# US 2012/0251878 A1 · Lithium secondary battery and manufacturing method therefor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2012/0251878 A1
- Document ID: US20120251878A1
- Status: Published application
- Kind: A1
- Application number: 13/498,362
- Filed: 2009-09-28
- Published: 2012-10-04
- Earliest claimed: 2009-09-28
- Inventors: Tomoyoshi Ueki; Koji Takahata; Masaya Takahashi; Hiroe Takenaka; Mariko Sumi; Mika Okubo
- Web page: https://patentgrep.com/patent/US20120251878A1

## CPC

- H01M 4/133: Electrodes based on carbonaceous material, e.g. graphite-intercalation compounds or CFx
- H01M 4/366: {as layered products}
- H01M 4/587: for inserting or intercalating light metals
- H01M 4/62: Selection of inactive substances as ingredients for active masses, e.g. binders, fillers
- H01M 10/052: Li-accumulators
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- H01M 2220/20: Batteries in motive systems, e.g. vehicle, ship, plane
- Y02E 60/10: Energy storage using batteries
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- Y02T 10/70: Energy storage systems for electromobility, e.g. batteries
- Y10T 29/49108: Electric battery cell making
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS
- Y02T: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO TRANSPORTATION
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

The lithium secondary battery provided by the present invention includes a negative electrode having a negative electrode collector and a negative electrode layer including a negative electrode active material and formed on the surface of the negative electrode collector, and is characterized in that the negative electrode layer comprises a negative electrode active material layer composed primarily of a negative electrode active material, and an insulating layer composed primarily of an insulating filler and formed on the negative electrode active material layer, and the ratio (Sb/Sa) of a pore specific surface area of the insulating layer (Sb: m2/g) to a pore specific surface area of the negative electrode active material layer (Sa: m2/g), as measured by a mercury porosimeter, satisfies the relationship 1.2≦(Sb/Sa)≦2.5.

## Claims

### Claim at position 1

-9. (canceled)

### Claim 10

A lithium secondary battery comprising a negative electrode having a negative electrode collector and a negative electrode layer including a negative electrode active material and formed on the surface of the negative electrode collector,
wherein the negative electrode layer comprises a negative electrode active material layer composed primarily of a negative electrode active material, and an insulating layer composed primarily of an insulating filler and formed on the negative electrode active material layer, and
a ratio (Sb/Sa) of a pore specific surface area of the insulating layer (Sb: m2/g) to a pore specific surface area of the negative electrode active material layer (Sa: m2/g), as measured by a mercury porosimeter, satisfies the relationship 1.2≦(Sb/Sa)≦2.5, and
in a pore distribution of the negative electrode layer as measured by the mercury porosimeter, the mode diameter of pores in the negative electrode active material layer is 0.19 μm to 0.21 μm, and the mode diameter of pores in the insulating layer is 0.72 μm to 0.75 μm.

### Claim 11 (depends on 10)

The lithium secondary battery according to claim 10, wherein a carbon material with a mean particle size (median diameter) of 1 μm to 50 μm based on a laser diffraction particle size distribution measurement is used as the negative electrode active material, and an inorganic oxide with a mean particle size (median diameter) of 0.1 μm to 15 μm based on the laser diffraction particle size distribution measurement is used as the insulating filler.

### Claim 12 (depends on 10)

The lithium secondary battery according to claim 10, wherein at least one material selected from the group consisting of alumina, silica, and magnesia is used as the inorganic oxide.

### Claim 13

A method for producing a lithium secondary battery including a negative electrode having a negative electrode collector and a negative electrode layer including a negative electrode active material and formed on the surface of the negative electrode collector, the method comprising the steps of:
providing a negative electrode active material layer composed primarily of a negative electrode active material on the surface of the negative electrode collector, and providing an insulating layer composed primarily of an insulating filler on the negative electrode active material layer, to thereby prepare a negative electrode in which a negative electrode layer comprising the negative electrode active material layer and the insulating layer is formed on the negative electrode collector,
wherein the negative electrode layer is formed such that a ratio (Sb/Sa) of a pore specific surface area of the insulating layer (Sb: m2/g) to a pore specific surface area of the negative electrode active material layer (Sa: m2/g), as measured by a mercury porosimeter, satisfies the relationship 1.2≦(Sb/Sa)≦2.5, and
the negative electrode layer is formed by providing the negative electrode active material layer such that the mode diameter of pores therein is 0.19 μm to 0.21 μm in a pore distribution of the negative electrode layer as measured by the mercury porosimeter, and by providing the insulating layer such that the mode diameter of pores therein is 0.72 μm to 0.75 μm in the pore distribution.

### Claim 14 (depends on 13)

The production method according to claim 13, wherein a carbon material with a mean particle size (median diameter) of 0.5 μm to 20 μm based on a laser diffraction particle size distribution measurement is used as the negative electrode active material, and an inorganic oxide with a mean particle size (median diameter) of 0.1 μm to 5 μm based on the laser diffraction particle size distribution measurement is used as the insulating filler.

### Claim 15 (depends on 13)

The production method according to claim 13, wherein at least one material selected from the group consisting of alumina, silica, and magnesia is used as the inorganic oxide.

### Claim 16 (depends on 10)

A vehicle comprising the lithium secondary battery according to claim 10.