# US 2012/0251860 A1 · Lithium-Iron Disulfide Cell Design

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2012/0251860 A1
- Document ID: US20120251860A1
- Status: Published application
- Kind: A1
- Application number: 13/073,118
- Filed: 2011-03-28
- Published: 2012-10-04
- Earliest claimed: 2011-03-28
- Assignees: Eveready Battery Company, Inc.
- Inventors: Jack W. Marple; Duane James; Weiwei Huang
- Web page: https://patentgrep.com/patent/US20120251860A1

## CPC

- H01M 6/04: Cells with aqueous electrolyte
- H01M 4/0495: {Chemical alloying}
- H01M 4/381: {Alkaline or alkaline earth metals elements (H01M4/40 takes precedence)}
- H01M 4/52: of nickel, cobalt or iron
- H01M 4/581: {Chalcogenides or intercalation compounds thereof}
- H01M 4/5815: {Sulfides}
- H01M 6/02: Details (of electrodes H01M4/00; of non-active parts H01M50/00)
- H01M 6/16: with organic electrolyte (H01M6/18 takes precedence)
- Y02E 60/10: Energy storage using batteries
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- Y10T 29/49108: Electric battery cell making
- Y10T 29/49115: including coating or impregnating
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

The invention relates to primary electrochemical cells, in addition to methods for manufacturing and discharging the same, having a jellyroll electrode assembly that includes a positive electrode with a coating comprising iron disulfide deposited on a current collector situated on the outermost circumference of the jellyroll, a lithium-based negative electrode and a polymeric separator. More particularly, the invention relates to a cell design which optimizes cell capacity and substantially eliminates premature voltage drop-off on intermittent service testing by eliminating the edge effect through, for example, deliberately relieving stack pressure and/or extending the distance lithium ions proximate to the terminal end of the positive electrode must travel to undergo an electrochemical reaction in that region.

## Claims

### Claim 1

An electrochemical cell comprising:
a container;
an organic, non-aqueous electrolyte;
an electrode assembly having an anode consisting essentially of lithium or a lithium alloy strip, a cathode comprising iron disulfide at least partially coated onto both sides of a solid, metallic foil current collector and a separator disposed between the anode and the cathode;
wherein the cell possesses an interfacial anode under-balance and the anode and the cathode are spirally wound so that less than 50% of an outermost surface of the electrode assembly, excluding the separator and optional non-active components, is covered by the anode; and
means for eliminating the edge effect positioned proximate to the cathode in the outermost surface of the electrode assembly.

### Claim 2 (depends on 1)

The cell according to claim 1, wherein the means for eliminating the edge effect comprises an retardant disposed on or in the cathode coating along an axial strip at a terminal edge of the cathode.

### Claim 3 (depends on 1)

The cell according to claim 1, wherein the means for eliminating the edge effect comprises a pore-blocking substance disposed within the cathode coating along an axial strip at a terminal edge of the cathode.

### Claim 4

An electrochemical cell comprising:
a container;
an organic, non-aqueous electrolyte;
an spirally wound electrode assembly having a separator, an anode consisting essentially of lithium or a lithium alloy strip and a cathode having active material disposed on both sides of a current collector having a terminal edge oriented on an outermost surface of the spirally wound electrode assembly;
a spacer situated proximate to the terminal edge having a thickness that is: i) at least twice the thickness of the cathode, inclusive of the coating on both sides and the current collector, or ii) greater than a combined thickness of the anode, the cathode and the separator; and
wherein the cell possesses an interfacial anode under-balance the anode and the cathode are spirally wound so as to have a cathode-outer wrap.

### Claim 5 (depends on 4)

The electrochemical cell according to claim 4, wherein the spacer comprises a plurality of members.

### Claim 6 (depends on 5)

The electrochemical cell according to claim 5, wherein the members are stacked on top of one another.

### Claim 7 (depends on 5)

The electrochemical cell according to claim 5, wherein the members are aligned along an axis that coincides with the terminal edge of the cathode.

### Claim 8 (depends on 4)

The electrochemical cell according to claim 4, wherein the spacer comprises an elastomeric material.

### Claim 9

A method for making a cathode outer wrap battery which does not experience premature voltage drop-off upon intermittent discharge of the battery, the method comprising:
continuously coating a cathode mixture comprising iron disulfide onto both sides of a solid foil current collector and subsequently creating a plurality of zones of reduced electrochemical activity on at least one side of the current collector;
cutting the coated cathode into individual strips to create a plurality of individual cathodes so that the zone of reduced electrochemical activity is positioned at a terminal end of each individual cathode;
providing a separator and an anode consisting essentially of lithium or a lithium alloy wherein the anode does not include a current collector;
spirally winding the anode, the individual cathode strip and the separator into a electrode assembly so that less than 50% of an outermost surface of the electrode assembly, excluding the separator and optional non-active components, is covered by the anode and the zone of reduced electrochemical activity is situated along the outermost surface of the electrode assembly; and
disposing the electrode assembly in a conductive container, introducing a non-aqueous electrolyte to the container and closing the container.

