# US 2012/0251839 A1 · Housing and manufacturing method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2012/0251839 A1
- Document ID: US20120251839A1
- Status: Published application
- Kind: A1
- Application number: 13/311,746
- Filed: 2011-12-06
- Published: 2012-10-04
- Earliest claimed: 2011-03-29
- Assignees: Foxconn Technology Co., Ltd.; Fu Zhun Precision Industry (Shen Zhen) Co., Ltd.
- Inventors: ZHE-XUAN ZHANG; SHIH-PIN WANG; YAN XIONG; CHE-CHAO CHU
- Web page: https://patentgrep.com/patent/US20120251839A1

## CPC

- C25D 5/10: Electroplating with more than one layer of the same or of different metals (for bearings C25D7/10)
- C25D 5/02: Electroplating of selected surface areas
- C25D 5/48: After-treatment of electroplated surfaces
- C25D 11/026: {Anodisation with spark discharge}
- H05K 5/0252: {Labels, e.g. for identification, markings or configuration store}
- Y10T 428/12486: Laterally noncoextensive components [e.g., embedded, etc.]
- Y10T 428/12611: Oxide-containing component
- Y10T 428/13: Hollow or container type article [e.g., tube, vase, etc.]
- C25D: PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTION OF COATINGS; ELECTROFORMING; APPARATUS THEREFOR
- H05K: PRINTED CIRCUITS; CASINGS OR CONSTRUCTIONAL DETAILS OF ELECTRIC APPARATUS; MANUFACTURE OF ASSEMBLAGES OF ELECTRICAL COMPONENTS
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A housing having a coating is disclosed. The housing comprises a base substrate made of metallic material; a micro-arc oxide layer formed on the base substrate; and a protection outer film formed on the micro-arc oxide layer and comprising a coating layer and a metallic layer, wherein the metallic layer is formed on the micro-arc oxide layer and covers a portion of the micro-arc oxide layer; and the coating layer is formed on a remaining portion of the micro-arc oxide layer so that the micro-arc oxide layer is covered by the metallic layer and the coating layer.

## Claims

### Claim 1

A housing, comprising:
a base substrate made of metallic material;
a micro-arc oxide layer formed on the base substrate; and
a protection outer film formed on the micro-arc oxide layer and comprising a coating layer and a metallic layer;
wherein, the metallic layer is formed on the micro-arc oxide layer and covers a portion of the micro-arc oxide layer; and the coating layer is formed on a remaining portion of the micro-arc oxide layer so that the micro-arc oxide layer is covered by the metallic layer and the coating layer.

### Claim 2 (depends on 1)

The housing of claim 1, wherein, the metallic layer is formed on a substantially central portion of the micro-arc oxide layer, the coating layer is formed on the micro-arc oxide layer and surrounds the metallic layer.

### Claim 3 (depends on 1)

The housing of claim 1, wherein a thickness of the coating layer is in a range from about 5 μm to about 10 μm, and a thickness of the metallic layer is in a range from about 1 μm to about 40 μm.

### Claim 4 (depends on 3)

The housing of claim 3, wherein the base substrate is made of magnesium, aluminum, titanium, aluminum alloy, magnesium alloy, or titanium alloy.

### Claim 5 (depends on 1)

The housing of claim 1, wherein the metallic layer comprises a first metallic layer and a second metallic layer formed on the first metallic layer.

### Claim 6 (depends on 5)

The housing of claim 5, wherein the first metallic layer is made of copper material and has a thickness in a range from about 1 μm to about 40 μm; the second metallic layer is made of chromium material and has a thickness in a range from about 0.1 μm to about 30 μm.

### Claim 7 (depends on 5)

The housing of claim 5, wherein the second metallic layer is made of gold, nickel, tin, cobalt, silver, platinum, rhodium or palladium.

### Claim 8

A housing manufacturing method, the method comprising:
providing a metallic base substrate;
forming a micro-arc oxide layer on the base substrate;
forming an electrophoresis layer on the micro-arc oxide layer of the base substrate;
removing a portion of the electrophoresis layer to expose the micro-arc oxide layer;
forming a first metallic layer on the exposed micro-arc oxide layer;
removing a remaining portion of the electrophoresis layer to expose the micro-arc oxide layer;
forming a coating layer on the micro-arc oxide layer and the first metallic layer; and
removing the coating layer formed on the first metallic layer and forming a second metallic layer on the first metallic layer.

### Claim 9 (depends on 8)

The housing manufacturing method of claim 8, removing of the coating layer comprises a ray carving process.

### Claim 10 (depends on 8)

The housing manufacturing method of claim 8 further comprises cleaning the base substrate before forming a micro-arc oxide layer on the base substrate.

### Claim 11 (depends on 10)

The housing manufacturing method of claim 10, cleaning of the base substrate comprises pre-cleaning the base substrate, and drying the substrate; wherein the pre-cleaning comprises an ultrasonic cleaning process, a pickling process, an alkaline cleaning process, or a washing process.

### Claim 12 (depends on 8)

The housing manufacturing method of claim 8, the forming a micro-arc oxide layer comprises an oxidation process to form a porous metal oxide ceramic film.

### Claim 13 (depends on 12)

The housing manufacturing method of claim 12, wherein the oxidation process is taken under a positive voltage in a range from about 300 to about 550 volts, a current density in a range from about 1 to about 9 amperes per square decimeter, and an oxidation time for about 3 to about 30 minutes.

### Claim 14 (depends on 13)

The housing manufacturing method of claim 13, wherein the thickness of the micro-arc oxide layer is in a range from about 1 μm to about 200 μm.

### Claim 15 (depends on 13)

The housing manufacturing method of claim 13, wherein the first metallic layer is made of copper material, and a thickness of the first metallic layer is in a range from about 1 μm to about 40 μm.

### Claim 16 (depends on 15)

The housing manufacturing method of claim 15, the forming the first metallic layer on the micro-arc oxide layer comprising:
immersing the base substrate into an alkaline liquid about 3-10 minutes under room temperature;
immersing the base substrate into a sodium hydroxide solution with a density about 15 g/L for about 0.5-2 minutes;
immersing the base substrate into a liquid mixture of copper sulfate, sodium potassium tartrate, sodium hydroxide, sodium carbonate, formaldehyde, and thiocarbamide for about 3-10 minutes;
electroplating a copper layer on the exposed micro-arc oxide layer of the base substrate.

### Claim 17 (depends on 16)

The housing manufacturing method of claim 16, wherein the alkaline liquid is mixed with Sodium tetrachloropalladate (II), 2-morpholinyl ethane sulfonic acid, and sodium chloride; the density of the Sodium tetrachloropalladate (II) is about 0.05-0.3 g/L.

### Claim 18 (depends on 17)

The housing manufacturing method of claim 17, wherein the electroplating of a copper layer is under a temperature of about 50-60° C., and a current density in a range from about 0.5 to about 10 amperes per square decimeter; a plating solution applied to the copper plating process is mixed by copper pyrophosphate and potassium pyrophosphate, a density of the copper pyrophosphate is about 70-100 g/L, and a density of the potassium pyrophosphate is about 300-400 g/L.