, wherein in Formulae 1 and 2, L is selected from the group consisting of Li, Na, and K.

### Claim 3 (depends on 1)

The composite of claim 1, wherein, in Formulae 1 and 2, M is La or Gd.

### Claim 4 (depends on 1)

The composite of claim 1, wherein the compound represented by Formula 1 is Li7La3Zr2O12.

### Claim 5 (depends on 1)

The composite of claim 1, wherein the compound represented by Formula 2 is Li5La3Ta2O12.

### Claim 6 (depends on 1)

The composite of claim 1, wherein a ratio of a main peak intensity of a Bragg 2θ angle of the lanthanum oxide (La2O3) in an X-ray diffraction spectrum to a main peak intensity of a Bragg 2θ angle of the compound selected from the group consisting of the compound represented by Formula 1 and the compound represented by Formula 2 in an X-ray diffraction spectrum is 35:100 to 45:100.

### Claim 7 (depends on 1)

The composite of claim 1, wherein a ratio of a main peak intensity of a Bragg 2θ angle of the oxide selected from the group consisting of the lanthanum zirconium oxide and the lanthanum tantalum oxide in an X-ray diffraction spectrum to a main peak intensity of a Bragg 2θ angle of the compound selected from the group consisting of the compound represented by Formula 1 and the compound represented by Formula 2 in an X-ray diffraction spectrum is 65:100 to 75:100.

### Claim 8 (depends on 1)

The composite of claim 1, wherein the oxide is La2Zr2O7.

### Claim 9 (depends on 1)

The composite of claim 1, wherein the composite comprises the compound of Formula 1, the lanthanum oxide, and the lanthanum zirconium oxide.

### Claim 10 (depends on 9)

The composite of claim 9, wherein a main peak of the composite in an X-ray diffraction spectrum appears in a range of about 15 to about 70 degrees.

### Claim 11 (depends on 1)

The composite of claim 1, wherein the composite comprises the compound of Formula 2, the lanthanum oxide, and the lanthanum tantalum oxide.

### Claim 12 (depends on 11)

The composite of claim 11, wherein a main peak of the composite in an X-ray diffraction spectrum appears in a range of about 10 to about 70 degrees.

### Claim 13 (depends on 1)

An electrode active material for a lithium secondary battery, the electrode active material comprising:
a core active material; and
a coating film formed on a surface of the core active material,
wherein the coating film comprises the composite of claim 1.

### Claim 14 (depends on 13)

The electrode active material of claim 13, wherein an amount of the core active material is about 1900 to about 9900 parts by weight based on 100 parts by weight of the composite.

### Claim 15 (depends on 1)

A method of preparing a composite, the method comprising:
mixing an alkali metal source, a tri-valent metal source, and at least one selected from the group consisting of a zirconium source and a tantalum source; and
heat treating the mixture to obtain the composite of claim 1,
wherein an amount of the alkali metal source is about 2.3 to about 3.1 mol, based on 1 mol of the tri-valent metal source.

### Claim 16 (depends on 15)

The method of claim 15, wherein the heat treatment is performed at a temperature of about 500 to about 1300° C.

### Claim 17 (depends on 1)

A method of preparing an electrode active material for a lithium secondary battery, the method comprising:
mixing a core active material, the composite of claim 1, and a solvent to prepare a mixture; and
drying the mixture.

### Claim 18 (depends on 17)

The method of claim 17, wherein the drying is performed at a temperature of about 80 to about 200° C.

### Claim 19 (depends on 13)

An electrode for a lithium secondary battery, the electrode comprising the electrode active material of claim 13.

### Claim 20 (depends on 19)

A secondary lithium battery comprising the electrode of claim 19.