### Claim 10 (depends on 9)

The method according to claim 9, wherein the zone of reduced electrochemical activity is created by creating a mass free zone prior to disposing the electrode assembly in the container.

### Claim 11 (depends on 10)

The method according to claim 10, wherein the mass free zone is created by providing a sacrificial substrate to the current collector prior to coating the cathode mixture and then removing the sacrificial substrate subsequent to coating the cathode mixture.

### Claim 12 (depends on 10)

The method according to claim 10, wherein the mass free zone is created by physically removing the cathode coating as the cathode is cut into individual strips.

### Claim 13 (depends on 9)

The method according to claim 9, wherein the zone of reduced electrochemical activity is created by discharging the cathode in the zone prior to disposing the electrode assembly in the container.

### Claim 14 (depends on 9)

The method according to claim 9, wherein the zone of reduced electrochemical activity is created by insulating the cathode mixture from ionic conductivity within the zone prior to disposing the electrode assembly in the container.

### Claim 15 (depends on 9)

The method according to claim 9, wherein the zone of reduced electrochemical activity is created by reducing an amount of active cathode material in the zone prior to disposing the electrode assembly in the container.

### Claim 16 (depends on 9)

The method according to claim 9, wherein the amount of cathode active material is reduced by reducing the thickness of the cathode coating.

### Claim 17 (depends on 9)

The method according to claim 9, wherein the zone of reduced electrochemical activity is created by utilizing an initiator to induce a change within the cathode.

### Claim 18 (depends on 17)

The method according to claim 17, wherein the initiator is selected from radiation, electromagnetic radiation or a light source.

### Claim 19 (depends on 17)

The method according to claim 17, wherein the cathode mixture includes a chemical which reacts with or to the initiator.

### Claim 20 (depends on 9)

The method according to claim 9, wherein the zone of reduced electrochemical activity is created by providing a spacer having a thickness that is: i) greater than a combined thickness of the anode, the cathode and the separator, or ii) at least twice the thickness of the cathode, inclusive of the coating on both sides and the current collector between the anode and the individual cathode strip proximate to the terminal end.

### Claim 21 (depends on 9)

The method according to claim 9, wherein the zone of reduced electrochemical activity is created by relieving electrode stack pressure at the terminal end as the cell discharged.

### Claim 22 (depends on 9)

The method according to claim 9, wherein the anode is provided in an amount to create an interfacial, theoretical anode-to-cathode input capacity ratio that is less than 1.0.

### Claim 23

An electrochemical cell comprising:
a container;
an organic, non-aqueous electrolyte;
an electrode assembly having an anode consisting essentially of lithium or a lithium alloy strip, a porous cathode comprising an active material containing iron disulfide or manganese dioxide disposed onto both sides of a metallic current collector and a separator disposed between the anode and the cathode;
wherein the cell the anode and the cathode are spirally wound so that less than 50% of an outermost surface of the electrode assembly, excluding the separator and optional non-active components, is covered by the anode; and
wherein the cathode includes a zone of reduced electrochemical reactivity throughout the entire cathode along its terminal edge on an outermost surface of the spirally wound electrode assembly.

### Claim 24 (depends on 23)

The electrochemical cell according to claim 23, wherein the zone of reduced electrochemical reactivity is characterized by a reduction or elimination of ionic conductivity of cathode pores within the zone.

### Claim 25 (depends on 23)

The electrochemical cell according to claim 23, wherein the zone of reduced electrochemical reactivity is created by a spacer having a thickness that is: i) at least twice the thickness of the cathode, inclusive of the coating on both sides and the current collector, or ii) greater than a combined thickness of the anode, the cathode and the separator inserted between the anode and the cathode proximate to the terminal edge of the cathode.

### Claim 26

A method for improving the discharge capacity of a lithium-iron disulfide cylindrical electrochemical cell with a cathode continuously coated onto both sides of a current collector, the method comprising:
providing a lithium-iron disulfide electrochemical cell with a spiral wound electrode assembly having an interfacial anode under-balance and a cathode outer wrap;
creating a localized area of reduced electrochemical activity at a terminal end of the cathode strip and positioning said localized area of reduced electrochemical activity proximate to the anode along the outermost surface; and
causing the cell to be discharged.